US3110704A Expired / Lapsed US ⏱️ 0.0 years remaining

Low pressure tetrafluoroethylene polymerization process

Assignee: EIDP Inc
•
Filing: 1960-03-31
•
Granted: 1963-11-12
•
Expires: 1980-03-31
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Halliwell Ronald Harry

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 17:01
CPC Classifications
C; C08; C08F; C08F114/00; C08F114/18; C08F114/26; Y; Y10; Y10S; Y10S526/00; Y10S526/915

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 46 words
A PROCESS FOR POLYMERRIZING TETRAFLUOROETHYLENE WHICH COMPRISES CONTACTING ETRAFLUOROETHYLENE AT A TEMPERATURE IN THE RANGE OF 30*C. TO 80*C. WITH AN AQUEOUS POLYMERIZATION MEDIUM CONTAINING AN INORGANIC REDOX INTIATOR SYSTEM AND COPPER ION ACCELERATOR, AT A PRESSURE IN THE RANGE OF 0.6 TO 4 ATMOSPHERES ABSOLUTE.
Claim 2
Dependent Claim 46 words
A PROCESS FOR POLYMERRIZING TETRAFLUOROETHYLENE WHICH COMPRISES CONTACTING ETRAFLUOROETHYLENE AT A TEMPERATURE IN THE RANGE OF 30*C. TO 80*C. WITH AN AQUEOUS POLYMERIZATION MEDIUM CONTAINING AN INORGANIC REDOX INTIATOR SYSTEM AND COPPER ION ACCELERATOR, AT A PRESSURE IN THE RANGE OF 0.6 TO 4 ATMOSPHERES ABSOLUTE.
Claim 3
Dependent Claim 75 words
A PROCESS FOR POLYMERIZING TETAFLUOROETHYLENE WHICH COMPRISES CONTACTING TETRAFLUOROETHYLENE AT A TEMPERATURE IN THE RANGE OF 30*C. TO 80*C. WITH AN AQUEOUS POLYMERIZATION MEDIUM CONTAINING, PERMILLION PARTS BY WEIGHT, 5 TO 180 PARTS PERSULFATE ION AND 10 TO 360 PARTS BISUFITE ION AS AN INORGANIC INIATOR, AND 0.02 TO 2 PARTS COPPER ION AND 1 TO 500 PARTS OF INERT HALOGENATED ORGANIC DISPERSING AGENT AS ACCELERATORS, UNDER A PRESSURE OF 0.6 TO 4 ATMOSPHERES ABSOLUTE.
Claim 4
Dependent Claim 75 words
A PROCESS FOR POLYMERIZING TETAFLUOROETHYLENE WHICH COMPRISES CONTACTING TETRAFLUOROETHYLENE AT A TEMPERATURE IN THE RANGE OF 30*C. TO 80*C. WITH AN AQUEOUS POLYMERIZATION MEDIUM CONTAINING, PERMILLION PARTS BY WEIGHT, 5 TO 180 PARTS PERSULFATE ION AND 10 TO 360 PARTS BISUFITE ION AS AN INORGANIC INIATOR, AND 0.02 TO 2 PARTS COPPER ION AND 1 TO 500 PARTS OF INERT HALOGENATED ORGANIC DISPERSING AGENT AS ACCELERATORS, UNDER A PRESSURE OF 0.6 TO 4 ATMOSPHERES ABSOLUTE.

References Cited (Backward Citations)

US2559752A Cited
US2820026A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1966-11-11 1967-05-13 1967-11-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1970-11-11 1971-05-13 1971-11-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1974-11-11 1975-05-13 1975-11-12 $7700.00 Window Closed / Lapsed