Patent US3296009A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3296009A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for providing textile floor covering with latex resin foam coating

Assignee: Hansawerke Lurman Schutte and Co
•
Filing: 1965-01-05
•
Granted: 1967-01-03
•
Expires: 1985-01-05
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Schutte Theodor
  • 👤 Jacobs Gunter

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 13:50
CPC Classifications
D; D06; D06N; D06N3/00; D06N3/04; D06N3/10; D06N7/00; D06N7/0063; D06N7/0071; D06N7/0073; D06N2203/00; D06N2203/02; D06N2203/04; D06N2203/045; D06N2205/00; D06N2205/04; D06N2205/20; D06N2207/00; D06N2207/12; D06N2207/123; D06N2209/00; D06N2209/10; D06N2209/106; D06N2211/00; D06N2211/06; D06N2211/066

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 292 words
PROCESS FOR PROVIDING TEXTILE FLOOR-COVERINGS WITH A STIFF RESILIENT COATING, ESSENTIALLY CONSISTING OF APPLYING TO ONE SURFACE OF THE TEXTILE FLOOR-COVERING A COMPOSITION CONSISTING ESSENTIALLY OF A FOAMED SUBSTANTIALLY UNIFORM MIXTURE PREPARED BY MIXING (A) A RUBBER LATEX DISPERSION (B) WITH AN AQUEOUS DISPERSION OF POLYVINYL ACETATE AND (C) WITH A FILLING MATERIAL SUBSTANTILLY FINELY AND UNIFORMLY DISTRIBUTED IN SAID MIXTURE AND COMPATIBLE WITH SAID MIXTURE, AND BY FOAMING THE RESULTING MIXTURE SAID AQUEOUS DISPERSION OF THE POLYVINYL ACETATE AND SAID FILLING MATERIAL BEING COMPATIBLE WITH SAID MIXTURE; 100 PARTS BY WEIGHT OF SAID COMPOSITION CONTAINING 2.5 TO 60 PARTS BY WEIGHT OF DRY RUBBER AND 1 TO 60 PARTS BY WEIGHT OF DRY POLYVINYL ACETATE IN A WEIGHT RATIO OF 1 TO 3 UP TO 8 TO 1 OF RUBBER TO POLYVINYL ACETATE, 0 TO 200 PARTS BY WEIGHT OF DRY FILLER, ALL OF SAID PARTS BEING BASED ON THE TOTAL WEIGHT OF DRY RUBBER AND DRY POLYVINYL ACETATE PRESENT IN THE COMPOSITION; HEATING THE RESULTING COATED TEXTILE FLOOR COVERING FORMED ON ONE SURFACE OF THE FLOORCOVERING, TO GELLING TEMPERATURE IN ORDER TO CAUSE GELLING OF THE COATING; PRESSING TOGETHER PART OF THE GELLED COATING AND THE CORRESPONDING REGISTERING TEXTILE FLOOR-COVERING ADHERED THERETO ON AT LEAST 1/4 TO 2/3 OF THE ENTIRE COATED SURFACE OF THE FLOOR-COVERING IN ORDER TO ATTAIN STRONG ADHERENCE BETWEEN SAID PART OF THE COATING AND THE CORRESPONDING PART OF THE FLOOR-COVERING, AND APPLYING SUBSTANTIALLY LOWER PRESSURE THAN THAT APPLIED IN SAID PRESSURE TOGETHER OF SAID PART OF THE GELLED COATING AND THE TEXTILE FLOOR-COVERING, TO THE REMAINING PART OF THE COATED TEXTILE FLOOR COVERING IN ORDER TO FORM RAISED PORTIONS OF HIGH ELASTICITY IN THE GELLED COATING; DRYING AND VULCANIZING BY HEATING THE COATED TEXTILE FLOOR-COVERING.
Claim 2
Dependent Claim 292 words
PROCESS FOR PROVIDING TEXTILE FLOOR-COVERINGS WITH A STIFF RESILIENT COATING, ESSENTIALLY CONSISTING OF APPLYING TO ONE SURFACE OF THE TEXTILE FLOOR-COVERING A COMPOSITION CONSISTING ESSENTIALLY OF A FOAMED SUBSTANTIALLY UNIFORM MIXTURE PREPARED BY MIXING (A) A RUBBER LATEX DISPERSION (B) WITH AN AQUEOUS DISPERSION OF POLYVINYL ACETATE AND (C) WITH A FILLING MATERIAL SUBSTANTILLY FINELY AND UNIFORMLY DISTRIBUTED IN SAID MIXTURE AND COMPATIBLE WITH SAID MIXTURE, AND BY FOAMING THE RESULTING MIXTURE SAID AQUEOUS DISPERSION OF THE POLYVINYL ACETATE AND SAID FILLING MATERIAL BEING COMPATIBLE WITH SAID MIXTURE; 100 PARTS BY WEIGHT OF SAID COMPOSITION CONTAINING 2.5 TO 60 PARTS BY WEIGHT OF DRY RUBBER AND 1 TO 60 PARTS BY WEIGHT OF DRY POLYVINYL ACETATE IN A WEIGHT RATIO OF 1 TO 3 UP TO 8 TO 1 OF RUBBER TO POLYVINYL ACETATE, 0 TO 200 PARTS BY WEIGHT OF DRY FILLER, ALL OF SAID PARTS BEING BASED ON THE TOTAL WEIGHT OF DRY RUBBER AND DRY POLYVINYL ACETATE PRESENT IN THE COMPOSITION; HEATING THE RESULTING COATED TEXTILE FLOOR COVERING FORMED ON ONE SURFACE OF THE FLOORCOVERING, TO GELLING TEMPERATURE IN ORDER TO CAUSE GELLING OF THE COATING; PRESSING TOGETHER PART OF THE GELLED COATING AND THE CORRESPONDING REGISTERING TEXTILE FLOOR-COVERING ADHERED THERETO ON AT LEAST 1/4 TO 2/3 OF THE ENTIRE COATED SURFACE OF THE FLOOR-COVERING IN ORDER TO ATTAIN STRONG ADHERENCE BETWEEN SAID PART OF THE COATING AND THE CORRESPONDING PART OF THE FLOOR-COVERING, AND APPLYING SUBSTANTIALLY LOWER PRESSURE THAN THAT APPLIED IN SAID PRESSURE TOGETHER OF SAID PART OF THE GELLED COATING AND THE TEXTILE FLOOR-COVERING, TO THE REMAINING PART OF THE COATED TEXTILE FLOOR COVERING IN ORDER TO FORM RAISED PORTIONS OF HIGH ELASTICITY IN THE GELLED COATING; DRYING AND VULCANIZING BY HEATING THE COATED TEXTILE FLOOR-COVERING.

References Cited (Backward Citations)

US2563478A Cited
US1919059A Cited
US2706183A Cited
US2628654A Cited
US2585109A Cited
US2795207A Cited
US2817597A Cited
US3144355A Cited
US3083124A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1970-01-02 1970-07-04 1971-01-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1974-01-02 1974-07-04 1975-01-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1978-01-02 1978-07-04 1979-01-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag