Method of vulcanizing butyl rubber, halosulfonated polyethylene, and nmethyl-n-nitroso-p-nitrosoaniline composition and resulting vulcanizate

Assignee: ExxonMobil Technology and Engineering Co
•
Filing: 1959-07-31
•
Granted: 1963-03-12
•
Expires: 1979-07-31
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 David R Hammel
  • 👤 Conrad J Jankowski

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 09:46
CPC Classifications
C; C08; C08L; C08L23/00; C08L23/02; C08L23/18; C08L23/20; C08L23/22

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 99 words
A METHOD OF PRODUCING A VULCANIZATE WITH INCREASED RESISTANCE TO WEAR AND IMPROVED RECOVERY AFTER INDENTATION WHICH COMPRISES: (A) COMPOUNDING 100 PARTS OF BUTYL RUBBER COPOLYMER SAID COPOLYMER COMPRISING 70 TO 99.5 PARTS BY WEIGHT OF A C4 TO C7 ISOOLEFIN AND 30 TO 0.5 PARTS BY WEIGHT OF A MULTIOFIN SELECTED FROM THE GROUP CONSULFONATED POLYOLEFIN SELECTED FROM THE GROUP CONSISTING OF CHLOROSULFONATED POLYETHYLENE AND BROMOSULFONATED POLYETHYLENE, AND 0.12 TO 4 PARTS OF NMETHYL-N-NITROSO-P-NITROSO ANILINE; AND (B) CURING SAID COMPOUNDED RUBBER COPOLYMER IN A MOLD AT A TEMPERATURE BETWEEN 137*C. AND 183*C. FOR ONE MINUTE TO FOUR HOURS.
Claim 2
Independent Claim 99 words
A METHOD OF PRODUCING A VULCANIZATE WITH INCREASED RESISTANCE TO WEAR AND IMPROVED RECOVERY AFTER INDENTATION WHICH COMPRISES: (A) COMPOUNDING 100 PARTS OF BUTYL RUBBER COPOLYMER SAID COPOLYMER COMPRISING 70 TO 99.5 PARTS BY WEIGHT OF A C4 TO C7 ISOOLEFIN AND 30 TO 0.5 PARTS BY WEIGHT OF A MULTIOFIN SELECTED FROM THE GROUP CONSULFONATED POLYOLEFIN SELECTED FROM THE GROUP CONSISTING OF CHLOROSULFONATED POLYETHYLENE AND BROMOSULFONATED POLYETHYLENE, AND 0.12 TO 4 PARTS OF NMETHYL-N-NITROSO-P-NITROSO ANILINE; AND (B) CURING SAID COMPOUNDED RUBBER COPOLYMER IN A MOLD AT A TEMPERATURE BETWEEN 137*C. AND 183*C. FOR ONE MINUTE TO FOUR HOURS.

References Cited (Backward Citations)

US2729608A Cited
US2683103A Cited
US2749323A Cited
US2874743A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1966-03-11 1966-09-10 1967-03-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1970-03-11 1970-09-10 1971-03-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1974-03-11 1974-09-10 1975-03-12 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag