Dry alkali chlorotitanates and method of making the same
Assignee: IIT Research Institute
•
Filing: 1957-02-08
•
Granted: 1958-10-21
•
Expires: 1977-02-08
Abstract
No abstract record available.
Inventors
- 👤 Fredric V Schossberger
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-07 08:20
CPC Classifications
C; C01; C01G; C01G23/00; C01G23/003; C01G23/002; C22; C22B; C22B34/00; C22B34/10; C22B34/12; C01P; C01P2006/00; C01P2006/80; C01P2006/82
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
134 words
THE METHOD OF MAKING A MATERIAL SELECTED FROM THE GROUP COMPRISING DRY ALKALI METAL CHLOROTITANATES AND AMMONIUM CHLOROTITANATE FROM TITANIUM-BEARING MATERIALS COMPRISING THE STEPS OF: MIXING SAID MATERIAL WITH AN ACID SELECTED FROM THE GROUP CONSISTING OF SULFURIC AND A MIXTURE OF HYDROCHLORIC AND SULFURIC TO FORM A TITANIUM SOLUTION; SEPARATING SAID TITANIUM SOLUTION FROM THE UNDISSOLVED MATERIALS THEREIN; TREATING SAID TITANIUM SOLUTION WITH HYDROGEN CHLORIDE GAS; ADDING A MATERIAL SELECTED FROM THE GROUP CONSISTING OF ALKALI METAL CHLORIDES AND AMMONIUM CHLORIDE WHEREBY A MATERIAL SELECTED FROM THE CLASS CONSISTING OF ALKALI METAL CHLOROTITANATE AND AMMONIUM CHLOROTITANATE IS PRECIPITATED; SEPARATING SAID PRECIPITATED CHLOROTITANATE FROM THE SUPERNATANT SOLUTION AND DRYING SAID CHLOROTITANATE TO LESS THAN 0.03% MOISTURE RETENTION BY PASSING HYDROGEN CHLORIDE GAS THERETHROUGH WHILE MAINTAINING SAID CHLOROTITANATE AT A TEMPERATURE 20* TO 300* CENTIGRADE.
Claim 2
Independent Claim
134 words
THE METHOD OF MAKING A MATERIAL SELECTED FROM THE GROUP COMPRISING DRY ALKALI METAL CHLOROTITANATES AND AMMONIUM CHLOROTITANATE FROM TITANIUM-BEARING MATERIALS COMPRISING THE STEPS OF: MIXING SAID MATERIAL WITH AN ACID SELECTED FROM THE GROUP CONSISTING OF SULFURIC AND A MIXTURE OF HYDROCHLORIC AND SULFURIC TO FORM A TITANIUM SOLUTION; SEPARATING SAID TITANIUM SOLUTION FROM THE UNDISSOLVED MATERIALS THEREIN; TREATING SAID TITANIUM SOLUTION WITH HYDROGEN CHLORIDE GAS; ADDING A MATERIAL SELECTED FROM THE GROUP CONSISTING OF ALKALI METAL CHLORIDES AND AMMONIUM CHLORIDE WHEREBY A MATERIAL SELECTED FROM THE CLASS CONSISTING OF ALKALI METAL CHLOROTITANATE AND AMMONIUM CHLOROTITANATE IS PRECIPITATED; SEPARATING SAID PRECIPITATED CHLOROTITANATE FROM THE SUPERNATANT SOLUTION AND DRYING SAID CHLOROTITANATE TO LESS THAN 0.03% MOISTURE RETENTION BY PASSING HYDROGEN CHLORIDE GAS THERETHROUGH WHILE MAINTAINING SAID CHLOROTITANATE AT A TEMPERATURE 20* TO 300* CENTIGRADE.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1961-10-20 | 1962-04-21 | 1962-10-21 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1965-10-20 | 1966-04-21 | 1966-10-21 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1969-10-20 | 1970-04-21 | 1970-10-21 | $7700.00 | Window Closed / Lapsed |