Method of bonding a rubbery composition to a reinforcing element

Assignee: Goodyear Tire and Rubber Co
•
Filing: 1961-06-28
•
Granted: 1965-06-22
•
Expires: 1981-06-28
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 James A Cardina

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 16:17
CPC Classifications
C; C08; C08J; C08J5/00; C08J5/04; C08J5/06; C08G; C08G8/00; C08G8/28; C09; C09J; C09J163/00; C08J2321/00; C08L; C08L2666/00; C08L2666/02; Y; Y10; Y10S; Y10S156/00; Y10S156/91

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 205 words
A PROCESS FOR TREATING A REINFORCING ELEMENT OF A POLYESTER RESIN TO IMPROVE ITS ABILITY TO ADHERE TO A RUBBERY COMPOSITION WHICH COMPRISES TREATING THE REINFORCING ELEMENT WITH AN ADHESIVE COMPOSITION COMPRISING A DISPERSION OF APOLYEPOXIDE, THE COMPONENTS OF A HEATCONVERTIBLE PHENOL/ALDEHYDE RESIN, AND A DIENE RUBBER LATEX TO DEPOSIT ON SAID ELEMENT FROM ABOUT .5 TO ABOUT 10% SOLIDS OF SAID POLYEPOXIDE, AND FROM ABOUT 1% TO ABOUT 20% SOLIDS OF SAID RESIN AND RUBBER LATEX WHEREIN THE RATION OF RESIN TO RUBBER LATEX RANGES FROM 1/10 TO 2.5/10, HEATING THE ADHESIVE COMPOSITION AT A TEMPERATURE INSUFFICIENT TO CAUSE A SUBSTANTIAL REACTION OF THE COMPONENTS OF SAID ADHESIVE COMPOSITION BUT AT A TEMPERATURE SUFFICIENT TO SOLIDIFY THE ADHESIVE COMPOSITION, THE COMPONENTS REMAINING SUBSTANTIALLY UNREACTED BECAUSE OF THE ABSENCE OF AN EPOXY CURING AGENT, APPLYING A SECOND ADHESIVE COMPOSITION CONTAINING COMPONENTS INCLUDING A HEAT-CONVERTIBLE ALDEHYDE RESIN AND A RUBBER LATEX CHEMICALLY REACTIVE WITH THE CHEMICALLY REACTIVE COMPONENTS OF THE SAID FIRST ADHESIVE COMPOSITION TO THE REINFORCING ELEMENT AND THEN HEATING THE REINFORCING ELEMENT AT A TEMPERATURE FROM ABOUT 350*F. TO ABOUT 410*F. FOR FROM ABOUT 2 TO ABOUT 5 MINUTES IN ORDER TO CONVERT THE COMPONENTS OF BOTH ADHESIVE COMPOSITIONS INTO A HOMOGENEOUS RESINOUS MASS.
Claim 2
Dependent Claim 205 words
A PROCESS FOR TREATING A REINFORCING ELEMENT OF A POLYESTER RESIN TO IMPROVE ITS ABILITY TO ADHERE TO A RUBBERY COMPOSITION WHICH COMPRISES TREATING THE REINFORCING ELEMENT WITH AN ADHESIVE COMPOSITION COMPRISING A DISPERSION OF APOLYEPOXIDE, THE COMPONENTS OF A HEATCONVERTIBLE PHENOL/ALDEHYDE RESIN, AND A DIENE RUBBER LATEX TO DEPOSIT ON SAID ELEMENT FROM ABOUT .5 TO ABOUT 10% SOLIDS OF SAID POLYEPOXIDE, AND FROM ABOUT 1% TO ABOUT 20% SOLIDS OF SAID RESIN AND RUBBER LATEX WHEREIN THE RATION OF RESIN TO RUBBER LATEX RANGES FROM 1/10 TO 2.5/10, HEATING THE ADHESIVE COMPOSITION AT A TEMPERATURE INSUFFICIENT TO CAUSE A SUBSTANTIAL REACTION OF THE COMPONENTS OF SAID ADHESIVE COMPOSITION BUT AT A TEMPERATURE SUFFICIENT TO SOLIDIFY THE ADHESIVE COMPOSITION, THE COMPONENTS REMAINING SUBSTANTIALLY UNREACTED BECAUSE OF THE ABSENCE OF AN EPOXY CURING AGENT, APPLYING A SECOND ADHESIVE COMPOSITION CONTAINING COMPONENTS INCLUDING A HEAT-CONVERTIBLE ALDEHYDE RESIN AND A RUBBER LATEX CHEMICALLY REACTIVE WITH THE CHEMICALLY REACTIVE COMPONENTS OF THE SAID FIRST ADHESIVE COMPOSITION TO THE REINFORCING ELEMENT AND THEN HEATING THE REINFORCING ELEMENT AT A TEMPERATURE FROM ABOUT 350*F. TO ABOUT 410*F. FOR FROM ABOUT 2 TO ABOUT 5 MINUTES IN ORDER TO CONVERT THE COMPONENTS OF BOTH ADHESIVE COMPOSITIONS INTO A HOMOGENEOUS RESINOUS MASS.

References Cited (Backward Citations)

US2902398A Cited
US2978784A Cited
US3036948A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1968-06-21 1968-12-21 1969-06-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1972-06-21 1972-12-21 1973-06-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1976-06-21 1976-12-21 1977-06-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag