Optical semiconductor element and fabricating method therefor
Abstract
Abstract A ZnO thin film is fabricated on the c-surface of a sapphire substrate through use of a laser molecular beam epitaxy (MBE) method―which is effective for epitaxial growth of an oxide thin film through control at an atomic level. The thus-formed ZnO thin film has a considerably high crystallinity; the half width of an X-ray rocking curve was 0.06°. The thin film is of an n-type and has a carrier density of 4 x 10 17 /cm 3 . The thin film fabricated in a state in which oxygen partial pressure is held constant at 10 -6 Torr has a structure in which hexagon-shaped nanocrystals of uniform size are close-packed, reflecting the crystal behavior of a wurtzite type. Since in each nanocrystal there is observed a spiral structure formed by steps of a unit cell height (0.5 nm), the nanocrystals are considered to grow in a thermodynamically equilibrated state. The lateral size of the nanocrystal can be controlled within the range of approximately 50 to 250 nm. A II-oxide optical semiconductor element utilizes a zinc oxide thin film containing magnesium or cadmium in a solid-solution state. Through addition of magnesium or cadmium, the band gap of zinc oxide can be controlled within the range of 3 to 4 eV.
Inventors
- 👤 Masashi Kawasaki
- 👤 Hideomi Koinuma
- 👤 Akira Ohtomo
- 👤 Yusaburo Segawa
- 👤 Takashi Yasuda
Bibliographic Details
Claims Analysis
Total Claims: 13References Cited (Backward Citations)
No citation records indexed.
USPTO Annuity & Maintenance Windows
Maintenance schedule is calculated for granted US utility patents.