Method for manufacturing thermal transfer recording material
Abstract
Abstract Translated from Japanese (57)【要約】 【構成】 基材と該基材上に、熱溶融性バインダー、柔 軟材、着色剤及び常温で固体の脂肪酸及び/又はその酸 誘導体を含有する熱溶融性インキ層を設けてなる感熱転 写型記録材の製造方法において、熱溶融性インキ層を基 材上に塗布などの手段で設けた後、40〜60℃にて1 2時間以上熱処理する感熱転写型記録材の製造方法。 【効果】 連続印字時に感熱転写型記録材の走行性が低 下することなく、凹凸の激しい一般紙への印字も可能で ある。 (57) [Summary] [Structure] A base material and a heat-meltable ink layer containing a heat-meltable binder, a softener, a colorant, and a fatty acid and / or an acid derivative thereof solid at room temperature are provided on the base material. In the method for producing a heat-sensitive transfer recording material, the heat-meltable ink layer is provided on a substrate by means such as coating, and then at 40 to 60 ° C. for 1 hour. A method for producing a heat-sensitive transfer recording material, wherein heat treatment is performed for 2 hours or more. [Effect] It is possible to perform printing on general paper having severe unevenness without lowering the running property of the heat-sensitive transfer recording material during continuous printing.
Inventors
- 👤 Eiichi Okabe
- 👤 鋭一 岡部
Bibliographic Details
Claims Analysis
Total Claims: 0References Cited (Backward Citations)
No citation records indexed.
USPTO Annuity & Maintenance Windows
Maintenance schedule is calculated for granted US utility patents.