Patent US3098739A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3098739A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for refining metals

Assignee: Huettenwerk Oberhausen AG
•
Filing: 1960-11-04
•
Granted: 1963-07-23
•
Expires: 1980-11-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Graef Rudolf
  • 👤 Bogdandy Ludwig Von

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 16:06
CPC Classifications
C; C21; C21C; C21C5/00; C21C5/56; C21C5/28; C21C5/30; C21C5/32; F; F27; F27B; F27B7/00; F27B7/20; F27B7/2083

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 182 words
IN A METHOD OF REFINING CARBON CONTAINING PIG IRON IN THE PRESENCE OF AN OXYGEN CONTAINING ATMOSPHERE IN A DRUM FURNACE ROTATABLE ABOUT A SUBSTANTIALLY HORIZONTAL AXIS AND ADAPTED TO RETAIN PIG IRON TO BE REFINED THROUGHOUT THE REFINING PROCESS, THE EMPLOYMENT OF THE FOLLOWING STEPS; FORMING A LIQUID SLAG LAYER, FEEDING IN SUCCESSION NEW QUANTITTIES OF SLAG FORMERS INTO SAID DRUM FURNACE AT ONE PORTION THEREOF WHILE THE REFINING PROCESS IS BEING CARRIED OUT, AND DURING SAID REFINING PROCESS, CORRESPONDING TO THE FEEDING OF NEW SLAG FORMERS INTO SAID DRUM FURNACE AND AT THE SAME RATE THEREOF AT AOTHER DRUM FURNACE PORTION SPACED FROM SAID FIRST DRUM FURNACE PORTION WITHDRAWING SLAG FROM THE SLAG LAYER FORMING ON THE PIG IRON BATH IN SAID DRUM FURNACE WHILE MAINTAINING THE SLAG LAYER FORMING ON THE PIG IRON BATH AT A DESIRED THINNESS WHEREBY THE AREA OF CONTACT OF SAID SLAG WITH THE FURNACE LINING IS REDUCED, AND WHILE RETAINING THE PIG IRON BATH IN SAID DRUM FURNACE UNTIL THE DESIRED REFINING OF SAID PIG IRON BATH IN SAID DRUM FURNACE HAS BEEN COMPLETED.
Claim 2
Dependent Claim 182 words
IN A METHOD OF REFINING CARBON CONTAINING PIG IRON IN THE PRESENCE OF AN OXYGEN CONTAINING ATMOSPHERE IN A DRUM FURNACE ROTATABLE ABOUT A SUBSTANTIALLY HORIZONTAL AXIS AND ADAPTED TO RETAIN PIG IRON TO BE REFINED THROUGHOUT THE REFINING PROCESS, THE EMPLOYMENT OF THE FOLLOWING STEPS; FORMING A LIQUID SLAG LAYER, FEEDING IN SUCCESSION NEW QUANTITTIES OF SLAG FORMERS INTO SAID DRUM FURNACE AT ONE PORTION THEREOF WHILE THE REFINING PROCESS IS BEING CARRIED OUT, AND DURING SAID REFINING PROCESS, CORRESPONDING TO THE FEEDING OF NEW SLAG FORMERS INTO SAID DRUM FURNACE AND AT THE SAME RATE THEREOF AT AOTHER DRUM FURNACE PORTION SPACED FROM SAID FIRST DRUM FURNACE PORTION WITHDRAWING SLAG FROM THE SLAG LAYER FORMING ON THE PIG IRON BATH IN SAID DRUM FURNACE WHILE MAINTAINING THE SLAG LAYER FORMING ON THE PIG IRON BATH AT A DESIRED THINNESS WHEREBY THE AREA OF CONTACT OF SAID SLAG WITH THE FURNACE LINING IS REDUCED, AND WHILE RETAINING THE PIG IRON BATH IN SAID DRUM FURNACE UNTIL THE DESIRED REFINING OF SAID PIG IRON BATH IN SAID DRUM FURNACE HAS BEEN COMPLETED.

References Cited (Backward Citations)

US1320483A Cited
US1328803A Cited
US2622977A Cited
US2918365A Cited
US2902358A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1966-07-22 1967-01-21 1967-07-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1970-07-22 1971-01-21 1971-07-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1974-07-22 1975-01-21 1975-07-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag