Patent US3240635A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3240635A Expired / Lapsed US ⏱️ 0.0 years remaining

Wire cloth and wire belts for use in paper making machines and method of making such wire cloth and wire belts

Assignee: Lindsay Wire Weaving Co
•
Filing: 1962-05-17
•
Granted: 1966-03-15
•
Expires: 1982-05-17
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Alfred G Hose
  • 👤 Laurence D Kunsman

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 17:06
CPC Classifications
D; D21; D21F; D21F1/00; D21F1/10; B; B21; B21F; B21F33/00; C; C22; C22C; C22C19/00; C22C19/07; C22C38/00; C22C38/18; C22C38/40; C22C38/52; C22C9/00; C22F; C22F1/00

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 172 words
A PROCESS FOR MAKING AN ENDLESS BELT FOR USE WITH PAPER MAKING MACHINES, HAVING INTERWOVEN SETS OF WARP AND SHUTE WIRES MADE FFOM PRECIPITATION HARDENABLE COPPER-BERYLLIUM-COBALT ALLOYS, THE STEPS INCLUDING REDUCING THE WARP AND SHUTE WIRES FROM AN INTERMEDIATE WIRE SIZE DOWN TO A FINISHED WIRE SIZE, HEATING THE WARP AND SHUTE WIRES TO A TEMPERATURE OF ABOUT 1,475*F., FOR A PERIOD OF TIME OF ABOUT 15 MINUTES AND QUENCHING THE WIRES TO SECURE A PREDETERMINED YIELD AND TENSILE STRENGTH SUITABLE FOR FORMING INTO WIRE CLOTH, WEAVING THE WARP AND SHUTE WIRES INTO A WOVEN WIRE CLOTH, JOINING THE ENDS OF THE WOVEN WIRE CLOTH TOGETHER TO FORM AN ENDLESS BELT, HEATING THE ENDLESS BELT TO A TEMPERATURE OF ABOUT BETWEEN 475*F. TO 650*F. FOR A PERIOD OF TIME RANGING BETWEEN 1/4 AND 3 HOURS AND COOLING THE BELT TO ROOM TEMPERATURE TO PROVIDE IN THE HARDENED BELT A WARPWISE TENSILE STRENGTH OF ABOUT 300 LBS. PER INCH OF WIDTH WITH A WARPWISE BENDING FATIGUE RESISTENCE OF ABOUT 16,000 CYCLES TO FAILURE.
Claim 2
Dependent Claim 173 words
A PROCESS FOR MAKING AN ENDLESS BELT FOR USE WITH PAPER MAKING MACHINES HAVING INTERWOVEN SETS OF WARP AND SHUTE WIRES MADE FROM PRECIPITATION HARDENABLE IRONNICKEL-CHROMIUM-COBALT ALLOYS, THE STEPS INCLUDING REDUCING THE WARP AND SHUTE WIRES FROM AN INTERMEDIATE WIRE SIZE DOWN TO A FINISHED WIRE SIZE, HEATING THE WARP AND SHUTE WIRES TO A TEMPERATURE OF ABOUT 1,475*F. FOR A PERIOD OF TIME OF ABOUT 15 MINUTES AND QUENCHING THE WIRES TO SECURE A PREDETERMINED YIELD AND TENSILE STRENGTH SUITABLE FOR FORMING INTO WIRE CLOTH, WEAVING THE WARP AND SHUTE WIRES INTO A WOVEN WIRE CLOTH, JOINING THE ENDS OF THE WOVEN WIRE CLOTH TOGETHER TO FORM AN ENDLESS BELT, HEATING THE ENDLESS BELT TO A TEMPERATURE BETWEEN ABOUT 600*F. TO 1,000*F. FOR A PERIOD OF TIME RANGING BETWEEN ABOUT 3 TO 5 HOURS, AND THEN COOLING THE WIRE TO ROOM TEMPERATURE TO PROVIDE IN THE HARDENED BELT A WARPWISE TENSILE STRENGTH OF ABOUT 500 LBS. PER INCH OF WIDTH WITH A WARPWISE BENDING FATIGUE RESISTANCE OF ABOUT 31,000 CYCLES OF FAILURE.

References Cited (Backward Citations)

US1975114A Cited
US2088449A Cited
US2288512A Cited
US2422477A Cited
US2482098A Cited
US2859149A Cited
US2908065A Cited
US2958618A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1969-03-14 1969-09-13 1970-03-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1973-03-14 1973-09-13 1974-03-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1977-03-14 1977-09-13 1978-03-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag