Process of applying promoters to catalyst particles

Assignee: Standard Oil Co
•
Filing: 1947-12-05
•
Granted: 1950-03-14
•
Expires: 1967-12-05
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Voorhees Vanderveer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 05:46
CPC Classifications
B; B01; B01J; B01J23/00; B01J23/70; B01J23/76

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 140 words
THE PROCESS OF MAKING A FINELY DIVIDED IRON CATALYST CONTAINING AN AVERAGE CONCENTRATION OF PROMOTER SELECTED FROM THE CLASS CONSISTING OF ALKALI AND ALKALINE EARTH METAL COMPOUNDS OF BETWEEN ABOUT .1 AND ABOUT 2.5%, WHICH COMPRISES THE STEPS OF CLASSIFYING THE FINELY DIVIDED IRON CATALYST INTO RELATIVELY FINE AND RELATIVELY COARSE PARTICLES, APPLYING A RELATIVELY DILUTE SOLUTION OF PROMOTOR TO THE SURFACE OF THE RELATIVELY FINE CATAYST PARTICLES, APPLYING A RELATIVELY STRONG SOLUTION OF PROMOTOR TO THE SURFACE OF THE RELATIVELY COARSE CATALYST PARTICLES, THE CONCENTRATION OF SOLUTION OF PROMOTOR BEING CORRELATED WITH THE WEIGHT OF THE IRON PARTICLES IN A DIRECT PROPORTION RELATIONSHIP, SEPARATELY DRYING THE TWO SIZES OF PROMOTED CATALYST, AND RECOMBINING TO PRODUCE A FLUIDIZABLE MIXTURE OF FINELY DIVIDED IRON CATALYST HAVING A UNIFORM PROPORTION OF PROMOTOR IN EACH SIZE RANGE BASED UPON THE WEIGHT OF CATALYST.
Claim 2
Dependent Claim 140 words
THE PROCESS OF MAKING A FINELY DIVIDED IRON CATALYST CONTAINING AN AVERAGE CONCENTRATION OF PROMOTER SELECTED FROM THE CLASS CONSISTING OF ALKALI AND ALKALINE EARTH METAL COMPOUNDS OF BETWEEN ABOUT .1 AND ABOUT 2.5%, WHICH COMPRISES THE STEPS OF CLASSIFYING THE FINELY DIVIDED IRON CATALYST INTO RELATIVELY FINE AND RELATIVELY COARSE PARTICLES, APPLYING A RELATIVELY DILUTE SOLUTION OF PROMOTOR TO THE SURFACE OF THE RELATIVELY FINE CATAYST PARTICLES, APPLYING A RELATIVELY STRONG SOLUTION OF PROMOTOR TO THE SURFACE OF THE RELATIVELY COARSE CATALYST PARTICLES, THE CONCENTRATION OF SOLUTION OF PROMOTOR BEING CORRELATED WITH THE WEIGHT OF THE IRON PARTICLES IN A DIRECT PROPORTION RELATIONSHIP, SEPARATELY DRYING THE TWO SIZES OF PROMOTED CATALYST, AND RECOMBINING TO PRODUCE A FLUIDIZABLE MIXTURE OF FINELY DIVIDED IRON CATALYST HAVING A UNIFORM PROPORTION OF PROMOTOR IN EACH SIZE RANGE BASED UPON THE WEIGHT OF CATALYST.

References Cited (Backward Citations)

US1148570A Cited
US2254806A Cited
US2276693A Cited
US2417164A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1953-03-13 1953-09-12 1954-03-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1957-03-13 1957-09-12 1958-03-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1961-03-13 1961-09-12 1962-03-14 $7700.00 Window Closed / Lapsed