US5474620A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Cut resistant laminate for the light incident surface of a photovoltaic module
Assignee: United Solar Systems Corp
•
Filing: 1994-05-16
•
Granted: 1995-12-12
•
Expires: 2014-05-16
Abstract
Abstract A composite laminate specifically adapted to protect the light incident surface of a photovoltaic module from cuts which could create a short circuit includes a plurality of stacked layer pairs. The first layer of each pair is a glass fiber material and the second layer is a thermoplastic. The layers are disposed in a mutually interpenetrating relationship and topped with a thin transparent protective layer, such as a layer of a fluoropolymer. this combination of layer pairs has been demonstrated to provide sufficient protection to meet Underwriters Laboratories specifications (UL 1703 Section 23. Cut Test) for flat plate photovoltaic modules and panels.
Inventors
- 👤 Prem Nath
- 👤 Craig N. Vogeli
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 07:07
CPC Classifications
H; H10; H10F; H10F19/00; H10F19/80; Y; Y02; Y02E; Y02E10/00; Y02E10/50; Y10; Y10T; Y10T156/00; Y10T156/10; Y10T156/1089; Y10T156/1092; Y10T156/1093
Claims Analysis
Total Claims: 19
Claim 1
Independent Claim
85 words
A cut-resistant laminated photovoltaic device comprising: a plurality of layer pairs disposed in a superposed relation upon a light-incident surface of a photovoltaic device, each layer pair including a sheet of glass fiber material having a thickness in the range of 2-8 mils and a layer of a thermoplastic polymer having a thickness in the range of 10-25 mils disposed in a coextensive and interpenetrating relationship; and a transparent protective member disposed upon a light incident surface of a topmost one of said layer pairs.
Claim 2
Dependent Claim
85 words
A cut-resistant laminated photovoltaic device comprising: a plurality of layer pairs disposed in a superposed relation upon a light-incident surface of a photovoltaic device, each layer pair including a sheet of glass fiber material having a thickness in the range of 2-8 mils and a layer of a thermoplastic polymer having a thickness in the range of 10-25 mils disposed in a coextensive and interpenetrating relationship; and a transparent protective member disposed upon a light incident surface of a topmost one of said layer pairs.
Claim 3
Dependent Claim
21 words
A device as in claim 1, wherein said sheet of glass fiber material comprises a sheet of woven glass fiber material.
Claim 4
Dependent Claim
21 words
A device as in claim 1, wherein said sheet of glass fiber material comprises a sheet of non-woven glass fiber material.
Claim 5
Dependent Claim
18 words
A device as in claim 1, wherein said sheet of glass fiber material is approximately 5 mils thick.
Claim 6
Dependent Claim
19 words
A device as in claim 1, wherein said layer of thermoplastic polymer comprises a layer of ethylene vinyl acetate.
Claim 7
Dependent Claim
36 words
A device as in claim 1, wherein said sheet of glass fiber material and layer of thermoplastic polymer of each layer pair are disposed in a completely interpenetrating relationship so that no voids are present therein.
Claim 8
Dependent Claim
15 words
A device as in claim 1, including at least three sheets of glass fiber material.
Claim 9
Dependent Claim
14 words
A device as in claim 1, wherein said transparent protective member comprises a fluoropolymer.
Claim 10
Independent Claim
163 words
A method for laminating a photovoltaic device, including the steps of: providing a photovoltaic device; providing a plurality of layer pairs, each layer pair including a sheet of a glass fiber material having a thickness in the range of 2-8 mils, and a layer of a thermoplastic polymer, having a thickness in the range of 10-25 mils. disposed in a coextensive relationship; disposing a first one of said layer pairs upon a light incident surface of said photovoltaic device; disposing a second one of said layer pairs upon said first one said layer pairs so as to form a layer pair stack; disposing a transparent, protective member atop said layer pair stack; and laminating said protective member, layer pair stack, and photovoltaic device together so that the sheet of glass fiber material and the layer of thermoplastic polymer of each layer pair are put in a mutually interpenetrating relationship, and the layer stack is adhered to the photovoltaic device and the protective member.
Claim 11
Independent Claim
163 words
A method for laminating a photovoltaic device, including the steps of: providing a photovoltaic device; providing a plurality of layer pairs, each layer pair including a sheet of a glass fiber material having a thickness in the range of 2-8 mils, and a layer of a thermoplastic polymer, having a thickness in the range of 10-25 mils. disposed in a coextensive relationship; disposing a first one of said layer pairs upon a light incident surface of said photovoltaic device; disposing a second one of said layer pairs upon said first one said layer pairs so as to form a layer pair stack; disposing a transparent, protective member atop said layer pair stack; and laminating said protective member, layer pair stack, and photovoltaic device together so that the sheet of glass fiber material and the layer of thermoplastic polymer of each layer pair are put in a mutually interpenetrating relationship, and the layer stack is adhered to the photovoltaic device and the protective member.
Claim 12
Dependent Claim
32 words
A method as in claim 9, including the further step of disposing a third one of said layer pairs atop said second layer pair so as to form the layer pair stack.
Claim 13
Dependent Claim
27 words
A method as in claim 9, wherein the step of laminating said protective member comprises applying pressure to said protective member, layer pair stack, and photovoltaic device.
Claim 14
Dependent Claim
24 words
A method as in claim 9, wherein said step of laminating comprises applying heat to said protective member, layer pair stack, and photovoltaic device.
Claim 15
Dependent Claim
37 words
A method as in claim 9, wherein the step of providing a plurality of layer pairs comprises providing a plurality of layer pairs which include a sheet of woven glass fiber material of approximately 5 mils thickness.
Claim 16
Dependent Claim
37 words
A method as in claim 9, wherein the step of providing a plurality of layer pairs comprises providing a plurality of layer pairs including a layer of ethylene vinyl acetate thermoplastic polymer of approximately 18 mils thickness.
Claim 17
Dependent Claim
22 words
A method as in claim 9, wherein the step of providing a photovoltaic device comprises providing a flexible, thin film photovoltaic device.
Claim 18
Independent Claim
136 words
A method for laminating a photovoltaic device, including the steps of: providing a photovoltaic device; providing at least three sheets of a glass fiber material having a thickness in the range of 2-8 mils; providing a plurality of layers of a thermoplastic material having at thickness in the range of 10-25 mils; disposing each of said layers in a coextensive relationship with a respective one of said sheets so as to form a layer pair stack; disposing a transparent, protective member atop said layer pair stack; and laminating said protective member, layer pair stack, and photovoltaic device together so that the sheet of glass fiber material and the layer of thermoplastic polymer of each layer pair are put in a mutually interpenetrating relationship, the layer stack is adhered to the photovoltaic device and the protective member.
Claim 19
Independent Claim
136 words
A method for laminating a photovoltaic device, including the steps of: providing a photovoltaic device; providing at least three sheets of a glass fiber material having a thickness in the range of 2-8 mils; providing a plurality of layers of a thermoplastic material having at thickness in the range of 10-25 mils; disposing each of said layers in a coextensive relationship with a respective one of said sheets so as to form a layer pair stack; disposing a transparent, protective member atop said layer pair stack; and laminating said protective member, layer pair stack, and photovoltaic device together so that the sheet of glass fiber material and the layer of thermoplastic polymer of each layer pair are put in a mutually interpenetrating relationship, the layer stack is adhered to the photovoltaic device and the protective member.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1998-12-11 | 1999-06-12 | 1999-12-12 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2002-12-11 | 2003-06-12 | 2003-12-12 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2006-12-11 | 2007-06-12 | 2007-12-12 | $7700.00 | Window Closed / Lapsed |