Method of coating metal on dielectric material

Assignee: Mycalex Corp of America
•
Filing: 1960-04-04
•
Granted: 1962-02-06
•
Expires: 1980-04-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 William E Rowe

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 23:46
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/004; G03F7/04; H; H05; H05K; H05K3/00; H05K3/02; H05K3/04; H05K2203/00; H05K2203/11; H05K2203/1105; Y; Y10; Y10S; Y10S430/00; Y10S430/136

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 171 words
THE METHOD OF COATING A METAL ON A PREDETERMINED PORTION OF THE SURFCE OF A DIELECTRIC MATERIAL, COMPRISING THE STEPS OF COATING SAID SURFACE WITH A LIQUID SILVER SUSPENSION, BAKING SAID SUSPENSION AT ABOUT 400*F. FOR ABOUT THIRTY MINUTES TO DRIVE OFF THE LIQUID FROM SAID SUSPENSION AND TO CAUSE SAID SILVER TO BOND TO SAID SURFACE, COATING SAID SILVER WITH A LIGHT SENSITIVE HEAT SHRINK ABLE SOLUTION CONSISTING ESSENTIALLY OF 16 OUNCES OF COMMERCIAL FISH GLUE, 3 OUNCES OF A 20, SOLUTION OF AMMONIUM DICHROMATE- 10 DROPS OF CONCENTRATED AMMONIA AND 1 GALON OF WATER, BAKING SAID SOLUTION AT ABOUT 100*F. UNTIL IT DRIES,DISPOSING A NEGATIVE OVER SAID DRIED SOLUTION, ILLUMINATING SAID NEGATIVE TO EXPOSE A PORTION OF SAID LIGHT SENSITIVE MATERIAL,DEVELOPING SAID LIGHT SENSITIVE MATERIAL IN WATER TO WASH AWAY THE EXPOSED PORTION THEREOF, AND BAKING THE REMAINING PORTION OF SAID LIGHT SENSITIVE MATERIAL AT ABOUT 400*F. FOR ABOUT THIRTY MINUTES TO CAUSE SAID MATERIAL TO SHRINK AND PULL THE UNDERLYING SILVER OFF SAID SURFACE OF SAID DIELECTRIC MATERIAL.
Claim 2
Independent Claim 171 words
THE METHOD OF COATING A METAL ON A PREDETERMINED PORTION OF THE SURFCE OF A DIELECTRIC MATERIAL, COMPRISING THE STEPS OF COATING SAID SURFACE WITH A LIQUID SILVER SUSPENSION, BAKING SAID SUSPENSION AT ABOUT 400*F. FOR ABOUT THIRTY MINUTES TO DRIVE OFF THE LIQUID FROM SAID SUSPENSION AND TO CAUSE SAID SILVER TO BOND TO SAID SURFACE, COATING SAID SILVER WITH A LIGHT SENSITIVE HEAT SHRINK ABLE SOLUTION CONSISTING ESSENTIALLY OF 16 OUNCES OF COMMERCIAL FISH GLUE, 3 OUNCES OF A 20, SOLUTION OF AMMONIUM DICHROMATE- 10 DROPS OF CONCENTRATED AMMONIA AND 1 GALON OF WATER, BAKING SAID SOLUTION AT ABOUT 100*F. UNTIL IT DRIES,DISPOSING A NEGATIVE OVER SAID DRIED SOLUTION, ILLUMINATING SAID NEGATIVE TO EXPOSE A PORTION OF SAID LIGHT SENSITIVE MATERIAL,DEVELOPING SAID LIGHT SENSITIVE MATERIAL IN WATER TO WASH AWAY THE EXPOSED PORTION THEREOF, AND BAKING THE REMAINING PORTION OF SAID LIGHT SENSITIVE MATERIAL AT ABOUT 400*F. FOR ABOUT THIRTY MINUTES TO CAUSE SAID MATERIAL TO SHRINK AND PULL THE UNDERLYING SILVER OFF SAID SURFACE OF SAID DIELECTRIC MATERIAL.

References Cited (Backward Citations)

US237112A Cited
US775818A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1965-02-05 1965-08-07 1966-02-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1969-02-05 1969-08-07 1970-02-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1973-02-05 1973-08-07 1974-02-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag