Abstract

No abstract record available.

Inventors

  • 👤 William J Dennis

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 11:24
CPC Classifications
D; D04; D04H; D04H1/00; D04H1/40; D04H1/42; D04H1/4209; D04H1/4218; B; B29; B29B; B29B15/00; B29B15/08; B29B15/10; B29B15/12; B29C; B29C70/00; B29C70/04; B29C70/28; B29C70/40; B29C70/50; D04H1/58; D04H1/587; D04H1/64; D04H1/655; B29K; B29K2025/00; B29K2067/00; B29K2067/06; B29K2105/00; B29K2105/06; B29K2105/08; B29K2105/0854

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 164 words
A METHOD OF MANUFACTURING A MAT OF FILIFORM MATERAIL WHICH COMPRISES INITIMATELY MIXING SUCH MATERIAL AND A FIRST DRY SOLID BINDER, FORMING SUCH MIXTURE INTO THE FORM OF A MAT, SPRAYING AT LEAST ONE SURFACE OF SAID MAT WITH A RELATIVELY VOLATILE LIQUID SUFFICIENTLY GENTLY TO AVOID PENETRATION OF SAID LIQUID INTO THE INTERIOR OF THE MAT, SO THAT SAID RELATIVELY VOLATILE LIQUID LIES AT SAID SURFACE OF SAID MAT, THEN SPRAYING SAID SURFACE OF THE MAT WITH A SECOND DRY SOLID BINDER, THE PRESENCE OF SAID RELATIVELY VOLATILE LIQUID AT THE SURFACE OF THE MAT SERVING TO MINIMIZE PENETRATION OF SAID SECOND DRY SOLID BINDER INTO THE INTERIOR OF THE MAT, THEREBY PRODUCING A HIGHER PROPORTION OF BINDER AT SAID SURFACE THAN IN THE INTERIOR OF THE MAT, AND FINALLY EFFECTING EVAPORATION OF SAID LIQUID AND SETTING OF BOTH SAID BINDERS TO PRODUCE A MAT HAVING AT SAID SURFACE A SURFACE LAYER WHICH IS MORE STRONGLY BONDED THAN THE INTERIOR OF THE MAT.
Claim 2
Independent Claim 164 words
A METHOD OF MANUFACTURING A MAT OF FILIFORM MATERAIL WHICH COMPRISES INITIMATELY MIXING SUCH MATERIAL AND A FIRST DRY SOLID BINDER, FORMING SUCH MIXTURE INTO THE FORM OF A MAT, SPRAYING AT LEAST ONE SURFACE OF SAID MAT WITH A RELATIVELY VOLATILE LIQUID SUFFICIENTLY GENTLY TO AVOID PENETRATION OF SAID LIQUID INTO THE INTERIOR OF THE MAT, SO THAT SAID RELATIVELY VOLATILE LIQUID LIES AT SAID SURFACE OF SAID MAT, THEN SPRAYING SAID SURFACE OF THE MAT WITH A SECOND DRY SOLID BINDER, THE PRESENCE OF SAID RELATIVELY VOLATILE LIQUID AT THE SURFACE OF THE MAT SERVING TO MINIMIZE PENETRATION OF SAID SECOND DRY SOLID BINDER INTO THE INTERIOR OF THE MAT, THEREBY PRODUCING A HIGHER PROPORTION OF BINDER AT SAID SURFACE THAN IN THE INTERIOR OF THE MAT, AND FINALLY EFFECTING EVAPORATION OF SAID LIQUID AND SETTING OF BOTH SAID BINDERS TO PRODUCE A MAT HAVING AT SAID SURFACE A SURFACE LAYER WHICH IS MORE STRONGLY BONDED THAN THE INTERIOR OF THE MAT.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1963-11-22 1964-05-23 1964-11-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1967-11-22 1968-05-23 1968-11-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1971-11-22 1972-05-23 1972-11-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag