US3105867A Expired / Lapsed US ⏱️ 0.0 years remaining

Metal foil lead-in conductor for electric lamp

Assignee: US Philips Corp
•
Filing: 1960-09-08
•
Granted: 1963-10-01
•
Expires: 1980-09-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Riksterus Auguste Johannes Meijer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 23:46
CPC Classifications
C; C03; C03C; C03C27/00; C03C27/04; C03C27/042; C03C27/046; H; H01; H01J; H01J5/00; H01J5/32; H01J5/38

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 134 words
A LEAD-IN CONDUCTOR FOR AN ELECTRIC LAMP COMPRISING A FOIL SEALED IN A QUARTZ-LIKE MATERIAL, SAID FOIL HAVING A THICKNESS GREATER IN ITS MID-SECTION THAN AT ITS EDGES, SAID FOIL COMPRISING A CORE OF REFRACTORY METAL, AN OXIDATION-PROTECTIVE OUTER LAYER SURROUNDING SAID CORE, AND A LAYER INTERMEDIATE THE OUTER LAYER AND THE CORE CONSISTING OF A METAL WHICH IS CAPABLE OF FORMING AN ALLOY WITH THE CORE METAL AND WHICH IS CAPABLE OF FORMING A PROTECTIVE OXIDE, SAID CORE HAVING A THICKNESS AT ITS MID-SECTION OF BETWEEN 15 AND 70 MICRONS, THE OUTER LAYER HAVING A THICKNESS OF ABOUT 0.5 TO 4 MICRONS, AND THE INTERMEDIATE LAYER HAVING A THICKNESS OF ABOUT 1 TO 8 MICRONS, SAID OUTER LAYER HAVING A MELTING POINT WHICH IS LOWER THAN THE SOFTENING TEMPERATURE OF THE QUARTZ-LIKE MATERIAL.
Claim 2
Dependent Claim 134 words
A LEAD-IN CONDUCTOR FOR AN ELECTRIC LAMP COMPRISING A FOIL SEALED IN A QUARTZ-LIKE MATERIAL, SAID FOIL HAVING A THICKNESS GREATER IN ITS MID-SECTION THAN AT ITS EDGES, SAID FOIL COMPRISING A CORE OF REFRACTORY METAL, AN OXIDATION-PROTECTIVE OUTER LAYER SURROUNDING SAID CORE, AND A LAYER INTERMEDIATE THE OUTER LAYER AND THE CORE CONSISTING OF A METAL WHICH IS CAPABLE OF FORMING AN ALLOY WITH THE CORE METAL AND WHICH IS CAPABLE OF FORMING A PROTECTIVE OXIDE, SAID CORE HAVING A THICKNESS AT ITS MID-SECTION OF BETWEEN 15 AND 70 MICRONS, THE OUTER LAYER HAVING A THICKNESS OF ABOUT 0.5 TO 4 MICRONS, AND THE INTERMEDIATE LAYER HAVING A THICKNESS OF ABOUT 1 TO 8 MICRONS, SAID OUTER LAYER HAVING A MELTING POINT WHICH IS LOWER THAN THE SOFTENING TEMPERATURE OF THE QUARTZ-LIKE MATERIAL.

References Cited (Backward Citations)

US2876377A Cited
US2966607A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1966-09-30 1967-04-01 1967-10-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1970-09-30 1971-04-01 1971-10-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1974-09-30 1975-04-01 1975-10-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag