Claims Analysis
Total Claims: 14
Claim 1
Independent Claim
87 words
A method of removing contaminants from interior surfaces of a single-wafer chamber for manufacturing semiconductor wafers, the method comprising the steps of providing heating lamps which face into the interior of the chamber, and elevating the temperature of the interior surfaces with the heating lamps to a sufficiently high temperature for a sufficient period of time after a predetermined number of wafers have been manufactured in the chamber to volatilize the contaminants on the interior surfaces and thereby remove contaminants from the interior surfaces of the chamber.
Claim 2
Independent Claim
87 words
A method of removing contaminants from interior surfaces of a single-wafer chamber for manufacturing semiconductor wafers, the method comprising the steps of providing heating lamps which face into the interior of the chamber, and elevating the temperature of the interior surfaces with the heating lamps to a sufficiently high temperature for a sufficient period of time after a predetermined number of wafers have been manufactured in the chamber to volatilize the contaminants on the interior surfaces and thereby remove contaminants from the interior surfaces of the chamber.
Claim 3
Dependent Claim
41 words
The method of claim 1 wherein the chamber is for etching the wafer, and wherein the step of elevating the temperature comprises the steps of heating the interior surfaces to about 250° to 350° C. for about three to seven minutes.
Claim 4
Dependent Claim
39 words
The method of claim 1 wherein the chamber is for photoresist mask removal, and wherein the step of elevating the temperature comprises the steps of heating the interior surfaces to about 175° C. for about two to three minutes.
Claim 5
Dependent Claim
23 words
The method of claim 3 further comprising the step of setting the pressure inside the chamber to about one millitorr to four torr.
Claim 6
Dependent Claim
42 words
The method of claim 1 wherein the chamber is for non-photoresist mask removal, and wherein the step of periodically elevating the temperature comprises the steps of heating the interior surfaces to about 350° to 400° C. for about one to two minutes.
Claim 7
Dependent Claim
23 words
The method of claim 5 further comprising the step of setting the pressure inside the chamber to about one millitorr to four torr.
Claim 8
Dependent Claim
32 words
The method of claim 1 wherein the step of providing heating lamps comprises the steps of situating the heating lamps outside the chamber and directing them through a window in the chamber.
Claim 9
Dependent Claim
31 words
The method of claim 1 wherein the step of elevating the temperature is carried out after every one to two lots of wafers, with approximately 15 to 30 wafers per lot.
Claim 10
Independent Claim
59 words
A method of decreasing the total down time of an etching chamber for cleaning by periodically elevating the temperature of the chamber to a temperature, and for a time, sufficient to volatilize contaminants on the internal chamber walls in the presence of an inert gas and outgassing the volatilized contaminants between conventional wet and dry cleanings of the chamber.
Claim 11
Independent Claim
59 words
A method of decreasing the total down time of an etching chamber for cleaning by periodically elevating the temperature of the chamber to a temperature, and for a time, sufficient to volatilize contaminants on the internal chamber walls in the presence of an inert gas and outgassing the volatilized contaminants between conventional wet and dry cleanings of the chamber.
Claim 12
Dependent Claim
31 words
The method of claim 9 wherein the temperature is raised to 250° to 350° C. for between 3 and 5 minutes at a pressure between about 10 -3 and 4 Torr.
Claim 13
Dependent Claim
29 words
The method of claim 4 wherein the steps of elevating the temperature and setting the pressure can occur prior to or following the mask removal of a semiconductor wafer.
Claim 14
Dependent Claim
37 words
The method of claim 11 wherein the steps of elevating the temperature and setting the pressure can occur while the wafer is in the chamber, thereby removing contaminants from the wafer as well as from the chamber.