Abstract

Abstract A composition and method for repairing damaged connective tissue is provided. The composition comprises pseudo-poly(amino acids) and/or classic poly(amino acids) that exhibit adhesiveness for connective tissues. The composition is formed into an adhesive tissue repair implant and pressed against the damaged tissue to adhere the adhesive composition to the tissue.

Inventors

  • 👤 Dale R. Peterson
  • 👤 Samuel I. Stupp

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 17:28
CPC Classifications
C; C09; C09J; C09J189/00; A; A61; A61L; A61L24/00; A61L24/04; A61L24/043; A61L24/10; A61L24/106

Claims Analysis

Total Claims: 20
Claim 1
Independent Claim 136 words
A pressure-sensitive adhesive composition comprising two different poly(amino acids), each of the formula H 2 N--Q--COOR 2 wherein Q is a divalent residue of a polypeptide formed from 1 to 3 species of amino acids, R 2 is H, a metal cation, or ammonium and wherein the amino acid components of Q are represented by the formula aX+bY+cZ wherein a, b, and c represent the respective mole fractions of the amino acids X, Y, and Z; a=0 to 1, b=0 to 1, and c<1; and a+b+c=1.0, and wherein X is selected from glutamate, asparagine, aspartate, and glutamine, Y is selected from lysine and arginine, and Z is an amino acid selected from cysteine, methionine, serine, threonine, glycine, alanine, valine, leucine, and isoleucine, and wherein the composition exhibits an adhesiveness of about 600 to about 150,000 Pa.
Claim 2
Dependent Claim 136 words
A pressure-sensitive adhesive composition comprising two different poly(amino acids), each of the formula H 2 N--Q--COOR 2 wherein Q is a divalent residue of a polypeptide formed from 1 to 3 species of amino acids, R 2 is H, a metal cation, or ammonium and wherein the amino acid components of Q are represented by the formula aX+bY+cZ wherein a, b, and c represent the respective mole fractions of the amino acids X, Y, and Z; a=0 to 1, b=0 to 1, and c<1; and a+b+c=1.0, and wherein X is selected from glutamate, asparagine, aspartate, and glutamine, Y is selected from lysine and arginine, and Z is an amino acid selected from cysteine, methionine, serine, threonine, glycine, alanine, valine, leucine, and isoleucine, and wherein the composition exhibits an adhesiveness of about 600 to about 150,000 Pa.
Claim 3
Dependent Claim 18 words
The composition of claim 1, wherein the composition is moldable at about 4° C. to about 60° C.
Claim 4
Dependent Claim 22 words
The composition of claim 1, further comprising a monomer selected from the group consisting of glutamate, aspartate, lysine, and histidine and arginine.
Claim 5
Dependent Claim 29 words
The composition of claim 1, wherein the polypeptide bears a negative charge at about physiological pH and further comprising an amino acid monomer with two or more positive charges.
Claim 6
Dependent Claim 19 words
The composition of claim 4, wherein the monomer is selected from the group consisting of lysine, arginine, or histidine.
Claim 7
Dependent Claim 29 words
The composition of claim 1, wherein the polypeptide bears a positive charge at about physiological pH and further comprising an amino acid monomer with two or more negative charges.
Claim 8
Dependent Claim 18 words
The composition of claim 6, wherein the monomer is selected from the group consisting of aspartate or glutamate.
Claim 9
Dependent Claim 10 words
The composition of claim 1, further comprising a bioactive agent.
Claim 10
Dependent Claim 155 words
A pressure-sensitive adhesive composition comprising (1) a poly(amino acid) of the formula H 2 N--Q--COOR 2 wherein Q is a divalent residue of a polypeptide formed from 1 to 3 species of amino acids, R 2 is H, a metal cation, or ammonium and wherein the amino acid components of Q are represented by the formula aX+bY+cZ wherein a, b, and c represent the respective mole fractions of the amino acids X, Y, and Z; a=0 to 1, b=0 to 1, and c<1; and a+b+c=1.0; (a) wherein X is selected from glutamate, asparagine, aspartate, and glutamine; (b) Y is selected from lysine and arginine; and (c) Z is an amino acid selected from cysteine, methionine, serine, threonine, glycine, alanine, valine, leucine, and isoleucine; (2) a monomer selected from the group consisting of glutamate, asparagine, aspartate, glutamine, lysine, arginine, and histidine; and (3) wherein the composition exhibits on adhesiveness of about 600 to about 150,000 Pa.
Claim 11
Dependent Claim 155 words
A pressure-sensitive adhesive composition comprising (1) a poly(amino acid) of the formula H 2 N--Q--COOR 2 wherein Q is a divalent residue of a polypeptide formed from 1 to 3 species of amino acids, R 2 is H, a metal cation, or ammonium and wherein the amino acid components of Q are represented by the formula aX+bY+cZ wherein a, b, and c represent the respective mole fractions of the amino acids X, Y, and Z; a=0 to 1, b=0 to 1, and c<1; and a+b+c=1.0; (a) wherein X is selected from glutamate, asparagine, aspartate, and glutamine; (b) Y is selected from lysine and arginine; and (c) Z is an amino acid selected from cysteine, methionine, serine, threonine, glycine, alanine, valine, leucine, and isoleucine; (2) a monomer selected from the group consisting of glutamate, asparagine, aspartate, glutamine, lysine, arginine, and histidine; and (3) wherein the composition exhibits on adhesiveness of about 600 to about 150,000 Pa.
Claim 12
Dependent Claim 29 words
The composition of claim 9, wherein the polypeptide bears a positive charge at about physiological pH and the monomer is selected from the group consisting of aspartate and glutamate.
Claim 13
Dependent Claim 30 words
The composition of claim 9, wherein the polypeptide bears a negative charge at about physiological pH and the monomer is selected from the group consisting of lysine, arginine, and histidine.
Claim 14
Independent Claim 174 words
A method for repairing damaged connective tissue, the method comprising the steps of (1) selecting a pressure-sensitive adhesive composition comprising a pseudo-poly(amino acid), or a poly(amino acid) of the formula H 2 N--Q--COOR 2 wherein Q is a divalent residue of a polypeptide formed from 1 to 3 species of amino acids, R 2 is H, a metal cation, or ammonium and wherein the amino acid components of Q are represented by the formula aX+bY+cZ, wherein a, b, and c represent the respective mole fractions by the amino acids X, Y, and Z, a+b is >0, and a+b+c=1.0; (a) wherein X is selected from glutamate, asparagine, aspartate, or glutamine; (b) wherein if X is only aspartate, b>0; (c) wherein Y is selected from lysine or arginine; and (d) wherein Z is selected from cysteine, methionine, serine, threonine, glycine, alanine, valine, leucine, isoleucine; (2) forming an adhesive tissue repair implant from the selected pressure-sensitive adhesive composition; and (3) pressing the tissue repair implant against the damaged tissue to adhere the adhesive composition to the tissue.
Claim 15
Independent Claim 174 words
A method for repairing damaged connective tissue, the method comprising the steps of (1) selecting a pressure-sensitive adhesive composition comprising a pseudo-poly(amino acid), or a poly(amino acid) of the formula H 2 N--Q--COOR 2 wherein Q is a divalent residue of a polypeptide formed from 1 to 3 species of amino acids, R 2 is H, a metal cation, or ammonium and wherein the amino acid components of Q are represented by the formula aX+bY+cZ, wherein a, b, and c represent the respective mole fractions by the amino acids X, Y, and Z, a+b is >0, and a+b+c=1.0; (a) wherein X is selected from glutamate, asparagine, aspartate, or glutamine; (b) wherein if X is only aspartate, b>0; (c) wherein Y is selected from lysine or arginine; and (d) wherein Z is selected from cysteine, methionine, serine, threonine, glycine, alanine, valine, leucine, isoleucine; (2) forming an adhesive tissue repair implant from the selected pressure-sensitive adhesive composition; and (3) pressing the tissue repair implant against the damaged tissue to adhere the adhesive composition to the tissue.
Claim 16
Independent Claim 187 words
A method for effecting repair of damaged connective tissue, the method comprising the steps of (1) selecting a pressure-sensitive adhesive composition comprising (a) a poly(amino acid) of the formula H 2 N--Q--COOR 2 wherein Q is a divalent residue of a polypeptide formed from 1 to 3 species of amino acids, R 2 is H, a metal cation, or ammonium and wherein the amino acid components of Q are represented by the formula aX+bY+cZ wherein a, b, and c represent the respective mole fractions of the amino acids X, Y, and Z; a=0 to 1, b=0 to 1; c<1; and a+b+c=1.0; (i) wherein X is selected from glutamate, asparagine, aspartate, and glutamine; (ii) Y is selected from lysine and arginine; and (iii) Z is an amino acid selected from cysteine, methionine, serine, threonine, glycine, alanine, valine, leucine, and isoleucine; and (b) a monomer selected from the group consisting of glutamate, aspartate, lysine, histidine, and arginine; (2) forming an adhesive tissue repair implant from the selected pressure-sensitive adhesive composition; and (3) pressing the tissue repair implant against the damaged tissue to adhere the adhesive composition to the tissue.
Claim 17
Independent Claim 187 words
A method for effecting repair of damaged connective tissue, the method comprising the steps of (1) selecting a pressure-sensitive adhesive composition comprising (a) a poly(amino acid) of the formula H 2 N--Q--COOR 2 wherein Q is a divalent residue of a polypeptide formed from 1 to 3 species of amino acids, R 2 is H, a metal cation, or ammonium and wherein the amino acid components of Q are represented by the formula aX+bY+cZ wherein a, b, and c represent the respective mole fractions of the amino acids X, Y, and Z; a=0 to 1, b=0 to 1; c<1; and a+b+c=1.0; (i) wherein X is selected from glutamate, asparagine, aspartate, and glutamine; (ii) Y is selected from lysine and arginine; and (iii) Z is an amino acid selected from cysteine, methionine, serine, threonine, glycine, alanine, valine, leucine, and isoleucine; and (b) a monomer selected from the group consisting of glutamate, aspartate, lysine, histidine, and arginine; (2) forming an adhesive tissue repair implant from the selected pressure-sensitive adhesive composition; and (3) pressing the tissue repair implant against the damaged tissue to adhere the adhesive composition to the tissue.
Claim 18
Independent Claim 173 words
A method for effecting repair of damaged connective tissue, the method comprising the steps of (1) selecting a pressure-sensitive adhesive composition comprising two different poly(amino acids), each of the formula H 2 N--Q--COOR 2 wherein Q is a divalent residue of a polypeptide formed from 1 to 3 species of amino acids, R 2 is H, a metal cation, or ammonium and wherein the amino acid components of Q are represented by the formula aX+bY+cZ wherein a, b, and c represent the respective mole fractions of the amino acids X, Y, and Z; a=0 to 1, b=0 to 1, and c<1; and a+b+c=1.0; (a) wherein X is selected from glutamate, asparagine, aspartate, and glutamine; (b) Y is selected from lysine and arginine; and (c) Z is an amino acid selected from cysteine, methionine, serine, threonine, glycine, alanine, valine, leucine, and isoleucine; (2) forming an adhesive tissue repair implant from the selected pressure-sensitive adhesive composition; and (3) pressing the tissue repair implant against the damaged tissue to adhere the adhesive composition to the tissue.
Claim 19
Independent Claim 173 words
A method for effecting repair of damaged connective tissue, the method comprising the steps of (1) selecting a pressure-sensitive adhesive composition comprising two different poly(amino acids), each of the formula H 2 N--Q--COOR 2 wherein Q is a divalent residue of a polypeptide formed from 1 to 3 species of amino acids, R 2 is H, a metal cation, or ammonium and wherein the amino acid components of Q are represented by the formula aX+bY+cZ wherein a, b, and c represent the respective mole fractions of the amino acids X, Y, and Z; a=0 to 1, b=0 to 1, and c<1; and a+b+c=1.0; (a) wherein X is selected from glutamate, asparagine, aspartate, and glutamine; (b) Y is selected from lysine and arginine; and (c) Z is an amino acid selected from cysteine, methionine, serine, threonine, glycine, alanine, valine, leucine, and isoleucine; (2) forming an adhesive tissue repair implant from the selected pressure-sensitive adhesive composition; and (3) pressing the tissue repair implant against the damaged tissue to adhere the adhesive composition to the tissue.
Claim 20
Dependent Claim 28 words
The method of claim 14, wherein the forming step comprises the step of maintaining the temperature of the adhesive composition at about 4° C. to about 60° C.

References Cited (Backward Citations)

US4157418A Cited
US4172934A Cited
US4242208A Cited
US4438198A Cited
US4440750A Cited
US4595713A Cited
US4694103A Cited
US4902508A Cited
US4956178A Cited
US5197973A Cited
US5171579A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2001-03-30 2001-09-29 2002-03-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2005-03-30 2005-09-29 2006-03-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2009-03-30 2009-09-29 2010-03-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag