Abstract

Abstract A polyimide surface (18) of a semiconductor device (12) is pretreat the polyimide layer with a hydroxyl amine solution at an elevated temperature to form functional groups that react with an underfill encapsulant (16) to form covalent bonds during a cure cycle between the polyimide layer and the encapsulant material between the semiconductor device and a substrate (10). The hydroxyl amine solution include a reagent such as 2,(2-aminoethoxy) ethanol dissolved in a solvent like N-methyl pyrolidione at 65° C. for sixty seconds. The hydroxyl amine solution may be sprayed onto the polyimide layer, or deposited by vapor deposition. The semiconductor die with the treated polyimide layer is attached to the substrate by DCA methods leaving a gap between the assemblies. The encapsulant is introduced between the semiconductor die and the substrate and cured to form a covalent bond with the polyimide layer and an environmental seal between the assemblies resulting in enhanced adhesion.

Inventors

  • 👤 Prosanto K. Mukerji

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 05:59
CPC Classifications
C; C08; C08J; C08J5/00; C08J5/12; C08J5/122; C08J7/00; C08J7/12; H; H10; H10W; H10W70/00; H10W70/60; H10W70/62; H10W70/65; H10W72/00; H10W72/30; H10W74/00; H10W74/01; H10W74/012; H10W74/10; H10W74/15; C08J2379/00; C08J2379/04; C08J2379/08; H05; H05K; H05K1/00; H05K1/02; H05K1/03; H05K1/0313; H05K1/032; H05K1/0346; H05K3/00; H05K3/38; H05K3/381; H10W72/851; H10W72/853; H10W72/856; H10W90/00; H10W90/701; H10W90/721; H10W90/724; H10W90/731; H10W90/734; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31721

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 34 words
A semiconductor device, comprising: a polyimide surface pretreated with a hydroxyl amine solution at an elevated temperature to form amino-ester and amide groups; and an encapsulant material with covalent bonds to said adhesive surface.
Claim 2
Dependent Claim 34 words
A semiconductor device, comprising: a polyimide surface pretreated with a hydroxyl amine solution at an elevated temperature to form amino-ester and amide groups; and an encapsulant material with covalent bonds to said adhesive surface.
Claim 3
Dependent Claim 40 words
The semiconductor device of claim 1 wherein said polyimide surface is heated to a range of 50° to 90° C. to form said amino-ester and amide groups on the polyimide surface which form said covalent bonds with said encapsulant material.
Claim 4
Dependent Claim 24 words
The semiconductor device of claim 2 wherein said hydroxyl amine solution includes one of a reagent group of 2,(2-aminoethoxy) ethane alcohol, amines and imidazole.
Claim 5
Dependent Claim 24 words
The semiconductor device of claim 3 wherein said hydroxyl amine solution includes one of a solvent group of N-methyl pyrolidione, N,N-dimethyl formamide, and γ-butyrolactone.

References Cited (Backward Citations)

US4276186A Cited
US5326643A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1998-08-14 1999-02-13 1999-08-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2002-08-14 2003-02-13 2003-08-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2006-08-14 2007-02-13 2007-08-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag