Abstract

Abstract A process for the manufacturing of thermoplastic products with a high creep strain resistance. The products are free from reinforcing additives. The process includes at least vacuum forming and/or blow moulding of a thermoplastic material such as a polyolefine. A number of product parts are manufactured from a number of preferably tube- or sheet-shaped work pieces. The work pieces are heated so that the thermoplastic material softens whereby they are given the desired shape by means of a mould and the influence of vacuum and/or pressure. The product parts produced are allowed to cool and post-shrink and are hereafter joined to a unit.

Inventors

  • 👤 Anders Valentinsson

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 08:10
CPC Classifications
B; B29; B29C; B29C66/00; B29C66/40; B29C66/47; B29C66/472; B29C51/00; B29C51/10; B29C51/26; B29C51/266; B29C51/267; B29C65/00; B29C65/02; B29C65/18; B29C65/20; B29C66/01; B29C66/05; B29C66/10; B29C66/11; B29C66/112; B29C66/1122; B29C66/114; B29C66/1142; B29C66/50; B29C66/51; B29C66/54; B29C66/543; B29C66/70; B29C66/71; B29C66/72; B29C66/723; B29C66/73; B29C66/739; B29C66/7392; B29C66/73921; B65; B65D; B65D19/00; B65D19/0004; B65D19/0006; B65D19/0008; B65D19/002; B65D19/0024; B65D19/0026; B29C2791/00; B29C2791/001; B29C2791/004; B29C2791/006; B29C2791/007; B29C65/06; B29C66/80; B29C66/83; B29C66/832; B29C66/8322; B29K; B29K2023/00; B29K2023/04; B29K2023/06; B29K2023/10; B29K2023/12; B29K2105/00; B29K2105/26; B29L; B29L2031/00; B29L2031/712; B29L2031/7178; B65D2519/00; B65D2519/00004; B65D2519/00009; B65D2519/00014; B65D2519/00034; B65D2519/00049; B65D2519/00069; B65D2519/00084; B65D2519/00104; B65D2519/00258; B65D2519/00283; B65D2519/00293; B65D2519/00313; B65D2519/00323; B65D2519/00328; B65D2519/00333; B65D2519/00368; B65D2519/00373; B65D2519/00547; B65D2519/00552; B65D2519/00557; B65D2519/00562; Y; Y10; Y10T; Y10T156/00; Y10T156/10; Y10T156/1002

Claims Analysis

Total Claims: 23
Claim 1
Independent Claim 397 words
A molding process for the manufacture of a product comprising at least a first product part and a second product part from a thermoplastic material selected from the group consisting of polyethylene, polypropylene and polybutylene which product has no reinforcing additives, in a mold having a first mold half and a second mold half, which together includes a shape-giving cavity being a negative depiction of the respective product part, the method comprising: forming the first product part, comprising: providing two mold halves, at least one of the mold halves having a projection in the shape-giving cavity thereby forming at least one protrusion in a work piece formed in said mold half; placing the mold halves so that a space is formed between the two mold halves and so that the shape-giving cavity of each mold half is directed toward each other; heating two work pieces which constitute an upper half and a lower half of the product part, thereby softening the thermoplastic material; shaping the work pieces toward the cavity of each mold half with the assistance of vacuum, blowing, and combinations thereof, to form shaped work pieces; moving the mold halves relatively toward one another and pressing the shaped work pieces together while the thermoplastic material is still hot to form a unitary hollow product part with the upper and lower halves of said product part being joined along their edges and by said at least one protrusion to increase mechanical strength and dimension stability; and cooling the first product part produced to the point where it can be removed from the mold though still at an elevated temperature; and further cooling the first product part for 1-2 days until the first product part has reached room temperature and post shrinking has been achieved; forming the second product part, comprising: injecting molten thermoplastic material into one or more mold cavities of the mold; allowing the thermoplastic material to solidify; opening the mold; cooling the second product part produced to the point where it can be removed from the mold though still at an elevated temperature; and removing the product part from the mold; further cooling the second product part for 1-2 days until the second product part has reached room temperature and post shrinking has been achieved; and joining the first product part to the second product part and receiving a high creep strain resistant product.
Claim 2
Dependent Claim 397 words
A molding process for the manufacture of a product comprising at least a first product part and a second product part from a thermoplastic material selected from the group consisting of polyethylene, polypropylene and polybutylene which product has no reinforcing additives, in a mold having a first mold half and a second mold half, which together includes a shape-giving cavity being a negative depiction of the respective product part, the method comprising: forming the first product part, comprising: providing two mold halves, at least one of the mold halves having a projection in the shape-giving cavity thereby forming at least one protrusion in a work piece formed in said mold half; placing the mold halves so that a space is formed between the two mold halves and so that the shape-giving cavity of each mold half is directed toward each other; heating two work pieces which constitute an upper half and a lower half of the product part, thereby softening the thermoplastic material; shaping the work pieces toward the cavity of each mold half with the assistance of vacuum, blowing, and combinations thereof, to form shaped work pieces; moving the mold halves relatively toward one another and pressing the shaped work pieces together while the thermoplastic material is still hot to form a unitary hollow product part with the upper and lower halves of said product part being joined along their edges and by said at least one protrusion to increase mechanical strength and dimension stability; and cooling the first product part produced to the point where it can be removed from the mold though still at an elevated temperature; and further cooling the first product part for 1-2 days until the first product part has reached room temperature and post shrinking has been achieved; forming the second product part, comprising: injecting molten thermoplastic material into one or more mold cavities of the mold; allowing the thermoplastic material to solidify; opening the mold; cooling the second product part produced to the point where it can be removed from the mold though still at an elevated temperature; and removing the product part from the mold; further cooling the second product part for 1-2 days until the second product part has reached room temperature and post shrinking has been achieved; and joining the first product part to the second product part and receiving a high creep strain resistant product.
Claim 3
Dependent Claim 106 words
The process according to claim 1 , further comprising molding at least one additional product part through injection molding by means of a mold comprising one or more mold cavities wherein the mold includes means for injecting a pressurized gas comprising: injecting molten thermoplastic material into a mold cavity of the mold; and injecting pressurized gas into the molten thermoplastic material in the mold cavity; allowing the thermoplastic material to solidify; evacuating the gas; opening the mold; removing the product part from the mold; allowing the product part to cool completely and post-shrink; and joining the post-shrunk at least one additional product part to the product.
Claim 4
Dependent Claim 25 words
The process according to claim 1 , wherein the thermoplastic material is constituted by a polymer with an average molecular mass in the range 200,000-2,000,000.
Claim 5
Dependent Claim 20 words
The process according to claim 3 , wherein the average molecular mass of the thermoplastic material is greater than 300,000.
Claim 6
Dependent Claim 60 words
The process according to claim 1 , wherein the thermoplastic material is constituted by a thermoplastic laminate with at least two layers, wherein the layers are constituted by a combination of at least two of the materials selected from the group consisting of virgin solid thermoplastic material, recycled solid thermoplastic material, virgin expanded thermoplastic material and recycled expanded thermoplastic material.
Claim 7
Dependent Claim 37 words
The process according to claim 1 , wherein said at least one protrusion joining the upper and lower halves of said first product part has a shape selected from the group consisting of a tower or ridge.
Claim 8
Dependent Claim 19 words
The process according to claim 1 , wherein each work piece is in a form consisting of a sheet.
Claim 9
Dependent Claim 26 words
The process according to claim 1 , wherein the two work pieces are provided in the form of a two separate sheets prior to said heating.
Claim 10
Dependent Claim 51 words
The process according to claim 1 , further comprising molding work pieces into at least one product part selected from the group consisting of a pallet deck, a foot and a skid of a pallet; and a pallet deck, a foot, a side wall and a skid of a pallet container.
Claim 11
Dependent Claim 53 words
The process according to claim 1 , further comprising molding one or both work pieces into at least one shape selected from the group consisting of a pallet deck, a foot and a skid of a pallet; and a pallet deck, a foot, a side wall and a skid of a pallet container.
Claim 12
Dependent Claim 36 words
The process according to claim 1 , wherein the two work pieces are part of a single tube, having a circumferential surface, wherein said circumferential surface serves as both the first and the second work piece.
Claim 13
Dependent Claim 29 words
The method of claim 1 , wherein the first product part is a first hollow pallet deck and the second product part is at least one hollow pallet skid.
Claim 14
Dependent Claim 34 words
The method of claim 12 , further comprising molding a second hollow deck member and wherein the product comprises three second product parts, wherein each of the second product parts a hollow pallet skid.
Claim 15
Dependent Claim 23 words
The method according to claim 1 , wherein said joining of the first product part to the second product part is by welding.
Claim 16
Dependent Claim 35 words
The process according to claim 14 , wherein said welding of the hollow pallet deck and the hollow pallet skids includes welding selected from the group consisting of butt welding, friction welding and filler welding.
Claim 17
Dependent Claim 35 words
The process according to claim 14 , wherein said welding of the hollow pallet deck and the hollow pallet skids includes welding selected from the group consisting of butt welding, friction welding and filler welding.
Claim 18
Dependent Claim 25 words
The process according to claim 14 , wherein said welding is selected from the group consisting of ultrasonic welding, low frequency welding and rotation welding.
Claim 19
Dependent Claim 585 words
A molding process for the manufacture of a product comprising a hollow pallet deck and a at least one hollow pallet skid from a thermoplastic material selected from the group consisting of polyethylene, polypropylene and polybutylene, which product has no reinforcing additives, in a mold having a first mold half and a second mold half, which together includes a shape-giving cavity being a negative depiction of the respective product part, the method comprising: forming one of either the pallet deck or the at least one skid, comprising: providing two mold halves, at least one of the mold halves having a projection in the shape-giving cavity thereby forming at least one protrusion in a work piece formed in said mold half; placing the mold halves so that a space is formed between the two mold halves and so that the shape-giving cavity of each mold half is directed toward each other; heating two work pieces which constitute an upper half and a lower half of the product part, thereby softening the thermoplastic material; shaping the work pieces toward the cavity of each mold half with the assistance of vacuum, blowing, and combinations thereof, to form shaped work pieces; moving the mold halves relatively toward one another and pressing the shaped work pieces together while the thermoplastic material is still hot to form a unitary hollow product part with the upper and lower halves of said product part being joined along their edges and by said at least one protrusion to increase mechanical strength and dimension stability; and cooling the first product part produced to the point where it can be removed from the mold though still at an elevated temperature; and further cooling the first product part for 1-2 days until the first product part has reached room temperature and post shrinking has been achieved; forming the other of the pallet deck or at least one skid, having a high creep strain resistance, no reinforcing additives, a mold, the mold having a first mold half and a second mold half, which together includes a shape-giving cavity being a negative depiction of the respective product part, the method comprising: providing two mold halves, at least one of the mold halves having a projection in the shape-giving cavity thereby forming at least one protrusion in a work piece formed in said mold half; placing the mold halves so that a space is formed between the two mold halves and so that the shape-giving cavity of each mold half is directed toward each other; heating two work pieces which constitute an upper half and a lower half of the product part, thereby softening the thermoplastic material; shaping the work pieces toward the cavity of each mold half with the assistance of vacuum, blowing, and combinations thereof, to form shaped work pieces; moving the mold halves relatively toward one another and pressing the shaped work pieces together while the thermoplastic material is still hot to form a unitary hollow product part with the upper and lower halves of said product part being joined along their edges and by said at least one protrusion to increase mechanical strength and dimension stability; and cooling the second product part produced to the point where it can be removed from the mold though still at an elevated temperature; and further cooling the second product part for 1-2 days until the second product part has reached room temperature and post shrinking has been achieved; and joining the hollow pallet deck and hollow pallet skids together.
Claim 20
Dependent Claim 585 words
A molding process for the manufacture of a product comprising a hollow pallet deck and a at least one hollow pallet skid from a thermoplastic material selected from the group consisting of polyethylene, polypropylene and polybutylene, which product has no reinforcing additives, in a mold having a first mold half and a second mold half, which together includes a shape-giving cavity being a negative depiction of the respective product part, the method comprising: forming one of either the pallet deck or the at least one skid, comprising: providing two mold halves, at least one of the mold halves having a projection in the shape-giving cavity thereby forming at least one protrusion in a work piece formed in said mold half; placing the mold halves so that a space is formed between the two mold halves and so that the shape-giving cavity of each mold half is directed toward each other; heating two work pieces which constitute an upper half and a lower half of the product part, thereby softening the thermoplastic material; shaping the work pieces toward the cavity of each mold half with the assistance of vacuum, blowing, and combinations thereof, to form shaped work pieces; moving the mold halves relatively toward one another and pressing the shaped work pieces together while the thermoplastic material is still hot to form a unitary hollow product part with the upper and lower halves of said product part being joined along their edges and by said at least one protrusion to increase mechanical strength and dimension stability; and cooling the first product part produced to the point where it can be removed from the mold though still at an elevated temperature; and further cooling the first product part for 1-2 days until the first product part has reached room temperature and post shrinking has been achieved; forming the other of the pallet deck or at least one skid, having a high creep strain resistance, no reinforcing additives, a mold, the mold having a first mold half and a second mold half, which together includes a shape-giving cavity being a negative depiction of the respective product part, the method comprising: providing two mold halves, at least one of the mold halves having a projection in the shape-giving cavity thereby forming at least one protrusion in a work piece formed in said mold half; placing the mold halves so that a space is formed between the two mold halves and so that the shape-giving cavity of each mold half is directed toward each other; heating two work pieces which constitute an upper half and a lower half of the product part, thereby softening the thermoplastic material; shaping the work pieces toward the cavity of each mold half with the assistance of vacuum, blowing, and combinations thereof, to form shaped work pieces; moving the mold halves relatively toward one another and pressing the shaped work pieces together while the thermoplastic material is still hot to form a unitary hollow product part with the upper and lower halves of said product part being joined along their edges and by said at least one protrusion to increase mechanical strength and dimension stability; and cooling the second product part produced to the point where it can be removed from the mold though still at an elevated temperature; and further cooling the second product part for 1-2 days until the second product part has reached room temperature and post shrinking has been achieved; and joining the hollow pallet deck and hollow pallet skids together.
Claim 21
Dependent Claim 17 words
The method of claim 18 , comprising forming two hollow pallet decks and three hollow pallet skids.
Claim 22
Dependent Claim 19 words
The process according to claim 18 , wherein said joining of the pallet deck and skid is by welding.
Claim 23
Dependent Claim 25 words
The process according to claim 20 , wherein said welding is selected from the group consisting of ultrasonic welding, low frequency welding and rotation welding.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2005-09-30 2006-04-01 2006-10-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2009-09-30 2010-04-01 2010-10-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2013-09-30 2014-04-01 2014-10-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag