Patent US2726951A successfully refreshed from Google Patents.
← Back to Patent Explorer
US2726951A Expired / Lapsed US ⏱️ 0.0 years remaining

Process of producing metal powder from metal carbonyl

Assignee: Huntington Alloys Corp
•
Filing: 1952-07-29
•
Granted: 1955-12-13
•
Expires: 1972-07-29
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Ramsay Alexander Gray
  • 👤 Albert E Wallis

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 17:41
CPC Classifications
B; B22; B22F; B22F9/00; B22F9/16; B22F9/30; B22F9/305

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 165 words
IN A PROCESS FOR PRODUCING METAL POWDER CHARACTERIZED BY A FIBROUS AND HAIR-LIKE STRUCTURE AND A BULK DENSITY OF ABOUT 0.3 TO 1.3 GRAMS PER CUBIC CENTIMETER BY DECOMPOSING METAL CARBONYL VAPOR, THE STEPS CONPRISING DIRECTING A STREAM OF METAL CARBONYL VAPOR OF AT LEAST 65* CONCENTRATION ADJACENT A HEATED SURFACE MAINTAINED AT AN ELEVATED DECOMPOSITION TEMPERATURE OF NOT MORE THAN ABOUT 400* C. WHILE MAINTAINING SAID VAPOR AT A FLOW RATE EQUIVALENT TO ABOUT 4 TO 10 LITRES OF LIQUID CARBONYL PER HOUR PER FOOT OF THE PERIMETER OF THE HEATED SURFACE CROSS SECTION, AND CAUSING SAID STREAM TO FLOW SUBSTANTIALLY LONGITUDINALLY ALONG SAID HEATED SURFACE WHILE CONTROLLING THE FLOW OF SAID STREAM DURING AT LEAST THE INITIAL PART OF THE DECOMPOSITION SO THAT THE VAPOR STREAM IS NOT MORE THAN 15 INCHES FROM A HEATED SURFACE AND SO THAT THE CROSS-SECTIONAL AREA OF SAID STREAM IS AT LEAST FIVE SQUARE FEET AND THE CROSS SECTION OF SAID STREAM IS OF SUBSTANTIALLY ELONGATED CONFIGURATION.
Claim 2
Dependent Claim 165 words
IN A PROCESS FOR PRODUCING METAL POWDER CHARACTERIZED BY A FIBROUS AND HAIR-LIKE STRUCTURE AND A BULK DENSITY OF ABOUT 0.3 TO 1.3 GRAMS PER CUBIC CENTIMETER BY DECOMPOSING METAL CARBONYL VAPOR, THE STEPS CONPRISING DIRECTING A STREAM OF METAL CARBONYL VAPOR OF AT LEAST 65* CONCENTRATION ADJACENT A HEATED SURFACE MAINTAINED AT AN ELEVATED DECOMPOSITION TEMPERATURE OF NOT MORE THAN ABOUT 400* C. WHILE MAINTAINING SAID VAPOR AT A FLOW RATE EQUIVALENT TO ABOUT 4 TO 10 LITRES OF LIQUID CARBONYL PER HOUR PER FOOT OF THE PERIMETER OF THE HEATED SURFACE CROSS SECTION, AND CAUSING SAID STREAM TO FLOW SUBSTANTIALLY LONGITUDINALLY ALONG SAID HEATED SURFACE WHILE CONTROLLING THE FLOW OF SAID STREAM DURING AT LEAST THE INITIAL PART OF THE DECOMPOSITION SO THAT THE VAPOR STREAM IS NOT MORE THAN 15 INCHES FROM A HEATED SURFACE AND SO THAT THE CROSS-SECTIONAL AREA OF SAID STREAM IS AT LEAST FIVE SQUARE FEET AND THE CROSS SECTION OF SAID STREAM IS OF SUBSTANTIALLY ELONGATED CONFIGURATION.

References Cited (Backward Citations)

US455228A Cited
US551220A Cited
US1836732A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1958-12-12 1959-06-13 1959-12-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1962-12-12 1963-06-13 1963-12-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1966-12-12 1967-06-13 1967-12-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag