Abstract A substrate is provided with a refractory oxide coating by contacting the substrate with a dispersion of' a solid particulate phase in a liquid phase, subsequently followed by firing to produce the coating, the dispersion comprising at least a first and a second refractory oxide component. In order to produce a coating of controlled purity, e.g. for certain catalytic, electronic or other applications, the first refractory oxide component (e.g. an alumina) is obtained from a purifiable liquid or solid precursor therefor and constitutes part at least of the solid phase, and the second refractory oxide component is either obtained from a purifiable liquid or solid precursor therefor and constitutes part of the solid phase or is a purifiable liquid precursor (e.g. a water-soluble silicone) constituting part at least of the liquid phase.

Inventors

  • 👤 James Anthony Cairns
  • 👤 Edward Sydney Lane
  • 👤 Thomas Campbell Prentice
  • 👤 David Leslie Ridgeway House Segal
  • 👤 David Campbell Sammon

Bibliographic Details

Application Number —
Jurisdiction EP
Data Source google_patents
Last Synchronized 2026-10-30 15:13
CPC Classifications
C; C01; C01F; C01F7/00; C01F7/02; C01F7/34; C01F7/36; B; B01; B01J; B01J37/00; B01J37/02; B01J37/0215; C04; C04B; C04B41/00; C04B41/45; C04B41/50; C04B41/5025; C23; C23D; C23D5/00; C23D5/10; C01P; C01P2006/00; C01P2006/80

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 113 words
A method of providing a substrate with a refractory oxide coating comprising contacting the substrate with a dispersion of a solid particulate phase in a liquid phase, subsequently followed by firing to produce the coating, the dispersion comprising at least a first and a second refractory oxide component, characterised in that the first refractory oxide component is obtained from a purifiable liquid or solid precursor therefor and constitutes part at least of the solid phase, and the second refractory oxide component is either obtained from a purifiable liquid or solid precursor therefor and constitutes part of the solid phase or is a purifiable liquid precursor constituting part at least of the liquid phase.
Claim 2
Independent Claim 113 words
A method of providing a substrate with a refractory oxide coating comprising contacting the substrate with a dispersion of a solid particulate phase in a liquid phase, subsequently followed by firing to produce the coating, the dispersion comprising at least a first and a second refractory oxide component, characterised in that the first refractory oxide component is obtained from a purifiable liquid or solid precursor therefor and constitutes part at least of the solid phase, and the second refractory oxide component is either obtained from a purifiable liquid or solid precursor therefor and constitutes part of the solid phase or is a purifiable liquid precursor constituting part at least of the liquid phase.
Claim 3
Dependent Claim 16 words
A method as claimed in Claim 1, wherein the first refractory oxide component is an alumina.
Claim 4
Dependent Claim 21 words
A method as claimed in Claim 2, wherein the alumina is made by the hydrolysis of a liquid organo aluminium compound.
Claim 5
Dependent Claim 16 words
A method as claimed in Claim 3, wherein the liquid organo aluminium compound is aluminium sec-butoxide.
Claim 6
Independent Claim 28 words
A method as claimed in any of the preceding claims, wherein the second refractory oxide component comprises a water-soluble silicone constituting part at least of the liquid phase.
Claim 7
Dependent Claim 15 words
A method as claimed in Claim 5, wherein the silicone is a silicone glycol copolymer.
Claim 8
Dependent Claim 13 words
A method as claimed in Claim 6, wherein the copolymer is dimethicone copolyol.
Claim 9
Independent Claim 29 words
A method as claimed in any of Claims 1 to 4, wherein the second refractoryoxide component comprises a quarternary ammonium silicate constituting part at least of the liquid phase.
Claim 10
Independent Claim 15 words
A method as claimed in any of the preceding claims wherein the substrate is non-metallic.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Maintenance schedule is calculated for granted US utility patents.

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag