Patent US3360593A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3360593A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of preparing fibers from solidified phosphorus-furnace slag

Assignee: FMC Corp
•
Filing: 1965-08-23
•
Granted: 1967-12-26
•
Expires: 1985-08-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Rau Eric
  • 👤 Jr William H Kibbel

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 04:35
CPC Classifications
C; C03; C03B; C03B37/00; C03B37/01; C03B37/04; C03B37/05; C03C; C03C13/00; C03C13/06

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 115 words
A METHOD OF PRODUCING FIBERS RESISTANT TO CRYSTALLIZATION AND PHYSICAL DEGRADATION ON AGING FROM A SOLIDIFIED FURNACE SLAG, COMPRISING HEATING SAID SLAG TO A CONDITIONING TEMPERATURE AT LEAST 100*C. ABOVE THE TEMPERATURE AT WHICH THE SLAG IS MELTED AND HAS A SPINNING VISCOSITY OF 15 POISES, HOLDING SAID MOLTEN SLAG AT SAID CONDITIONING TEMPERATURE FOR A CONDITIONING TIME OF AT LEAST 10 MINUTES TO PRODUCE A CONDITIONED SLAG, FEEDING SAID CONDITIONED SLAG TO A SPINNER WHEEL WHICH THROWS STREAMS OF SAID MOLTEN, CONDITIONED SLAG OUTWARDLY, SAID SLAG BEING AT A CONDITIONING TEMPERATURE ON SAID SPINNER WHEEL, AND INTERCEPTING SAID STREAMS BY A HIGH VELOCITY FLOW OF A GASEOUS FLUID TO ATTENUATE THE STREAMS INTO FIBERS.
Claim 2
Independent Claim 115 words
A METHOD OF PRODUCING FIBERS RESISTANT TO CRYSTALLIZATION AND PHYSICAL DEGRADATION ON AGING FROM A SOLIDIFIED FURNACE SLAG, COMPRISING HEATING SAID SLAG TO A CONDITIONING TEMPERATURE AT LEAST 100*C. ABOVE THE TEMPERATURE AT WHICH THE SLAG IS MELTED AND HAS A SPINNING VISCOSITY OF 15 POISES, HOLDING SAID MOLTEN SLAG AT SAID CONDITIONING TEMPERATURE FOR A CONDITIONING TIME OF AT LEAST 10 MINUTES TO PRODUCE A CONDITIONED SLAG, FEEDING SAID CONDITIONED SLAG TO A SPINNER WHEEL WHICH THROWS STREAMS OF SAID MOLTEN, CONDITIONED SLAG OUTWARDLY, SAID SLAG BEING AT A CONDITIONING TEMPERATURE ON SAID SPINNER WHEEL, AND INTERCEPTING SAID STREAMS BY A HIGH VELOCITY FLOW OF A GASEOUS FLUID TO ATTENUATE THE STREAMS INTO FIBERS.

References Cited (Backward Citations)

US2793395A Cited
US3097085A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1970-12-25 1971-06-26 1971-12-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1974-12-25 1975-06-26 1975-12-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1978-12-25 1979-06-26 1979-12-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag