Austenitic stainless steel alloy

Assignee: Carpenter Steel Co
•
Filing: 1964-09-15
•
Granted: 1968-01-09
•
Expires: 1984-09-15
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Walter C Ziolkowski

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 06:08
CPC Classifications
G; G21; G21C; G21C7/00; G21C7/06; G21C7/24; C; C22; C22C; C22C38/00; C22C38/18; C22C38/40; Y; Y02; Y02E; Y02E30/00; Y02E30/30; Y10; Y10S; Y10S376/00; Y10S376/90

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 121 words
AN AUSTENITIC STAINLELSS STEEL ALLOY COMPRISING, IN APPROXIMATE PERCENT BY WEIGHT, UP TO .25% CARBON, UP TO 10% MANGANESE, UP TO 2% SILICON, UP TO 1% OF THE GROUP PHOSPHOROUS, SULFUR AND SELENIUM, 12% TO 26% CHROMIUM, 3.5% TO 22% NICKEL, UP TO 4% MOLYBDENUM, UP TO 4% COPPER, UP TO 4% ALUMINUM, UP TO 1.25% TITANIUM, UP TO 1.25% COLUMBIUM, UP TO .7% NITROGEN, FROM .2% TO 3% OF AT LEAST ONE ELEMENT FROM THE GROUP CONSISTING OF GADOLINIUM, EUROPIUM, SAMARIUM AND DYSPROSIUM WITH THE COMBINED TOTAL OF THE ELEMENTS FROM SAID GROUP NOT EXCEEDING 3%, THE REMAINDER BEING SUBSTANTIALLY IRON, AND THE ELEMENTS BEING BALANCED SO THAT AN AS-CAT INGOT OF THE ALLOY CONTAINS ABOUT 5% TO 25% FERRITE.
Claim 2
Dependent Claim 121 words
AN AUSTENITIC STAINLELSS STEEL ALLOY COMPRISING, IN APPROXIMATE PERCENT BY WEIGHT, UP TO .25% CARBON, UP TO 10% MANGANESE, UP TO 2% SILICON, UP TO 1% OF THE GROUP PHOSPHOROUS, SULFUR AND SELENIUM, 12% TO 26% CHROMIUM, 3.5% TO 22% NICKEL, UP TO 4% MOLYBDENUM, UP TO 4% COPPER, UP TO 4% ALUMINUM, UP TO 1.25% TITANIUM, UP TO 1.25% COLUMBIUM, UP TO .7% NITROGEN, FROM .2% TO 3% OF AT LEAST ONE ELEMENT FROM THE GROUP CONSISTING OF GADOLINIUM, EUROPIUM, SAMARIUM AND DYSPROSIUM WITH THE COMBINED TOTAL OF THE ELEMENTS FROM SAID GROUP NOT EXCEEDING 3%, THE REMAINDER BEING SUBSTANTIALLY IRON, AND THE ELEMENTS BEING BALANCED SO THAT AN AS-CAT INGOT OF THE ALLOY CONTAINS ABOUT 5% TO 25% FERRITE.

References Cited (Backward Citations)

USRE24243E Cited
US2190486A Cited
US2104836A Cited
US2643949A Cited
US2683663A Cited
US3189445A Cited
US3189446A Cited
US3168397A Cited
US3245782A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1971-01-08 1971-07-10 1972-01-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1975-01-08 1975-07-10 1976-01-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1979-01-08 1979-07-10 1980-01-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag