Low-temperature reduction of nickel chloride

Assignee: Crowley-Republic Steel Corp
•
Filing: 1950-05-23
•
Granted: 1953-06-16
•
Expires: 1970-05-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Edward A Beidler

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 09:54
CPC Classifications
C; C22; C22B; C22B23/00; C22B23/02; C22B23/021; B; B01; B01J; B01J23/00; B01J23/70

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 120 words
THE PROCESS OF INITIATING THE REDUCTION OF SOLID NICKEL CHLORIDE (NICL2) WITH HYDROGEN BY A DRY GAS-TO-SOLID REACTION TO FORM METALLIC NICKEL IN A TEMPERATURE RANGE IN WHICH HYDROGEN AND NICL2 WILL NOT COMMENCE TO REACT TOGETHER TO ANY SUBSTANTIAL EXTENT IN THE ABSENCE OF A REACTIONINTIATING CATALYST, COMPRISING THE STEPS OF CONTACTING DRY SOLID NICL2, WHICH IS SUBSTANTIALLY FREE OF METALLIC NICKEL, WITH A GAS CONTAINING HYDROGEN AS ITS ESSENTIAL ACTIVE REDUCING INGREDIENT, WHILE MAINTAINING SAID NICL2 IN THE TEMPERATURE RANGE OF ABOUT 475* F. TO ABOUT 650* F. AND CAUSING THE REACTION TO START BY PROVIDING IN CONTACT WITH THE NICL2 AT LEAST ABOUT 0.1% (BY WEIGHT BASED UPON THE NICL2) OF METALLIC NICKEL AS A REACTION-INITIATING CATALYST.
Claim 2
Dependent Claim 120 words
THE PROCESS OF INITIATING THE REDUCTION OF SOLID NICKEL CHLORIDE (NICL2) WITH HYDROGEN BY A DRY GAS-TO-SOLID REACTION TO FORM METALLIC NICKEL IN A TEMPERATURE RANGE IN WHICH HYDROGEN AND NICL2 WILL NOT COMMENCE TO REACT TOGETHER TO ANY SUBSTANTIAL EXTENT IN THE ABSENCE OF A REACTIONINTIATING CATALYST, COMPRISING THE STEPS OF CONTACTING DRY SOLID NICL2, WHICH IS SUBSTANTIALLY FREE OF METALLIC NICKEL, WITH A GAS CONTAINING HYDROGEN AS ITS ESSENTIAL ACTIVE REDUCING INGREDIENT, WHILE MAINTAINING SAID NICL2 IN THE TEMPERATURE RANGE OF ABOUT 475* F. TO ABOUT 650* F. AND CAUSING THE REACTION TO START BY PROVIDING IN CONTACT WITH THE NICL2 AT LEAST ABOUT 0.1% (BY WEIGHT BASED UPON THE NICL2) OF METALLIC NICKEL AS A REACTION-INITIATING CATALYST.

References Cited (Backward Citations)

US1373654A Cited
US1783662A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1956-06-15 1956-12-15 1957-06-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1960-06-15 1960-12-15 1961-06-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1964-06-15 1964-12-15 1965-06-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag