Copolymers of methyl methacrylate possessing good elongation values

Assignee: Dow Chemical Co
•
Filing: 1953-08-24
•
Granted: 1961-03-07
•
Expires: 1973-08-24
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 John L Lang
  • 👤 Jones Clifford
  • 👤 Arthur F Roche
  • 👤 Frank L Ingley

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 13:42
CPC Classifications
C; C08; C08F; C08F220/00; C08F220/02; C08F220/10; C08F220/12; C08F220/14; C08F212/00; C08F212/02; C08F212/04; C08F212/06; C08F212/08; C08F212/10; C08F220/42; C08F220/44

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 118 words
A METHOD OF MAKING A THERMOPLASTIC, MOLDABLE COPOLYMER, CHARACTERIZED BY AN ULTIMATE ELONGATION OF MORE THAN 10 PERCENT, WHICH COMPRISES COPOLYMERIZING AT LEAST THE FIRST TWO OF THE MONOMERIC COMPOUNDS METHYL METHACRYLATE, ACRYLONITRILE AND STYRENE, IN ONE OF THE PROPORTIONS REPRESENTED BY POINTS FALLING WITHIN AND ON THE PERIMETER OF AREA A ON THE ANNEXED DRAWING, BY HEATING A HOMOGENEOUS LIQUID POLYMERIZATION MIXTURE CONSISTING ESSENTIALLY OF SUCH MONOMERIC COMPOUNDS AND THE COPOLYMER PRODUCT OF POLYMERIZATION THEREOF AT A POLYMERIZATION TEMPERATURE BETWEEN ABOUT 130*C. AND ABOUT 155*C., THE PROPORTION OF COPOLYMER PRODUCT BEING FROM 10 TO 50 PERCENT BY WEIGHT OF THE POLYMERIZATION MIXTURE, MAINTAINING THE PROPORTIONS OF MONOMERIC COMPOUNDS AND THE PORTION OF COPOLYMER PRODUCT IN THE POLY-
Claim 2
Independent Claim 118 words
A METHOD OF MAKING A THERMOPLASTIC, MOLDABLE COPOLYMER, CHARACTERIZED BY AN ULTIMATE ELONGATION OF MORE THAN 10 PERCENT, WHICH COMPRISES COPOLYMERIZING AT LEAST THE FIRST TWO OF THE MONOMERIC COMPOUNDS METHYL METHACRYLATE, ACRYLONITRILE AND STYRENE, IN ONE OF THE PROPORTIONS REPRESENTED BY POINTS FALLING WITHIN AND ON THE PERIMETER OF AREA A ON THE ANNEXED DRAWING, BY HEATING A HOMOGENEOUS LIQUID POLYMERIZATION MIXTURE CONSISTING ESSENTIALLY OF SUCH MONOMERIC COMPOUNDS AND THE COPOLYMER PRODUCT OF POLYMERIZATION THEREOF AT A POLYMERIZATION TEMPERATURE BETWEEN ABOUT 130*C. AND ABOUT 155*C., THE PROPORTION OF COPOLYMER PRODUCT BEING FROM 10 TO 50 PERCENT BY WEIGHT OF THE POLYMERIZATION MIXTURE, MAINTAINING THE PROPORTIONS OF MONOMERIC COMPOUNDS AND THE PORTION OF COPOLYMER PRODUCT IN THE POLY-

References Cited (Backward Citations)

US2123599A Cited
US1933052A Cited
US2117321A Cited
US2160054A Cited
US2412034A Cited
US2486241A Cited
US2417293A Cited
US2537031A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1964-03-06 1964-09-05 1965-03-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1968-03-06 1968-09-05 1969-03-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1972-03-06 1972-09-05 1973-03-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag