Patent US3634208A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3634208A Expired / Lapsed US ⏱️ 0.0 years remaining

Coloring method of aluminum anodic oxide coating film

Assignee: Aiden KK
•
Filing: 1969-09-25
•
Granted: 1972-01-11
•
Expires: 1989-09-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Alumite is colored by first subjecting same to an alternating current electrolyzing treatment in an electrolyte followed by a direct current electrolyzing treatment in a coloring solution in which the alumite is the cathode.

Inventors

  • 👤 Koichi Kuroda

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 21:59
CPC Classifications
C; C25; C25D; C25D11/00; C25D11/02; C25D11/04; C25D11/18; C25D11/20; C25D11/22

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 27 words
A method as claimed in claim 1 wherein the direct current electrolyzing treatment is effected for about 2 minutes at a current density of about 0.6 A/dm.2.
Claim 2
Dependent Claim 14 words
A method as claimed in claim 1 wherein the electrolytic solution is sulfuric acid.
Claim 3
Dependent Claim 22 words
A method as claimed in claim 1 wherein the electrolyte containing color producing metallic ions comprises KAu(CN)2, citric acid and sodium citrate.
Claim 4
Dependent Claim 27 words
A method as claimed in claim 1 wherein the alternating current electrolyzing treatment is effected for about 2 minutes at a current density of about 1.5 A/dm.2.
Claim 5
Dependent Claim 27 words
A method as claimed in claim 5 wherein the direct current electrolyzing treatment is effected for about 2 minutes at a current density of about 0.6 A/dm.2.
Claim 6
Dependent Claim 21 words
A method as claimed in claim 1 wherein the electrolyte containing color producing metallic ions comprises NiSO4, boric acid and NH4CL.
Claim 7
Dependent Claim 11 words
The product produced by the method as claimed in claim 7.
Claim 8
Dependent Claim 38 words
A method as claimed in claim 1 wherein the anodic aluminum oxide is prepared by an oxidizing aluminum in a bath which is the same as the electrolytic solution in which the alternating current electrolyzing treatment is effected.
Claim 9
Dependent Claim 13 words
A method as claimed in claim 9 wherein the bath is sulfuric acid.
Claim 10
Dependent Claim 11 words
The product produced by the method as claimed in claim 10.

References Cited (Backward Citations)

US3382160A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1975-01-10 1975-07-12 1976-01-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1979-01-10 1979-07-12 1980-01-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1983-01-10 1983-07-12 1984-01-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag