Production of fine gold particles
Abstract
Abstract PURPOSE: To produce singly dispersed fine gold particles having a narrow particle size distribution by adding an amphoteric surfactant to an aq. soln. contg. iodoauric acid ions and by further adding alkali hydroxide to the aq. soln. to decompose gold iodide. CONSTITUTION: An amphoteric surfactant such as acrylic acid amine is added to an aq. soln. contg. iodoauric acid ions prepd. by dissolving gold iodide in an aq. potassium iodide soln. or by other method. Alkali hydroxide is then added to the aq. soln. to decompose gold iodide. The proper concn. of the alkali hydroxide is about 0.1W6N. The pref. reaction temp. is about 20W70°C and the particle size of formed particles can be controlled by changing the temp. condition. The reaction is terminated at ≥about 12.5, preferably ≥about 13 pH. Thus, singly dispersed fine gold particles of ≤several μm particle size are obtd. COPYRIGHT: (C)1989,JPO&Japio
Inventors
- 👤 Motoyuki Nakanishi
Bibliographic Details
Claims Analysis
Total Claims: 0References Cited (Backward Citations)
No citation records indexed.
USPTO Annuity & Maintenance Windows
Maintenance schedule is calculated for granted US utility patents.