Heating of solid earthen material, measuring moisture and resistivity

Assignee: Battelle Memorial Institute Inc
•
Filing: 1992-05-13
•
Granted: 1994-07-19
•
Expires: 2012-05-13
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The present invention includes a method of treating solid earthen material having volatile, semi-volatile, and non-volatile contaminants. Six electrodes are inserted into a region of earthen material to be treated in a substantially equilateral hexagonal arrangement. Six phases of voltages are applied to corresponding electrodes. The voltages are adjusted within a first range of voltages to create multiple current paths between pairs of the electrodes. The current paths are evenly distributed throughout the region defined by the electrodes and therefore uniformly heat the region. The region of earthen material is heated to a temperature sufficient to substantially remove volatile and semi-volatile contaminants by promoting microbial action. This temperature is less than a melting temperature of the earthen material.

Inventors

  • 👤 William O. Heath
  • 👤 Richard L. Richardson
  • 👤 Steven C. Goheen

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 05:46
CPC Classifications
B; B09; B09C; B09C1/00; B09C1/06; E; E02; E02D; E02D3/00; E02D3/11; H; H05; H05B; H05B3/00; H05B3/0004; H05B3/02; H05B3/03; B09C2101/00

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 142 words
A method for treating solid earthen material having volatile, semi-volatile, and non-volatile contaminants in the presence of microbial organisms, the method comprising the steps of: (a) inserting a plurality of electrodes into solid earthen material, the electrodes being arranged in a selected geometric perimeter defining a region of material to be treated; (b) applying at least six phases of voltages to corresponding ones of the electrodes; (c) adjusting the voltages within a first selected range of voltages to heat the material substantially uniformly throughout the region to a temperature sufficient to promote activity of microbial organisms feeding on voltage, semi-volatile, and non-volatile contaminants within the region of material; and (d) controlling the voltages for maintaining the temperature of the material for a time sufficient for the microbial organisms to substantially biodegrade the volatile, semi-volatile, and non-volatile contaminants within the region of material.
Claim 2
Independent Claim 142 words
A method for treating solid earthen material having volatile, semi-volatile, and non-volatile contaminants in the presence of microbial organisms, the method comprising the steps of: (a) inserting a plurality of electrodes into solid earthen material, the electrodes being arranged in a selected geometric perimeter defining a region of material to be treated; (b) applying at least six phases of voltages to corresponding ones of the electrodes; (c) adjusting the voltages within a first selected range of voltages to heat the material substantially uniformly throughout the region to a temperature sufficient to promote activity of microbial organisms feeding on voltage, semi-volatile, and non-volatile contaminants within the region of material; and (d) controlling the voltages for maintaining the temperature of the material for a time sufficient for the microbial organisms to substantially biodegrade the volatile, semi-volatile, and non-volatile contaminants within the region of material.
Claim 3
Dependent Claim 17 words
The method of claim 1 wherein the voltage ranges from 1000 volts AC to 100,000 volts AC.
Claim 4
Dependent Claim 13 words
The method of claim 1 wherein a starting voltage is 1000 volts AC.
Claim 5
Dependent Claim 17 words
The method of claim 1 wherein the frequency of the voltage is from 60 to 500 hertz.
Claim 6
Dependent Claim 14 words
The method of claim 1 wherein the frequency of the voltage is 60 hertz.
Claim 7
Dependent Claim 11 words
The method of claim 1 wherein the voltages are direct current.
Claim 8
Independent Claim 151 words
A method for treating solid earthen material having volatile, semivolatile, and non-volatile contaminants in the presence of microbial organisms, the method comprising the steps of: (a) inserting a plurality of electrodes into solid earthen material, the electrodes being arranged in a selected geometric perimeter defining a region of material to be treated; (b) applying at least six phases of voltages to individual electrodes within said plurality of electrodes;; (c) adjusting the voltages within a first selected range of voltages to heat the material substantially uniformly throughout the region to a temperature sufficient to promote activity of microbial organisms feeding on voltage, semi-volatile, and non-volatile contaminants within the region of material; and (d) controlling the voltages for maintaining the temperature of from 20° C. to 40° C. within the material for a time sufficient for the microbial organisms to substantially biodegrade the volatile, semi-volatile, and non-volatile contaminants within the region of material.
Claim 9
Independent Claim 151 words
A method for treating solid earthen material having volatile, semivolatile, and non-volatile contaminants in the presence of microbial organisms, the method comprising the steps of: (a) inserting a plurality of electrodes into solid earthen material, the electrodes being arranged in a selected geometric perimeter defining a region of material to be treated; (b) applying at least six phases of voltages to individual electrodes within said plurality of electrodes;; (c) adjusting the voltages within a first selected range of voltages to heat the material substantially uniformly throughout the region to a temperature sufficient to promote activity of microbial organisms feeding on voltage, semi-volatile, and non-volatile contaminants within the region of material; and (d) controlling the voltages for maintaining the temperature of from 20° C. to 40° C. within the material for a time sufficient for the microbial organisms to substantially biodegrade the volatile, semi-volatile, and non-volatile contaminants within the region of material.
Claim 10
Independent Claim 146 words
A method for treating solid earthen material having volatile, semi-volatile, and non-volatile contaminants in the presence of microbial organisms which comprises the steps of: (a) inserting a plurality of electrodes into solid earthen material, the electrodes being arranged in a selected geometric perimeter defining a region of material to be treated; (b) applying at least six phases of voltages to individual electrodes within said plurality of electrodes; (c) adjusting the voltages within a first selected range of voltages to heat the material substantially uniformly throughout the region to a temperature sufficient to promote activity of microbial organisms feeding on voltage, semi-volatile, and non-volatile contaminants within the region of material; and (d) controlling the voltages for maintaining a temperature of 30° C. within the material for a time sufficient for the microbial organisms to substantially biodegrade the volatile, semi-volatile, and non-volatile contaminants within the region of material.
Claim 11
Independent Claim 146 words
A method for treating solid earthen material having volatile, semi-volatile, and non-volatile contaminants in the presence of microbial organisms which comprises the steps of: (a) inserting a plurality of electrodes into solid earthen material, the electrodes being arranged in a selected geometric perimeter defining a region of material to be treated; (b) applying at least six phases of voltages to individual electrodes within said plurality of electrodes; (c) adjusting the voltages within a first selected range of voltages to heat the material substantially uniformly throughout the region to a temperature sufficient to promote activity of microbial organisms feeding on voltage, semi-volatile, and non-volatile contaminants within the region of material; and (d) controlling the voltages for maintaining a temperature of 30° C. within the material for a time sufficient for the microbial organisms to substantially biodegrade the volatile, semi-volatile, and non-volatile contaminants within the region of material.
Claim 12
Independent Claim 131 words
A method for treating solid earthen material having volatile, semi-volatile, and non-volatile contaminants, the method comprising the steps of: (a) inserting a plurality of electrodes into solid earthen material, the electrodes being arranged in a selected geometric perimeter defining a region of material to be treated; (b) applying at least six phases of voltages to corresponding ones of the electrodes; (c) adjusting the voltages within a first selected range of voltages to heat the material substantially uniformly throughout the region to a temperature sufficient to bioremediate the voltage, semi-volatile, and non-volatile contaminants within the region of material; and (d) controlling the voltages for maintaining the temperature of the material for a time sufficient for the added energy to substantially bioremediate the volatile, semi-volatile, and non-volatile contaminants within the region of material.
Claim 13
Independent Claim 131 words
A method for treating solid earthen material having volatile, semi-volatile, and non-volatile contaminants, the method comprising the steps of: (a) inserting a plurality of electrodes into solid earthen material, the electrodes being arranged in a selected geometric perimeter defining a region of material to be treated; (b) applying at least six phases of voltages to corresponding ones of the electrodes; (c) adjusting the voltages within a first selected range of voltages to heat the material substantially uniformly throughout the region to a temperature sufficient to bioremediate the voltage, semi-volatile, and non-volatile contaminants within the region of material; and (d) controlling the voltages for maintaining the temperature of the material for a time sufficient for the added energy to substantially bioremediate the volatile, semi-volatile, and non-volatile contaminants within the region of material.
Claim 14
Dependent Claim 18 words
A method according to claim 9, wherein the temperature is from about 0° C. to about 100° C.
Claim 15
Dependent Claim 13 words
A method according to claim 9, wherein the temperature is about 100° C.

References Cited (Backward Citations)

US4671701A Cited
US4849360A Cited
US4956535A Cited
US4765902A Cited
US4850745A Cited
US4982788A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1997-07-18 1998-01-17 1998-07-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2001-07-18 2002-01-17 2002-07-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2005-07-18 2006-01-17 2006-07-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag