Abstract

No abstract record available.

Inventors

  • 👤 Fritzsching Peter Rudolph
  • 👤 Robert C Gilardi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 17:00
CPC Classifications
D; D21; D21H; D21H19/00; D21H19/10; D21H19/12

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 143 words
A METHOD OF COATING A PRINTED PAPER SHEET HAVING A DRY PRINTED SURFACE WHICH COMPRISES APPLYING AN AQUEOUS SOLUTION CONSISTING ESSENTIALLY OF WATER AND FROM ABOUT 5 PERCENT TO 30 PERCENT BY WEIGHT OF POLYVINYL ALCOHOL HAVING A DEGREE OF HYDROLYSIS RANGING FROM 96 PERCENT TO 100 PERCENT AND A VISCOSITY IN 4 PER CENT AQUEOUS SOLUTION AT 20*C. RANGING FROM ABOUT 2 TO 150 CENTIPOISES TO SAID DRY PRINTED SURFACE OF SAID PAPER SHEET, SAID SOLUTION BEING APPLIED IN A QUANTITY TO PROVIDED ABOUT 0.6 POUND TO ABOUT 4 POUNDS OF POLYVINYL ALCOHOL PER 1,000 SQUARE FEET OF SAID PAPER SHEET, AND DRYING THE PAPER SHEET AT A SHEET TEMPERATURE OF ABOUT 160* TO 195*F. TO A MOISTURE CONTENT OF AT MOST 4 PERCENT, TO PRODUCE A THIN, WATER-RESISTANT, TRANSPARENT FILM OF POLYVINYL ALCOHOL SUPERIMPOSED ON SAID PRINTED SURFACE OF SAID SHEET.
Claim 2
Independent Claim 143 words
A METHOD OF COATING A PRINTED PAPER SHEET HAVING A DRY PRINTED SURFACE WHICH COMPRISES APPLYING AN AQUEOUS SOLUTION CONSISTING ESSENTIALLY OF WATER AND FROM ABOUT 5 PERCENT TO 30 PERCENT BY WEIGHT OF POLYVINYL ALCOHOL HAVING A DEGREE OF HYDROLYSIS RANGING FROM 96 PERCENT TO 100 PERCENT AND A VISCOSITY IN 4 PER CENT AQUEOUS SOLUTION AT 20*C. RANGING FROM ABOUT 2 TO 150 CENTIPOISES TO SAID DRY PRINTED SURFACE OF SAID PAPER SHEET, SAID SOLUTION BEING APPLIED IN A QUANTITY TO PROVIDED ABOUT 0.6 POUND TO ABOUT 4 POUNDS OF POLYVINYL ALCOHOL PER 1,000 SQUARE FEET OF SAID PAPER SHEET, AND DRYING THE PAPER SHEET AT A SHEET TEMPERATURE OF ABOUT 160* TO 195*F. TO A MOISTURE CONTENT OF AT MOST 4 PERCENT, TO PRODUCE A THIN, WATER-RESISTANT, TRANSPARENT FILM OF POLYVINYL ALCOHOL SUPERIMPOSED ON SAID PRINTED SURFACE OF SAID SHEET.

References Cited (Backward Citations)

US2256853A Cited
US2362026A Cited
US2597863A Cited
US2582357A Cited
US2929931A Cited
US2949382A Cited
US3087920A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1968-11-15 1969-05-17 1969-11-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1972-11-15 1973-05-17 1973-11-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1976-11-15 1977-05-17 1977-11-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag