Abstract

Abstract An ink composition and method of printing naturally formed patterns on the surface of various materials, such as paper, glass, ceramic, metal or plastics. The printing method uses a coating liquid of a composition comprising a principal component and a hardener component, applying the component system to a surface through the use of any of a plurality of application methods, and drying the applied surface in two stages which includes a primary drying stage, partly at room temperature, and a forced air drying stage, at elevated temperatures. The process results in a decorative lightly textured surface of a crackled appearance. The principal component of the coating composition consists of a polyol resin, ethylene glycol acetate, ethyl acetate, toluene, filler and pigment. The hardener component consists of blocked isocyanate, ethyl acetate and toluene. The method of the present invention includes mixing of the principal component with the hardener component so that, during the coating and drying stages, the polyol resin reacts with the blocked isocyanate while part of the solvent and blocked isocyanate is volatilized from the coated surface layer of the coating liquid. Natural patterns are formed on the surface of coating materials during hardening as hardening is delayed in the inner layer of the coating liquid while the surface layer shrinks.

Inventors

  • 👤 Chung-Il Ahn
  • 👤 Chan-Hee Shin

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 09:56
CPC Classifications
A; A47; A47L; A47L11/00; A47L11/02; A47L11/20; A47L11/201; C; C09; C09D; C09D5/00; C09D5/28; A47L11/40; A47L11/4036; A47L11/4047; A47L9/00; A47L9/02; A47L9/06; A47L9/0686; B; B05; B05D; B05D5/00; B05D5/06; B05D5/061; B05D5/062; C09D175/00; C09D175/04

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 155 words
A method of preparing a decorative surface coating on a substrate comprising: mixing a principle component and a hardener component in a bulk ratio from 1:2 (v/v) to 2:1 (v/v) to form a liquid coating composition, said principle component consisting of 10-90% by volume of a polyol resin, 3-30% by volume of ethylene glycol acetate, 4-35% by volume of ethyl acetate, 2-20% by volume of toluene, 1-2% by volume of a filler, and 0.01-3% by volume of a pigment, said hardener component consisting of 70-80% by volume of a blocked isocyanate, 10-15% by volume of ethyl acetate, and 10-15% by volume of toluene; applying said liquid coating composition to a surface of a substrate to form a coated product; and, drying said coated product in a primary drying stage at ambient temperatures followed by a forced drying stage at elevated temperatures to obtain an end product having a decorative textured surface of a patterned appearance.
Claim 2
Independent Claim 155 words
A method of preparing a decorative surface coating on a substrate comprising: mixing a principle component and a hardener component in a bulk ratio from 1:2 (v/v) to 2:1 (v/v) to form a liquid coating composition, said principle component consisting of 10-90% by volume of a polyol resin, 3-30% by volume of ethylene glycol acetate, 4-35% by volume of ethyl acetate, 2-20% by volume of toluene, 1-2% by volume of a filler, and 0.01-3% by volume of a pigment, said hardener component consisting of 70-80% by volume of a blocked isocyanate, 10-15% by volume of ethyl acetate, and 10-15% by volume of toluene; applying said liquid coating composition to a surface of a substrate to form a coated product; and, drying said coated product in a primary drying stage at ambient temperatures followed by a forced drying stage at elevated temperatures to obtain an end product having a decorative textured surface of a patterned appearance.
Claim 3
Dependent Claim 30 words
The method according to claim 1, wherein said liquid coating composition is applied by a coating process selected from the group consisting of screen printing, spray coating, and roller coating.
Claim 4
Dependent Claim 26 words
The method according to claim 1, wherein the forced drying stage is conducted at elevated temperatures from 90° to 150° C. for 2 to 20 minutes.

References Cited (Backward Citations)

US3872044A Cited
US4017493A Cited
US4247666A Cited
US4383076A Cited
US4473601A Cited
US4533703A Cited
US4761212A Cited
US5118372A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2000-06-30 2000-12-30 2001-07-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2004-06-30 2004-12-30 2005-07-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2008-06-30 2008-12-30 2009-07-01 $7700.00 Window Closed / Lapsed