US5472659A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method for continuously manufacturing compound corrugated pipe having smooth portions
Assignee: Individual
•
Filing: 1993-11-19
•
Granted: 1995-12-05
•
Expires: 2013-11-19
Abstract
Abstract For the continuous manufacture of a compound pipe with a spigot which is substantially smooth on its outside, the compound pipe including a smooth internal tube and an external tube provided with transverse grooves and welded together with the internal tube, an external tube and an internal tube are extruded, the latter into the external tube. While the spigot which is substantially smooth on the outside is manufactured, its external wall is pressure-relieved by compensation chambers.
Inventors
- 👤 Ralph-Peter Hegler
- 👤 Wilhelm Hegler
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-06 01:45
CPC Classifications
B; B29; B29D; B29D99/00; B29D99/001; B29D99/0014; B29C; B29C48/00; B29C48/03; B29C48/09; B29C48/11; B29C48/13; B29C48/25; B29C48/30; B29C48/303; B29C49/00; B29C49/0015; B29C49/0021; B29C49/0024; B29C49/02; B29C49/04; B29C2791/00; B29C2791/004; B29C2791/006; B29C48/001; B29C48/0011; B29C48/002; B29C48/10; B29C48/16; B29C48/18; B29C48/22; B29C49/0025; B29L; B29L2023/00; B29L2023/18; B29L2023/183; B29L2023/186
Claims Analysis
Total Claims: 3
Claim 1
Independent Claim
318 words
A method for a continuous manufacture of a compound pipe (23) of plastic material with a corrugated portion having an outer diameter (d') and with a substantially cylindrical spigot (46) which has a substantially smooth outside and an outer diameter (D) which is smaller than said outer diameter (d') of said corrugated portion, the compound pipe (23) consisting of a smooth internal pipe (45) having a constant inner diameter (d), and an external pipe (42) provided with transverse grooves (24) in the corrugated portion and provided with said substantially smooth outside on said spigot (46) and welded together with the internal pipe (45), comprising the following method steps: an external tube (41) of molten plastic material having an external wall (52) is extruded with an inaccurate metering of said molten plastic material; by a partial vacuum applied from its outside, the external tube (41) is provided with a corrugation with the transverse grooves (24) to form an outer portion of said corrugated portion; an internal tube (43) of molten plastic material having an outer surface is extruded with an inaccurate metering of said molten plastic material into the external tube (41); the internal tube (43) is pressed against corrugation troughs (44) of the external tube (41), where it is welded together with the external tube (41) to form said corrugated portion; at predetermined intervals the external tube (41) is formed by said partial vacuum into said outer portion of said spigot (46); the internal tube (43) is pressed from its inside with its full outer surface against said substantially smooth-walled outer portion of the external tube (41); and the external wall (52) of said substantially smooth-walled outer portion of the external tube (41) is pressure-relieved in small surface sections to form small projections as compensation of said inaccurate metering of said molten plastic material of at least one of said external tube (41) and said internal tube (43).
Claim 2
Independent Claim
318 words
A method for a continuous manufacture of a compound pipe (23) of plastic material with a corrugated portion having an outer diameter (d') and with a substantially cylindrical spigot (46) which has a substantially smooth outside and an outer diameter (D) which is smaller than said outer diameter (d') of said corrugated portion, the compound pipe (23) consisting of a smooth internal pipe (45) having a constant inner diameter (d), and an external pipe (42) provided with transverse grooves (24) in the corrugated portion and provided with said substantially smooth outside on said spigot (46) and welded together with the internal pipe (45), comprising the following method steps: an external tube (41) of molten plastic material having an external wall (52) is extruded with an inaccurate metering of said molten plastic material; by a partial vacuum applied from its outside, the external tube (41) is provided with a corrugation with the transverse grooves (24) to form an outer portion of said corrugated portion; an internal tube (43) of molten plastic material having an outer surface is extruded with an inaccurate metering of said molten plastic material into the external tube (41); the internal tube (43) is pressed against corrugation troughs (44) of the external tube (41), where it is welded together with the external tube (41) to form said corrugated portion; at predetermined intervals the external tube (41) is formed by said partial vacuum into said outer portion of said spigot (46); the internal tube (43) is pressed from its inside with its full outer surface against said substantially smooth-walled outer portion of the external tube (41); and the external wall (52) of said substantially smooth-walled outer portion of the external tube (41) is pressure-relieved in small surface sections to form small projections as compensation of said inaccurate metering of said molten plastic material of at least one of said external tube (41) and said internal tube (43).
Claim 3
Dependent Claim
16 words
A method according to claim 1, wherein the external wall (52) is pressure-relieved in annular-shaped zones.
References Cited (Backward Citations)
EP0237900A1
Cited
US4865797A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1998-12-04 | 1999-06-05 | 1999-12-05 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2002-12-04 | 2003-06-05 | 2003-12-05 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2006-12-04 | 2007-06-05 | 2007-12-05 | $7700.00 | Window Closed / Lapsed |