Patent US3308096A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3308096A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of continuous manufacturing of a phenol-aldehyde resin

Assignee: Individual
•
Filing: 1965-08-23
•
Granted: 1967-03-07
•
Expires: 1985-08-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Ivanov Petr Sergeevich
  • 👤 Diomkin Vladimir Mikhailovich

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 19:11
CPC Classifications
C; C08; C08G; C08G8/00; C08G8/04; C08G8/08; B; B01; B01J; B01J10/00; B01J10/02; B01J19/00; B01J19/28; B01J2219/00; B01J2219/00049; B01J2219/00051; B01J2219/00074; B01J2219/00087; B01J2219/00094; B01J2219/00101; B01J2219/00121; B01J2219/00159; B01J2219/00162; Y; Y02; Y02P; Y02P20/00; Y02P20/50; Y02P20/582

Claims Analysis

Total Claims: 1
Claim 1
Independent Claim 264 words
A CONTINUOUS PROCESS FOR PRODUCING PHENOL-ALDEHYDE RESINS, COMPRISING POLYCONDENSATION OF A PHENOL WITH AN ALDEHYDE IN THE PRESENCE OF A CATALYST, SEPARATING FROM THE REACTION MASS PRODUCED AT THE POLYCONDENSATION STAGE A LAYER CONSISTING OF RESINOUS POLYCONDENSATION PRODUCTS INSOLUBLE IN WATER, SEPARATING AND REMOVING AN AQUEOUS LAYER FROM SAID RESINOUS POLYCONDENSATION PRODUCTS; THEREAFTER DRYING SAID RESINOUS POLYCONDENSATION PRODUCTS EFFECTED BY CONTINUOUSLY PASSING SAID PRODUCTS THROUGH AN EXTERNALLY HEATED ELONGATED PASSAGEWAY, SAID PASSAGEWAY HAVING AN INLET END MAINTAINED AT A PRESSURE SLIGHTLY HIGHER THAN THE PRESSURE AT THE OUTLET END OF SAID PASSAGEWAY, THEREBY ASSISTING SAID PRODUCTS TO FLOW IN SAID PASSAGEWAY FROM THE RELATIVELY HIGHER PRESSURE INLET TOWARDS THE RELATIVELY LOWER PRESSURE OUTLET AND ALONG WHICH THESE PRODUCTS TRAVEL TOGETHER WITH THE VAPORS OF VOLATILE SUBSTANCES WHICH ARE LIBERATED FROM SAID PRODUCTS AS THE RESULT OF HEATING, THE HEAT EXCHANGE AREAS OF SAID PASSAGEWAY BEING SUFFICIENT TO TRANSFER TO SAID PRODUCTS AN AMOUNT OF HEAT WHICH PERMITS OF DIMINISHING AS THE RESULT OF EVAPORATION THE CONTENT OF VOLATILE SUBSTANCES IN SAID PRODUCTS, POLYCONDENSATION PRODUCTS BEING FED INTO SAID PASSAGEWAY IN SUCH AN AMOUNT PER UNIT TIME AND SAID PASSAGEWAY HAVING A CROSS SECTIONAL AREA RELATED TO SAID AMOUNT SO THAT THE TRAVEL VELOCITY OF VOLATILE SUBSTANCES IN THE PASSAGEWAY REACHES AT LEAST 15 MM. PER SEC., SEPARATING THE RESIN FROM SAID VAPORS OF VOLATILE SUBSTANCES, COOLING AND LIQUEFYING SAID VAPORS OF VOLATILE SUBSTANCES, WHICH ARE LIBERATED FROM THE RESINOUS POLYCONDENSSATION PRODUCTS, USING THE PRODUCED CONDENSATE, WHICH IS AN AQUEOUS SOLUTION OF UNCONVERTED STARTING COMPONENTS, PREDOMINANTLY A PHENOL, AS RAW MATERIAL AT THE POLYCONDENSATION STAGE.

References Cited (Backward Citations)

US2658054A Cited
US2750354A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1970-03-06 1970-09-05 1971-03-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1974-03-06 1974-09-05 1975-03-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1978-03-06 1978-09-05 1979-03-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag