← Back to Patent Explorer
US5498447A Expired / Lapsed US ⏱️ 0.0 years remaining

Coating method

Assignee: Sumitomo Pharma Co Ltd
•
Filing: 1993-04-27
•
Granted: 1996-03-12
•
Expires: 2013-04-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A coating method which is characterized in that, when the surfaces of solid particles kept flowing are spray-coated with a thermally melted wax, a two-fluid nozzle adapted to mix a thermally melted wax with a heating gas in and eject the resultant mixture from one flow passage and eject a heating gas from the other flow passage is used, the two-fluid nozzle having spray ports of a diameter of 1.5 to 5.8 mm, and the two-fluid nozzle having no needle valve. According to this method, the use of an organic solvent for melting wax is omitted, and complicated operations for pulverizing a wax and for thermally melting the wax powder after it has been deposed on solid particles are not required. This method can also prevents clogging of the nozzle, powdering of the melted wax and forming of agglomerated solid, and permits simple and easy production of sustained release preparations and preparations for masking materials of unpleasant and bitter tastes.

Inventors

  • 👤 Hiroyuki Nishii
  • 👤 Masaru Kobayashi
  • 👤 Kazutoshi Toya
  • 👤 Nobuo Uchiyama

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 08:39
CPC Classifications
A; A61; A61K; A61K9/00; A61K9/48; A61K9/50; A61K9/5089; A61J; A61J3/00; A61J3/005; B; B01; B01J; B01J2/00; B01J2/003; B01J2/16; A61K9/5073; A61K9/5078

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 79 words
A coating method for spray-coating the surfaces of solid particles with a thermally melted wax, which comprises ejecting a mixture of a thermally melted wax and a heating gas from one of the flow passages of a two-fluid nozzle and, simultaneously, ejecting heating gas from the other flow passage of said two-fluid nozzle, the diameter of spray ports of said two-fluid nozzle being in the range of 1.5 to 5.8 mm, and said two-fluid nozzle having no needle valve.
Claim 2
Dependent Claim 79 words
A coating method for spray-coating the surfaces of solid particles with a thermally melted wax, which comprises ejecting a mixture of a thermally melted wax and a heating gas from one of the flow passages of a two-fluid nozzle and, simultaneously, ejecting heating gas from the other flow passage of said two-fluid nozzle, the diameter of spray ports of said two-fluid nozzle being in the range of 1.5 to 5.8 mm, and said two-fluid nozzle having no needle valve.
Claim 3
Dependent Claim 100 words
The method according to claim 1, wherein said wax is one of the following or mixtures thereof: a) a higher alcohol selected from the group consisting of cetyl alcohol, stearyl alcohol and myristryl alcohol; b) a higher fatty acid selected from the group consisting of myristic acid, palmitic acid, stearic acid and behenic acid; c) a higher fatty acid glycerin ester selected from the group consisting of monoglyceride, diglyceride, triglyceride and polyglyceride; d) a higher hydrocarbon selected from the group consisting of paraffin, ceresin, and microcrystalline wax; or e) a fat, oil or wax which is solid at room temperature.
Claim 4
Dependent Claim 49 words
The method according to claim 2, wherein said oil is a member selected from the group consisting of hydrogenated soybean oil, hydrogenated castor oil, Japan wax and hydrogenated beef tallow, and said wax is a member selected from the group consisting of carnauba wax, candelilla wax and bees wax.
Claim 5
Dependent Claim 45 words
The method according to claim 1, wherein the temperature of the thermally melted wax and the heating gas are controlled so that the temperature thereof at the surfaces of the solid particles is 1° to 100° C. higher than a melting point of said wax.
Claim 6
Dependent Claim 24 words
The method according to claim 1, wherein the pressure of the heating gas is in the range of 0.05 to 10 kg/cm 2 .
Claim 7
Dependent Claim 44 words
The method according to claim 1, wherein the solid particles are kept flowing by using a fluidized bed granulator, a centrifugal granulator, a conventional coating pan, a side vented coating pan, a vacuum coating pan, a high-shear mixer, or a combination of these apparatuses.
Claim 8
Dependent Claim 24 words
The method according to claim 4, wherein said temperature is controlled to 5° to 70° C. higher than the melting point of said wax.
Claim 9
Dependent Claim 37 words
The method according to claim 1, wherein said wax is heated to a temperature of 1° to 50° C. higher than the melting point of said wax and said gas is heated to 100° to 800° C.
Claim 10
Dependent Claim 26 words
The method according to claim 1, wherein said one of the flow passages is from 1 to 30 cm from the surfaces of said solid particles.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1999-03-12 1999-09-11 2000-03-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2003-03-12 2003-09-11 2004-03-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2007-03-12 2007-09-11 2008-03-12 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag