Claims Analysis
Total Claims: 24
Claim 1
Independent Claim
125 words
A ferroelectric capacitor comprising a ferroelectric layer to which a pair of electrodes are connected wherein: the ferroelectric layer includes an oxide of a layered crystal structure consisting of bismuth (Bi), oxygen, at least one first element selected from the group consisting of strontium (Sr), calcium (Ca) and barium (Ba), and at least one second element selected from the group consisting of tantalum (Ta) and niobium (Nb) with a formula of the oxide being represented by Bi x (Sr, Ca, Ba) y (Ta, Nb) 2 O 9 ±d, wherein 1.70≦x≦2.50, 0.60≦y≦1.20 and 0≦d≦1.00 and the first element of the ferroelectric layer having a variation of proportions in one direction so that the proportion changes from one side of the ferroelectric layer to the other side.
Claim 2
Dependent Claim
125 words
A ferroelectric capacitor comprising a ferroelectric layer to which a pair of electrodes are connected wherein: the ferroelectric layer includes an oxide of a layered crystal structure consisting of bismuth (Bi), oxygen, at least one first element selected from the group consisting of strontium (Sr), calcium (Ca) and barium (Ba), and at least one second element selected from the group consisting of tantalum (Ta) and niobium (Nb) with a formula of the oxide being represented by Bi x (Sr, Ca, Ba) y (Ta, Nb) 2 O 9 ±d, wherein 1.70≦x≦2.50, 0.60≦y≦1.20 and 0≦d≦1.00 and the first element of the ferroelectric layer having a variation of proportions in one direction so that the proportion changes from one side of the ferroelectric layer to the other side.
Claim 3
Dependent Claim
37 words
A ferroelectric capacitor according to claim 1, the ferroelectric capacitor being formed on a substrate wherein: the proportion of the first element increases from a side close to the substrate to a side opposite to the substrate.
Claim 4
Dependent Claim
55 words
A ferroelectric capacitor according to claim 2, wherein the proportion of the first element is such that the value of `y` in the formula falls in the range of 0.7 to 0.9 inclusive on the side close to the substrate and the range of 0.9 to 1.1 inclusive on the side opposite to the substrate.
Claim 5
Dependent Claim
37 words
A ferroelectric capacitor according to claim 1, the ferroelectric capacitor being formed on a substrate wherein: the proportion of the first element decreases from a side close to the substrate to a side opposite to the substrate.
Claim 6
Dependent Claim
55 words
A ferroelectric capacitor according to claim 4, wherein the proportion of the first element is such that the value of `y` in the formula falls in the range of 0.9 to 1.1 inclusive on the side close to the substrate and the range of 0.7 to 0.9 inclusive on the side opposite to the substrate.
Claim 7
Dependent Claim
14 words
A ferroelectric capacitor according to claim 1 wherein the first element is strontium (Sr).
Claim 8
Dependent Claim
28 words
A ferroelectric capacitor according to claim 1 wherein 85 percent or more of the ferroelectric layer consists of a crystal phase of the oxide of layered crystal structure.
Claim 9
Independent Claim
140 words
A method of manufacturing a ferroelectric capacitor comprising a ferroelectric layer to which a pair of electrodes are connected, the ferroelectric layer including an oxide of a layered crystal structure consisting of bismuth (Bi), oxygen, at least one first element selected from the group consisting of strontium (Sr), calcium (Ca) and barium (Ba), and at least one second element selected from the group consisting of tantalum (Ta) and niobium (Nb), with a formula of the oxide being represented by Bi x (Sr, Ca, Ba) y (Ta, Nb) 2 O 9 ±d, wherein 1.70≦x≦2.50, 0.60≦y≦1.20 and 0≦d≦1.00, including the step of: forming the ferroelectric layer by stacking a plurality of layers of the oxide, and varying the proportions of the first element in the layers so that the proportions change from one side of the ferroelectric layer to the other side.
Claim 10
Independent Claim
140 words
A method of manufacturing a ferroelectric capacitor comprising a ferroelectric layer to which a pair of electrodes are connected, the ferroelectric layer including an oxide of a layered crystal structure consisting of bismuth (Bi), oxygen, at least one first element selected from the group consisting of strontium (Sr), calcium (Ca) and barium (Ba), and at least one second element selected from the group consisting of tantalum (Ta) and niobium (Nb), with a formula of the oxide being represented by Bi x (Sr, Ca, Ba) y (Ta, Nb) 2 O 9 ±d, wherein 1.70≦x≦2.50, 0.60≦y≦1.20 and 0≦d≦1.00, including the step of: forming the ferroelectric layer by stacking a plurality of layers of the oxide, and varying the proportions of the first element in the layers so that the proportions change from one side of the ferroelectric layer to the other side.
Claim 11
Dependent Claim
36 words
A method according to claim 8, the ferroelectric capacitor being formed on a substrate wherein: the proportion of the first element increases from a side close to the substrate to a side opposite to the substrate.
Claim 12
Dependent Claim
54 words
A method according to claim 9, wherein the proportion of the first element is such that the value of `y` in the formula falls in the range of 0.7 to 0.9 inclusive on the side close to the substrate and the range of 0.9 to 1.1 inclusive on the side opposite to the substrate.
Claim 13
Dependent Claim
37 words
A method according to claim 8, wherein the ferroelectric capacitor being formed on a substrate wherein: the proportion of the first element decreases from a side close to the substrate to a side opposite to the substrate.
Claim 14
Dependent Claim
54 words
A method according to claim 11, wherein the proportion of the first element is such that the value of `y` in the formula falls in the range of 0.9 to 1.1 inclusive on the side close to the substrate and the range of 0.7 to 0.9 inclusive on the side opposite to the substrate.
Claim 15
Dependent Claim
13 words
A method according to claim 8, wherein the first element is strontium (Sr).
Claim 16
Dependent Claim
27 words
A method according to claim 8, wherein 85 percent or more of the ferroelectric layer consists of a crystal phase of the oxide of layered crystal structure.
Claim 17
Dependent Claim
129 words
A memory cell including a ferroelectric capacitor comprising a ferroelectric layer to which a pair of electrodes are connected wherein: the ferroelectric layer includes an oxide of a layered crystal structure consisting of bismuth (Bi), oxygen, at least one first element selected from the group consisting of strontium (Sr), calcium (Ca) and barium (Ba), and at least one second element selected from the group consisting of tantalum (Ta) and niobium (Nb), with a formula of the oxide being represented by Bi x (Sr, Ca, Ba) y (Ta, Nb) 2 O 9 ±d, wherein 1.70≦x≦2.50, 0.60≦y≦1.20 and 0≦d≦1.00 and the first element of the ferroelectric layer having a variation of proportions in one direction so that the proportion changes from one side of the ferroelectric layer to the other side.
Claim 18
Dependent Claim
129 words
A memory cell including a ferroelectric capacitor comprising a ferroelectric layer to which a pair of electrodes are connected wherein: the ferroelectric layer includes an oxide of a layered crystal structure consisting of bismuth (Bi), oxygen, at least one first element selected from the group consisting of strontium (Sr), calcium (Ca) and barium (Ba), and at least one second element selected from the group consisting of tantalum (Ta) and niobium (Nb), with a formula of the oxide being represented by Bi x (Sr, Ca, Ba) y (Ta, Nb) 2 O 9 ±d, wherein 1.70≦x≦2.50, 0.60≦y≦1.20 and 0≦d≦1.00 and the first element of the ferroelectric layer having a variation of proportions in one direction so that the proportion changes from one side of the ferroelectric layer to the other side.
Claim 19
Dependent Claim
38 words
A memory cell according to claim 15, wherein the ferroelectric capacitor being formed on a substrate wherein: the proportion of the first element increases from a side close to the substrate to a side opposite to the substrate.
Claim 20
Dependent Claim
55 words
A memory cell according to claim 16 wherein the proportion of the first element is such that the value of `y` in the formula falls in the range of 0.7 to 0.9 inclusive on the side close to the substrate and the range of 0.9 to 1.1 inclusive on the side opposite to the substrate.
Claim 21
Dependent Claim
38 words
A memory cell according to claim 15, wherein the ferroelectric capacitor being formed on a substrate wherein: the proportion of the first element decreases from a side close to the substrate to a side opposite to the substrate.
Claim 22
Dependent Claim
55 words
A memory cell according to claim 18, wherein the proportion of the first element is such that the value of `y` in the formula falls in the range of 0.9 to 1.1 inclusive on the side close to the substrate and the range of 0.7 to 0.9 inclusive on the side opposite to the substrate.
Claim 23
Dependent Claim
14 words
A memory cell according to claim 15, wherein the first element is strontium (Sr).
Claim 24
Dependent Claim
28 words
A memory cell according to claim 15, wherein 85 percent or more of the ferroelectric layer consists of a crystal phase of the oxide of layered crystal structure.