A per-wafer method of stressing gate oxide on a wafer including a substrate and a layer of said gate oxide thereon, said gate oxide fabricated to have a desired breakdown voltage V nominal , the method comprising a step of coupling, prior to deposition of gate material overlying said gate oxide, a source of voltage V S between an upper surface of said gate oxide and a lower surface of said wafer for less than about twenty-five minutes; wherein said voltage V S has a magnitude less than said desired breakdown voltage V nominal .
Claim 2
Dependent Claim
95 words
A per-wafer method of stressing gate oxide on a wafer including a substrate and a layer of said gate oxide thereon, said gate oxide fabricated to have a desired breakdown voltage V nominal , the method comprising a step of coupling, prior to deposition of gate material overlying said gate oxide, a source of voltage V S between an upper surface of said gate oxide and a lower surface of said wafer for less than about twenty-five minutes; wherein said voltage V S has a magnitude less than said desired breakdown voltage V nominal .
Claim 3
Dependent Claim
43 words
The method of claim 1, wherein said step of coupling includes coupling to said upper surface of said gate oxide using a probe selected from the group consisting of (i) a liquid conductor, (ii) a conductive plasma, and (iii) a conductive conforming membrane.
Claim 4
Dependent Claim
36 words
The method of claim 1, wherein said step of coupling includes coupling to said lower surface of said wafer using a probe selected from the group consisting of (i) a liquid conductor, and (ii) an electrode.
Claim 5
Dependent Claim
26 words
The method of claim 1, wherein said step of coupling is carried out at a temperature ranging from of about 20° C. to about 150° C.
Claim 6
Dependent Claim
16 words
The method of claim 1, wherein said step of coupling is continued for about five minutes.
Claim 7
Dependent Claim
118 words
A per-wafer method of stressing gate oxide on a wafer including a substrate, a layer of said gate oxide thereon, and a layer of conductive gate material formed on said layer of said gate oxide, said gate oxide fabricated to have a desired breakdown voltage V nominal , the method comprising a step of coupling a source of voltage V S between an upper surface of said conductive gate material, and a lower surface of said wafer; wherein said voltage V S has a magnitude less than said desired breakdown voltage V nominal ; and wherein said step of coupling is carried out before said layer of conductive gate material is defined to create more than one gate.
Claim 8
Dependent Claim
118 words
A per-wafer method of stressing gate oxide on a wafer including a substrate, a layer of said gate oxide thereon, and a layer of conductive gate material formed on said layer of said gate oxide, said gate oxide fabricated to have a desired breakdown voltage V nominal , the method comprising a step of coupling a source of voltage V S between an upper surface of said conductive gate material, and a lower surface of said wafer; wherein said voltage V S has a magnitude less than said desired breakdown voltage V nominal ; and wherein said step of coupling is carried out before said layer of conductive gate material is defined to create more than one gate.
Claim 9
Dependent Claim
40 words
The method of claim 6, wherein said step of coupling includes coupling to said lower surface of said wafer using a probe selected from the group consisting of (i) a liquid conductor, (ii) a conforming membrane, and (iii) an electrode.
Claim 10
Dependent Claim
23 words
The method of claim 6, wherein said gate material is selected from the group consisting of (i) polysilicon, (ii) polycide, and (iii) metal.
Claim 11
Dependent Claim
16 words
The method of claim 7, wherein said probe includes an electrode made from said gate material.
Claim 12
Dependent Claim
25 words
The method of claim 6, wherein said step of coupling is carried out at a temperature ranging from about 20° C. to about 150° C.
Claim 13
Dependent Claim
18 words
The method of claim 6, wherein said step of coupling is continued for less than about five minutes.
Claim 14
Dependent Claim
139 words
A per-wafer method of stressing gate oxide on a wafer including a substrate, a layer of said gate oxide thereon, and a layer of conductive gate material formed on said layer of said gate oxide, said gate oxide fabricated to have a desired breakdown voltage V nominal , and said layer of conductive gate material being defined into a plurality of separate gates, the method comprising a step of simultaneously coupling a source of voltage V S between an upper surface of each one of said separate gates and a lower surface of said wafer; wherein said voltage V S has a magnitude less than said desired breakdown voltage V nominal ; and wherein said step of coupling is carried out without depositing over said conductive gate material a metal layer that is removed following said step of coupling.
Claim 15
Dependent Claim
139 words
A per-wafer method of stressing gate oxide on a wafer including a substrate, a layer of said gate oxide thereon, and a layer of conductive gate material formed on said layer of said gate oxide, said gate oxide fabricated to have a desired breakdown voltage V nominal , and said layer of conductive gate material being defined into a plurality of separate gates, the method comprising a step of simultaneously coupling a source of voltage V S between an upper surface of each one of said separate gates and a lower surface of said wafer; wherein said voltage V S has a magnitude less than said desired breakdown voltage V nominal ; and wherein said step of coupling is carried out without depositing over said conductive gate material a metal layer that is removed following said step of coupling.
Claim 16
Dependent Claim
48 words
The method of claim 12, wherein said step of coupling includes coupling to said upper surface of each one of said separate gates using a probe selected from the group consisting of (i) a liquid conductor, (ii) a conductive plasma, and ( iii ) a conductive conforming membrane.
Claim 17
Dependent Claim
36 words
The method of claim 12, wherein said step of coupling includes coupling to said lower surface of said wafer using a probe selected from the group consisting of (i) a liquid conductor, and (ii) an electrode.
Claim 18
Dependent Claim
25 words
The method of claim 12, wherein said step of coupling is carried out at a temperature ranging from about 100° C. to about 150° C.
Claim 19
Dependent Claim
28 words
The method of claim 12, wherein said method is carried out after formation and subsequent etch-back of a layer of dielectric material overlying said layer of gate material.