Patent EP0331283A1 successfully refreshed from Google Patents.
← Back to Patent Explorer
EP0331283A1 Expired / Lapsed EP ⏱️ 0.0 years remaining

High stability porous zirconium oxide spherules

Assignee: University of Minnesota Twin Cities
•
Filing: 1989-01-27
•
Granted: —
•
Expires: 2009-01-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The present invention provides a stable stationary phase for chromatography which comprises porous ZrO₂ spherules coated with a polymer coating wherein said coated spherules have a pore size from about 20-500 Å and a particle diameter range of about 0.5-500 microns, and are stable in basic media to pHs of up to about l4.

Inventors

  • 👤 Peter W. Carr
  • 👤 Martin O. Rigney
  • 👤 Eric F. Funkenbusch
  • 👤 Patrick L. Coleman
  • 👤 Douglas A. Hanggi

Bibliographic Details

Application Number —
Jurisdiction EP
Data Source google_patents
Last Synchronized 2026-10-27 09:38
CPC Classifications
B; B01; B01J; B01J20/00; B01J20/281; B01J20/282; B01J20/02; B01J20/06; B01J20/28; B01J20/28014; B01J20/28016; B01J20/28019; B01J20/286; B01J20/30; B01J20/32; B01J20/3202; B01J20/3204; B01J20/3231; B01J20/3242; B01J20/3268; B01J20/3272; B01J20/3274; B01J39/00; B01J39/08; B01J39/12; B82; B82Y; B82Y30/00; C; C01; C01G; C01G25/00; C01G25/02; C12; C12N; C12N11/00; C12N11/14; G; G01; G01N; G01N33/00; G01N33/48; G01N33/50; G01N33/53; G01N33/543; G01N33/551; G01N33/553; B01D; B01D15/00; B01D15/08; B01D15/26; B01D15/32; B01D15/325; C01P; C01P2004/00; C01P2004/30; C01P2004/32; C01P2004/60; C01P2004/61; C01P2004/62; C01P2004/64; C01P2004/80; C01P2006/00; C01P2006/12; C01P2006/14; C01P2006/16; C01P2006/17; G01N30/00; G01N30/02; G01N30/50; G01N30/52; G01N2030/524; G01N2030/525

Claims Analysis

Total Claims: 21
Claim 1
Independent Claim 48 words
A bed comprising porous ZrO₂ spherules of about 20-500 microns in diameter, about 1-200 m²/g sur­face area and of about 0.5-500 Å pore diameter; wherein said spherules form the packing of an HPLC column and are substantially stable in an aqueous solution of a pH of about 1-14.
Claim 2
Dependent Claim 48 words
A bed comprising porous ZrO₂ spherules of about 20-500 microns in diameter, about 1-200 m²/g sur­face area and of about 0.5-500 Å pore diameter; wherein said spherules form the packing of an HPLC column and are substantially stable in an aqueous solution of a pH of about 1-14.
Claim 3
Dependent Claim 31 words
The bed of claim 1 wherein the spherules are about 45-500 microns in diameter and have a surface area of about 40-150 m²/g and an average pore diameter of about 100-300Å.
Claim 4
Dependent Claim 106 words
The bed of claim 1 wherein the porous ZrO₂ spherules are characterized by having been prepared by a process consisting essentially of: (a) centrifuging an aqueous sol containing colloidal ZrO₂ particles to yield a residue of ZrO₂ particles and a supernatant; (b) recovering said residue; (c) redispersing said residue in an about equal volume of water to form an aqueous sol con­taining colloidal ZrO₂ particles; (d) dispersing the aqueous sol in a liquid medium which extracts the water from the sol to afford gelled ZrO₂ spherules; (e) recovering the gelled spherules from the medium; and (f) heating the gelled spherules to yield solid porous ZrO₂ spherules.
Claim 5
Dependent Claim 13 words
The bed of claim 3 wherein steps (a)-(c) are repeated about 2-5 times.
Claim 6
Dependent Claim 41 words
Porous ZrO₂ spherules coated with a hydrophobic crosslinked polymer coating wherein said coated spherules have a pore size from about 20-500 Å and a particle diameter range of about 0.5-500 microns, and are stable to about pH 14 in aqueous media.
Claim 7
Dependent Claim 41 words
Porous ZrO₂ spherules coated with a hydrophobic crosslinked polymer coating wherein said coated spherules have a pore size from about 20-500 Å and a particle diameter range of about 0.5-500 microns, and are stable to about pH 14 in aqueous media.
Claim 8
Dependent Claim 11 words
The spherules of claim 5 wherein the polymer coating comprises polybutadiene.
Claim 9
Dependent Claim 29 words
The spherules of claim 5 wherein the surface of the ZrO₂ spherules is modified by treatment with inorganic phosphate to impart both cation-exchange and hydrophobic characteristics to said spherules.
Claim 10
Dependent Claim 11 words
The spherules of claim 7 wherein the inorganic phosphate is H₃PO₄.
Claim 11
Dependent Claim 32 words
The spherules of claim 5 wherein the surface of the ZrO₂ spherules is deactivated by treatment with an effective amount of an organophosphorus compound prior to application of the hydrophobic polymer coating.
Claim 12
Dependent Claim 28 words
The ZrO₂ spherules of claim 9 wherein the surface of the coated spherules is deactivated by treatment with an effective amount of an unsaturated organo­phosphonate or organophosphonic acid.
Claim 13
Dependent Claim 11 words
The ZrO₂ spherules of claim 10 wherein the organo­phosphonate is allylphosphonate.
Claim 14
Dependent Claim 32 words
The ZrO₂ spherules of claim 5 wherein the surface of the coated spherules is deactivated by treatment with an effective amount of an organophosphorus compound following application of the hydrophobic polymer coating.
Claim 15
Dependent Claim 28 words
The ZrO₂ spherules of claim 5 wherein the surface of the coated spherules is deactivated by treatment with an effective amount of an unsaturated organo­phosphonate or organophosphonic acid.
Claim 16
Dependent Claim 12 words
The ZrO₂ spherules of claim 13 wherein the organo­phosphonate is allyl phosphonate.
Claim 17
Dependent Claim 30 words
A thin layer chromatography plate comprising a substrate coated with a mixture of a binder and a particulate support material comprising the spheru­les of claims 5, 7, 10 or 12.
Claim 18
Dependent Claim 24 words
The bed of claim 1 wherein the surface of the ZrO₂ spherules is modified by treatment with inorganic phosphate or with an organophosphorus compound.
Claim 19
Dependent Claim 45 words
A bed comprising porous ZrO₂ spherules of about 20-500 microns in diameter, about 1-200 m²/g sur­face area and of about 0.5-500 Å pore diameter; wherein said spherules are substantially stable in an aqueous solution of a pH of about 1-14, and comprise an immobilized protein.
Claim 20
Dependent Claim 45 words
A bed comprising porous ZrO₂ spherules of about 20-500 microns in diameter, about 1-200 m²/g sur­face area and of about 0.5-500 Å pore diameter; wherein said spherules are substantially stable in an aqueous solution of a pH of about 1-14, and comprise an immobilized protein.
Claim 21
Dependent Claim 13 words
The bed of claim 17 which comprises an enzyme immo­bilized on said spherules.

References Cited (Backward Citations)

EP0162716A2 Cited
DE3440018C1 Cited
EP0216730A2 Cited
EP0273756A2 Cited
EP0280673A2 Cited

USPTO Annuity & Maintenance Windows

Maintenance schedule is calculated for granted US utility patents.

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag