Patent US3224072A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3224072A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of forming an electrical connection to an insulating base

Assignee: BAC AND BRITISH AEROSPACE
•
Filing: 1962-12-27
•
Granted: 1965-12-21
•
Expires: 1982-12-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Summers Leo Ewart Arthur
  • 👤 Horwood Roger John

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 18:09
CPC Classifications
H; H05; H05K; H05K1/00; H05K1/02; H05K1/09; C; C03; C03C; C03C17/00; C03C17/34; C03C17/36; C03C17/40; C23; C23C; C23C14/00; C23C14/02; C23C14/024; C23C14/025; C23C14/22; C23C14/54; C23C14/541; H01; H01B; H01B1/00; C04; C04B; C04B2235/00; C04B2235/60; C04B2235/604; H05K2201/00; H05K2201/03; H05K2201/0302; H05K2201/0317; H05K3/00; H05K3/38; H05K3/388; Y; Y10; Y10S; Y10S228/00; Y10S228/903; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49124; Y10T29/4913; Y10T29/49144; Y10T29/49147; Y10T29/49149; Y10T29/49155; Y10T29/49162

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 122 words
A METHOD OF FORMING ON AN INSULATING BASE AN ELEMENT OF A METAL OF HIGH ELECTRICAL CONDUCTIVITY COMPRISING THE STEPS OF DEPOSITING ON THE BASE IN A VACUUM CHAMBER A PRIMARY LAYER OF A METAL DIFFERENT FROM SAID HIGHLY CONDUCTIVE METAL AND WHICH WILL PROVIDE GOOD BONDS BOTH BETWEEN ITSELF AND THE MATERIAL OF THE BASE AND BETWEEN ITSELF AND SAID HIGHLY CONDUCTIVE METAL, THEN DEPOSITING ON SAID PRIMARY LAYER BY VACUUM DEPOSITION AT LEAST THREE LAYERS OF SAID HIGHLY CONDUCTIVE METAL, THE TEMPERATURE OF THE BASE BEING REDUCED FOR THE DEPOSITING OF EACH SUCCESSIVE LAYER OF SAID HIGHLY CONDUCTIVE METAL AND THE DEPOSITION OF EACH SUCCESSIVE LAYER OF HIGHLY CONDUCTIVE METAL BEING CONTINUED UNTIL IT IS THICKER THAN THE PRECEEDING ONE.
Claim 2
Independent Claim 122 words
A METHOD OF FORMING ON AN INSULATING BASE AN ELEMENT OF A METAL OF HIGH ELECTRICAL CONDUCTIVITY COMPRISING THE STEPS OF DEPOSITING ON THE BASE IN A VACUUM CHAMBER A PRIMARY LAYER OF A METAL DIFFERENT FROM SAID HIGHLY CONDUCTIVE METAL AND WHICH WILL PROVIDE GOOD BONDS BOTH BETWEEN ITSELF AND THE MATERIAL OF THE BASE AND BETWEEN ITSELF AND SAID HIGHLY CONDUCTIVE METAL, THEN DEPOSITING ON SAID PRIMARY LAYER BY VACUUM DEPOSITION AT LEAST THREE LAYERS OF SAID HIGHLY CONDUCTIVE METAL, THE TEMPERATURE OF THE BASE BEING REDUCED FOR THE DEPOSITING OF EACH SUCCESSIVE LAYER OF SAID HIGHLY CONDUCTIVE METAL AND THE DEPOSITION OF EACH SUCCESSIVE LAYER OF HIGHLY CONDUCTIVE METAL BEING CONTINUED UNTIL IT IS THICKER THAN THE PRECEEDING ONE.
Claim 3
Independent Claim 156 words
A METHOD OF FORMING ON AN INSULATING BASE AN ELEMENT OF GOLD AND OF CONNECTING A GOLD WIRE THERETO, COMPRISING THE STEPS OF DEPOSITING ON THE BASE IN A VACUUM CHAMBER A PRIMARY LAYER OF A DIFFERENT METAL WHICH WILL PROVIDE GOOD BONDS BOTH BETWEN ITSELF AND THE MATERIAL OF THE BASE AND BETWEEN ITSELF AND GOLD, THEN DEPOSITING ON SAID PRIMARY LAYER BY A VACUUM DEPOSITION METHOD COMPRISING THE EVAPORATION OF A GOLD SOURCE AT LEAST THREE LAYERS OF GOLD, THE TEMPERATURE OF THE BASE BEING REDUCED FOR THE DEPOSITING OF EACH SUCCESSIVE LAYER OF GOLD AND THE DEPOSITION OF EACH SUCCESSIVE LAYER OF GOLD BEING CONTINUED UNTIL IT IS THICKER THAN THE PRECEEDING ONE, PREHEATING THE INSULATING BASE WITH A STREAM OF HOT INERT GAS AN BONDING THE GOLD WIRE TO THE TOP LAYER OF THE DEPOSITED GOLD ELELMETN BY THE APPLICATION OF HEAT AN DPRESSURE IN THE PRESENCE OF THE HOT INERT GAS.
Claim 4
Independent Claim 156 words
A METHOD OF FORMING ON AN INSULATING BASE AN ELEMENT OF GOLD AND OF CONNECTING A GOLD WIRE THERETO, COMPRISING THE STEPS OF DEPOSITING ON THE BASE IN A VACUUM CHAMBER A PRIMARY LAYER OF A DIFFERENT METAL WHICH WILL PROVIDE GOOD BONDS BOTH BETWEN ITSELF AND THE MATERIAL OF THE BASE AND BETWEEN ITSELF AND GOLD, THEN DEPOSITING ON SAID PRIMARY LAYER BY A VACUUM DEPOSITION METHOD COMPRISING THE EVAPORATION OF A GOLD SOURCE AT LEAST THREE LAYERS OF GOLD, THE TEMPERATURE OF THE BASE BEING REDUCED FOR THE DEPOSITING OF EACH SUCCESSIVE LAYER OF GOLD AND THE DEPOSITION OF EACH SUCCESSIVE LAYER OF GOLD BEING CONTINUED UNTIL IT IS THICKER THAN THE PRECEEDING ONE, PREHEATING THE INSULATING BASE WITH A STREAM OF HOT INERT GAS AN BONDING THE GOLD WIRE TO THE TOP LAYER OF THE DEPOSITED GOLD ELELMETN BY THE APPLICATION OF HEAT AN DPRESSURE IN THE PRESENCE OF THE HOT INERT GAS.

References Cited (Backward Citations)

US2220545A Cited
GB846559A Cited
GB874965A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1968-12-20 1969-06-21 1969-12-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1972-12-20 1973-06-21 1973-12-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1976-12-20 1977-06-21 1977-12-21 $7700.00 Window Closed / Lapsed