Refractory practices

Assignee: Harbison Walker Refractories Co
•
Filing: 1961-04-07
•
Granted: 1962-12-25
•
Expires: 1981-04-07
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Davies Ben
  • 👤 Ernest P Weaver

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 09:57
CPC Classifications
C; C04; C04B; C04B35/00; C04B35/01; C04B35/013; C10; C10C; C10C1/00; C10C1/005; Y; Y10; Y10S; Y10S264/00; Y10S264/36

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 124 words
A METHOD OF FORMING SLAG-RESISTANT PITCH BONDED BASIC REFRACTORY BRICK COMPRISING A PITCH, HAVING A SOFTENING RANGE OF ABOUT 15/* TO 250*F., TO A TEMPERATURE ABOUE ITS SOFTENING POINT, PROVIDING A REFRACTORY AGGREGATE BATCH OF GRAIN OF AT LEAST ONE MEMBER SELECTED FROM THE GROUP CONSISTING OF DEAD BURNED LIME, DEAD BURNED DOLOMITE AND DEAD BURNED MAGNESIA MIXING SAID REFRACTORY AGGREGATE AND ABOUT 3 TO 8 WEIGHT PERCENT, BASED ON THE WEIGHT OF SAID AGGREGATE, OF SAID LIQUEFIED PITCH THEN INCORPORATING IN THE RESULTING MIXTURE ABOUT 2 TO 12 WEIGHT PERCENT, BASED ON THE WEIGHT OF SAID REFRACTORY AGGREGATE, OF A SOLID, POWDERED PITCH HAVING A SOFTENING POINT IN THE TEMPERATURE RANGE OF ABOUT 275* TO 450*F., AND PRESSING BRICK FROM THE RESULTING BATCH.
Claim 2
Independent Claim 124 words
A METHOD OF FORMING SLAG-RESISTANT PITCH BONDED BASIC REFRACTORY BRICK COMPRISING A PITCH, HAVING A SOFTENING RANGE OF ABOUT 15/* TO 250*F., TO A TEMPERATURE ABOUE ITS SOFTENING POINT, PROVIDING A REFRACTORY AGGREGATE BATCH OF GRAIN OF AT LEAST ONE MEMBER SELECTED FROM THE GROUP CONSISTING OF DEAD BURNED LIME, DEAD BURNED DOLOMITE AND DEAD BURNED MAGNESIA MIXING SAID REFRACTORY AGGREGATE AND ABOUT 3 TO 8 WEIGHT PERCENT, BASED ON THE WEIGHT OF SAID AGGREGATE, OF SAID LIQUEFIED PITCH THEN INCORPORATING IN THE RESULTING MIXTURE ABOUT 2 TO 12 WEIGHT PERCENT, BASED ON THE WEIGHT OF SAID REFRACTORY AGGREGATE, OF A SOLID, POWDERED PITCH HAVING A SOFTENING POINT IN THE TEMPERATURE RANGE OF ABOUT 275* TO 450*F., AND PRESSING BRICK FROM THE RESULTING BATCH.

References Cited (Backward Citations)

US3015850A Cited
US2640759A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1965-12-24 1966-06-25 1966-12-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1969-12-24 1970-06-25 1970-12-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1973-12-24 1974-06-25 1974-12-25 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag