← Back to Patent Explorer
US5960283A Expired / Lapsed US ⏱️ 0.0 years remaining

Nonvolatile semiconductor memory device and method of fabrication of the same

Assignee: Intellectual Ventures I LLC
•
Filing: 1997-10-08
•
Granted: 1999-09-28
•
Expires: 2017-10-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A nonvolatile semiconductor memory device and a method of fabrication thereof wherein the nonvolatile semiconductor memory device has at least one memory cell transistor of DAS type and an externally-accessible conduction layer electrically connected to the channel region of the transistor.

Inventors

  • 👤 Yasuo Sato

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 02:40
CPC Classifications
H; H10; H10B; H10B41/00; H10B41/30; H10B69/00; H10D; H10D30/00; H10D30/60; H10D30/68; H10D30/681; H10D30/684; H10D30/685

Claims Analysis

Total Claims: 46
Claim 1
Independent Claim 270 words
A method of manufacturing a nonvolatile semiconductor memory device, comprising the steps of: introducing impurities of second conduction type different from said first conduction type into a predetermined region of the semiconductor substrate of first conduction type, and heat-treating the assembly thereby to form at least one field oxide film electrically isolating two element-activating regions from each other while at the same time activating the impurities of second conduction type thereby to form an impurities diffusion layer of second conduction type under said field oxide film; forming a stacked gate including a floating gate formed on at least one of said two element-activating regions through a first insulating film and a control gate formed on said floating gate through a second insulating film; introducing impurities of first conduction type into regions on the two sides of said stacked gate on the surface of said semiconductor substrate, introducing impurities of second conduction type larger in diffusion coefficient than said impurities of first conduction type into one of said two regions, heat-treating the assembly thereby to activate the impurities of first conduction type and the impurities of second conduction type and to form a pair of first diffusion layers by diffusion of the impurities of first conduction type in said two regions, said method further comprising the steps of forming a second diffusion layer surrounding said first diffusion layer in one of said regions by diffusion of the impurities of second conduction type and having a terminal section reaching the surface of one of said element-activating regions; and forming a conduction layer electrically connected to said second diffusion layer and externally accessible.
Claim 2
Independent Claim 270 words
A method of manufacturing a nonvolatile semiconductor memory device, comprising the steps of: introducing impurities of second conduction type different from said first conduction type into a predetermined region of the semiconductor substrate of first conduction type, and heat-treating the assembly thereby to form at least one field oxide film electrically isolating two element-activating regions from each other while at the same time activating the impurities of second conduction type thereby to form an impurities diffusion layer of second conduction type under said field oxide film; forming a stacked gate including a floating gate formed on at least one of said two element-activating regions through a first insulating film and a control gate formed on said floating gate through a second insulating film; introducing impurities of first conduction type into regions on the two sides of said stacked gate on the surface of said semiconductor substrate, introducing impurities of second conduction type larger in diffusion coefficient than said impurities of first conduction type into one of said two regions, heat-treating the assembly thereby to activate the impurities of first conduction type and the impurities of second conduction type and to form a pair of first diffusion layers by diffusion of the impurities of first conduction type in said two regions, said method further comprising the steps of forming a second diffusion layer surrounding said first diffusion layer in one of said regions by diffusion of the impurities of second conduction type and having a terminal section reaching the surface of one of said element-activating regions; and forming a conduction layer electrically connected to said second diffusion layer and externally accessible.
Claim 3
Dependent Claim 20 words
A method according to claim 1, wherein said first conductivity type is N-type and said second conductivity type is P-type.
Claim 4
Independent Claim 296 words
A method of fabricating a nonvolatile semiconductor memory device having a plurality of memory cells, comprising the steps of: introducing impurities of second conduction type different from first conduction type into a predetermined region of a semiconductor substrate of first conduction type, and heat-treating said impurities of second conduction type thereby to form at least a field oxide film for electrically isolating two element-activating regions from each other and to activate said impurities of second conduction type, thereby forming an impurities diffusion layer of second conduction type under said field oxide film; introducing impurities of second conduction type into a plurality of predetermined areas of said element-forming region using a mask having a pattern corresponding to the data to be written in said memory cells; forming a plurality of transistor gate structures for a plurality of memory cells according to a predetermined pattern on at least one of said two element-forming regions; introducing impurities of first conduction type into two regions on the two sides of each of said gate structure of said semiconductor substrate, introducing impurities of second conduction type larger in diffusion coefficient than said impurities of first conduction type into one of said two regions, heat-treating the assembly thereby to activate and diffuse said impurities of first conduction type and said impurities of second conduction type, thereby forming a pair of first diffusion layers by diffusion of impurities of first conduction type in said two regions and forming a second diffusion layer by diffusion of said impurities of second conduction type, said second diffusion layer surrounding said first diffusion layer in one of said two regions and having a terminal section reaching the surface of said semiconductor substrate; and forming a conduction layer electrically connected to said second diffusion layer and externally accessible.
Claim 5
Independent Claim 296 words
A method of fabricating a nonvolatile semiconductor memory device having a plurality of memory cells, comprising the steps of: introducing impurities of second conduction type different from first conduction type into a predetermined region of a semiconductor substrate of first conduction type, and heat-treating said impurities of second conduction type thereby to form at least a field oxide film for electrically isolating two element-activating regions from each other and to activate said impurities of second conduction type, thereby forming an impurities diffusion layer of second conduction type under said field oxide film; introducing impurities of second conduction type into a plurality of predetermined areas of said element-forming region using a mask having a pattern corresponding to the data to be written in said memory cells; forming a plurality of transistor gate structures for a plurality of memory cells according to a predetermined pattern on at least one of said two element-forming regions; introducing impurities of first conduction type into two regions on the two sides of each of said gate structure of said semiconductor substrate, introducing impurities of second conduction type larger in diffusion coefficient than said impurities of first conduction type into one of said two regions, heat-treating the assembly thereby to activate and diffuse said impurities of first conduction type and said impurities of second conduction type, thereby forming a pair of first diffusion layers by diffusion of impurities of first conduction type in said two regions and forming a second diffusion layer by diffusion of said impurities of second conduction type, said second diffusion layer surrounding said first diffusion layer in one of said two regions and having a terminal section reaching the surface of said semiconductor substrate; and forming a conduction layer electrically connected to said second diffusion layer and externally accessible.
Claim 6
Dependent Claim 20 words
A method according to claim 3, wherein said first conductivity type is N-type and said second conductivity type is P-type.
Claim 7
Independent Claim 161 words
A method of fabricating a semiconductor memory device comprising the steps of: forming a charge accumulating layer for accumulating electric charges over a semiconductor substrate; forming a control gate over said charge accumulating layer, said control gate constituting a gate structure of a memory cell transistor together with said charge accumulating layer; forming a pair of impurity diffusion layers of a first conductivity type in a surface of said semiconductor substrate at both sides of said gate structure; forming a second impurity diffusion layer of a second conductivity type different from said first conductivity type to surround one of said pair of first impurity diffusion layers, so that said second impurity diffusion layer provides a channel region of said memory cell transistor; forming an extension of said second impurity diffusion layer so as to extend in said semiconductor substrate; and forming a conductor layer electrically connected to said extension of said second impurity diffusion layer so as to be externally accessible.
Claim 8
Independent Claim 161 words
A method of fabricating a semiconductor memory device comprising the steps of: forming a charge accumulating layer for accumulating electric charges over a semiconductor substrate; forming a control gate over said charge accumulating layer, said control gate constituting a gate structure of a memory cell transistor together with said charge accumulating layer; forming a pair of impurity diffusion layers of a first conductivity type in a surface of said semiconductor substrate at both sides of said gate structure; forming a second impurity diffusion layer of a second conductivity type different from said first conductivity type to surround one of said pair of first impurity diffusion layers, so that said second impurity diffusion layer provides a channel region of said memory cell transistor; forming an extension of said second impurity diffusion layer so as to extend in said semiconductor substrate; and forming a conductor layer electrically connected to said extension of said second impurity diffusion layer so as to be externally accessible.
Claim 9
Dependent Claim 59 words
A method according to claim 5, further comprising the steps of: forming a first insulating film on the surface of said semiconductor substrate so that said charge accumulating layer is formed on said first insulating film; and forming a second insulating film on said charge accumulating layer so that said control gate is formed on said second insulating film.
Claim 10
Dependent Claim 20 words
A method according to claim 5, wherein said charge accumulating layer is a floating gate of said memory cell transistor.
Claim 11
Dependent Claim 87 words
A method according to claim 5, further comprising the step of: forming an element-isolation structure on said semiconductor substrate for defining element activating regions isolated from each other by said element-isolation structure, wherein said memory cell transistor is formed in one of said element activating regions and said extension of said second impurity diffusion layer is formed to extend from said one of said element activating regions to another one of said element activating regions through a portion of said semiconductor substrate disposed beneath said element-isolation structure.
Claim 12
Dependent Claim 15 words
A method according to claim 8, wherein said element-isolation structure includes an elongated element-isolation electrode.
Claim 13
Dependent Claim 17 words
A method according to claim 8, wherein said element-isolation structure includes an elongated element-isolation field oxide film.
Claim 14
Dependent Claim 20 words
A method according to claim 5, wherein said first conductivity type is N-type and said second conductivity type is P-type.
Claim 15
Dependent Claim 61 words
A method according to claim 5, further comprising the steps of: forming an interlayer insulating film over said semiconductor substrate to cover said memory cell transistor; and forming said conductor layer to extend over said interlayer insulating film and to be connected to said extension of said second impurity diffusion layer through a contact hole formed in said interlayer insulating film.
Claim 16
Dependent Claim 17 words
A method according to claim 5, wherein said semiconductor memory device is a nonvolatile semiconductor memory device.
Claim 17
Independent Claim 127 words
A method of fabricating a semiconductor device comprising the steps of: forming a gate structure on a first region of a semiconductor substrate; forming a pair of impurity diffusion layers of a first conductivity type in second regions of said semiconductor substrate disposed on both sides of said first region so that said pair of impurity diffusion layers constitute a transistor together with said gate structure; forming a second impurity diffusion layer of a second conductivity type different from said first conductivity type to surround one of said pair of first impurity diffusion layers, so that said second impurity diffusion layer provides a channel region of said transistor; and forming a conductor layer electrically connected to said second impurity diffusion layer so as to be externally accessible.
Claim 18
Independent Claim 127 words
A method of fabricating a semiconductor device comprising the steps of: forming a gate structure on a first region of a semiconductor substrate; forming a pair of impurity diffusion layers of a first conductivity type in second regions of said semiconductor substrate disposed on both sides of said first region so that said pair of impurity diffusion layers constitute a transistor together with said gate structure; forming a second impurity diffusion layer of a second conductivity type different from said first conductivity type to surround one of said pair of first impurity diffusion layers, so that said second impurity diffusion layer provides a channel region of said transistor; and forming a conductor layer electrically connected to said second impurity diffusion layer so as to be externally accessible.
Claim 19
Dependent Claim 80 words
A method according to claim 14, further comprising the steps of: forming an extension of said second impurity diffusion layer to extend to a surface of said semiconductor substrate; and forming an interlayer insulating film over said semiconductor substrate to cover said transistor, so that said conductor layer is formed on said interlayer insulating film and said conductor layer is connected to said extension of said second impurity diffusion layer through a contact hole formed in said interlayer insulating film.
Claim 20
Dependent Claim 86 words
A method according to claim 14, further comprising the step of: forming an element-isolation structure on said semiconductor substrate for defining element activating regions isolated from each other by said element-isolation structure, and wherein said transistor is formed in one of said element activating regions and said extension of said second impurity diffusion layer is formed to extend from said one of said element activating regions to another one of said element activating regions through a portion of said semiconductor substrate disposed beneath said element-isolation structure.
Claim 21
Dependent Claim 15 words
A method according to claim 16, wherein said element-isolation structure includes an elongated element-isolation electrode.
Claim 22
Dependent Claim 17 words
A method according to claim 16, wherein said element-isolation structure includes an elongated element-isolation field oxide film.
Claim 23
Dependent Claim 20 words
A method according to claim 14, wherein said first conductivity type is N-type and said second conductivity type is P-type.
Claim 24
Dependent Claim 16 words
A method according to claim 14, wherein said semiconductor substrate is of the first conductivity type.
Claim 25
Independent Claim 132 words
A method of fabricating a semiconductor memory device comprising the steps of: forming a gate structure on a first region of a semiconductor substrate; forming a pair of impurity diffusion layers of a first conductivity type in second regions of said semiconductor substrate disposed on both sides of said first region so that said pair of impurity diffusion layers constitute a memory cell transistor together with said gate structure; forming a second impurity diffusion layer of a second conductivity type different from said first conductivity type to surround one of said pair of first impurity diffusion layers, so that said second impurity diffusion layer provides a channel region of said memory cell transistor; and forming a conductor layer electrically connected to said second impurity diffusion layer so as to be externally accessible.
Claim 26
Independent Claim 132 words
A method of fabricating a semiconductor memory device comprising the steps of: forming a gate structure on a first region of a semiconductor substrate; forming a pair of impurity diffusion layers of a first conductivity type in second regions of said semiconductor substrate disposed on both sides of said first region so that said pair of impurity diffusion layers constitute a memory cell transistor together with said gate structure; forming a second impurity diffusion layer of a second conductivity type different from said first conductivity type to surround one of said pair of first impurity diffusion layers, so that said second impurity diffusion layer provides a channel region of said memory cell transistor; and forming a conductor layer electrically connected to said second impurity diffusion layer so as to be externally accessible.
Claim 27
Dependent Claim 44 words
A method according to claim 21, wherein said semiconductor memory device is a nonvolatile semiconductor memory device and said gate structure includes a charge accumulating layer formed over a surface of said semiconductor substrate and a control gate formed over said charge accumulating layer.
Claim 28
Dependent Claim 15 words
A method according to claim 22, wherein said charge accumulating layer is a floating gate.
Claim 29
Dependent Claim 59 words
A method according to claim 22, further comprising the steps of: forming a first insulating film on the surface of said semiconductor substrate so that said charge accumulating layer is formed on said first insulating film; and forming a second insulating film on said charge accumulating layer so that said control gate is formed on said second insulating film.
Claim 30
Dependent Claim 82 words
A method according to claim 21, further comprising the steps of: forming an extension of said second impurity diffusion layer to extend to a surface of said semiconductor substrate; and forming an interlayer insulating film over said semiconductor substrate to cover said memory cell transistor, so that said conductor layer is formed on said interlayer insulating film and said conductor layer is connected to said extension of said second impurity diffusion layer through a contact hole formed in said interlayer insulating film.
Claim 31
Dependent Claim 88 words
A method according to claim 21, further comprising the step of: forming an element-isolation structure on said semiconductor substrate for defining element activating regions isolated from each other by said element-isolation structure, and wherein said memory cell transistor is formed in one of said element activating regions and said extension of said second impurity diffusion layer is formed to extend from said one of said element activating regions to another one of said element activating regions through a portion of said semiconductor substrate disposed beneath said element-isolation structure.
Claim 32
Dependent Claim 15 words
A method according to claim 26, wherein said element-isolation structure includes an elongated element-isolation electrode.
Claim 33
Dependent Claim 17 words
A method according to claim 26, wherein said element-isolation structure includes an elongated element-isolation field oxide film.
Claim 34
Dependent Claim 20 words
A method according to claim 21, wherein said first conductivity type is N-type and said second conductivity type is P-type.
Claim 35
Dependent Claim 16 words
A method according to claim 21, wherein said semiconductor substrate is of the first conductivity type.
Claim 36
Independent Claim 187 words
A method of fabricating a semiconductor memory device including a plurality of memory cell transistors, said method comprising the steps of: forming a gate structure for each of said memory cell transistors over a surface of a semiconductor substrate at its predetermined region, said gate structure including a charge accumulating layer for accumulating electric charges; forming a pair of first impurity diffusion layers of a first conductivity type in the surface of said semiconductor substrate, so that said pair of first impurity diffusion layers constitute one of the memory cell transistors together with said gate structure; forming a second impurity diffusion layer of a second conductivity type different from said first conductivity type in the surface of said semiconductor substrate to surround one of said pair of first impurity diffusion layers, said second impurity diffusion layer constituting a channel region of said one of the memory cell transistors; forming an extension of said second impurity diffusion layer to extend within the surface of said semiconductor substrate; and forming a conductor layer connected to said extension of said second impurity diffusion layer so as to be externally accessible.
Claim 37
Independent Claim 187 words
A method of fabricating a semiconductor memory device including a plurality of memory cell transistors, said method comprising the steps of: forming a gate structure for each of said memory cell transistors over a surface of a semiconductor substrate at its predetermined region, said gate structure including a charge accumulating layer for accumulating electric charges; forming a pair of first impurity diffusion layers of a first conductivity type in the surface of said semiconductor substrate, so that said pair of first impurity diffusion layers constitute one of the memory cell transistors together with said gate structure; forming a second impurity diffusion layer of a second conductivity type different from said first conductivity type in the surface of said semiconductor substrate to surround one of said pair of first impurity diffusion layers, said second impurity diffusion layer constituting a channel region of said one of the memory cell transistors; forming an extension of said second impurity diffusion layer to extend within the surface of said semiconductor substrate; and forming a conductor layer connected to said extension of said second impurity diffusion layer so as to be externally accessible.
Claim 38
Dependent Claim 27 words
A method according to claim 31, wherein said charge accumulating layer is a floating gate and said gate structure includes said floating gate and a control gate.
Claim 39
Dependent Claim 55 words
A method according to claim 32, wherein said step of forming a gate structure comprises forming a first insulating film on the surface of said semiconductor substrate, forming the floating gate on said first insulating film, forming a second insulating film on said floating gate and forming the control gate on said second insulating film.
Claim 40
Dependent Claim 90 words
A method according to claim 31, further comprising the step of: forming an element-isolation structure on said semiconductor substrate for defining element activating regions isolated from each other by said element-isolation structure, and wherein each of said memory cell transistors is formed in one of said element activating regions and said extension of said second impurity diffusion layer is formed to extend from said one of said element activating regions to another one of said element activating regions through a portion of said semiconductor substrate disposed beneath said element-isolation structure.
Claim 41
Dependent Claim 15 words
A method according to claim 34, wherein said element-isolation structure includes an elongated element-isolation electrode.
Claim 42
Dependent Claim 17 words
A method according to claim 34, wherein said element-isolation structure includes an elongated element-isolation field oxide film.
Claim 43
Dependent Claim 20 words
A method according to claim 31, wherein said first conductivity type is N-type and said second conductivity type is P-type.
Claim 44
Dependent Claim 61 words
A method according to claim 31, further comprising the steps of: forming an interlayer insulating film over said semiconductor substrate to cover said memory cell transistors; and forming said conductor layer to extend over said interlayer insulating film and to be connected to said extension of said second impurity diffusion layer through a contact hole formed in said interlayer insulating film.
Claim 45
Dependent Claim 17 words
A method according to claim 31, wherein said semiconductor memory device is a nonvolatile semiconductor memory device.
Claim 46
Dependent Claim 16 words
A method according to claim 39, wherein said nonvolatile semiconductor memory device is a mask ROM.

References Cited (Backward Citations)

US4161039A Cited
JPS54156483A Cited
US4317273A Cited
US4757032A Cited
US5079603A Cited
US5034790A Cited
US5235200A Cited
US5278787A Cited
US5553018A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2002-09-27 2003-03-29 2003-09-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2006-09-27 2007-03-29 2007-09-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2010-09-27 2011-03-29 2011-09-28 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag