Abstract

Abstract A triazine-based mixture, used as a multichip module device dielectric (14), is made more robust and more resistant to temperature extremes by making it to be of from twenty to sixty percent by weight of triazine and of one to ten percent by weight of siloxane-caprolactone copolymer. The foregoing mixture can be made to have a higher resolution by including zero to twenty percent by weight of novolak epoxy acrylate. The entire mixture preferably additionally comprises two to eight percent by weight of bisphenol-A diglycidyl ether monoepoxyacrylate, zero to twenty percent by weight of carboxyl-terminated butadiene nitrile rubber, two to six percent of N-vinylpyrrolidone, one to ten percent of trimethylolpropanetriacrylate, zero to five weight percent glycidoxypropyltrimethoxysilane, 0.05 to five weight percent photoinitiator, zero to two percent pigment, 0.1 to one percent surfactant, zero to 0.3 percent copper benzoylacetonate, and thirty to fifty percent solvent.

Inventors

  • 👤 Paula J. Brown
  • 👤 Treliant Fang
  • 👤 Jose A. Ors
  • 👤 Venkataram R. Raju
  • 👤 Akshay V. Shah

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 16:03
CPC Classifications
H; H10; H10W; H10W99/00; G; G03; G03F; G03F7/00; G03F7/004; G03F7/027; H05; H05K; H05K3/00; H05K3/46; H05K3/4644; H05K3/4673; H05K3/4676; H05K2201/00; H05K2201/01; H05K2201/0137; H05K2201/0162; H05K3/0011; H05K3/0017; H05K3/0023; Y; Y10; Y10S; Y10S428/00; Y10S428/901; Y10T; Y10T428/00; Y10T428/24; Y10T428/24802; Y10T428/24917

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 60 words
A method for making a circuit device comprising the steps of: applying a mixture to a substrate; solidifying at least part of the mixture to form a solid film layer; and using the film layer as a dielectric; wherein said mixture comprises from twenty to sixty weight percent of triazine and from one to ten weight percent of siloxane-caprolactone copolymer.
Claim 2
Independent Claim 60 words
A method for making a circuit device comprising the steps of: applying a mixture to a substrate; solidifying at least part of the mixture to form a solid film layer; and using the film layer as a dielectric; wherein said mixture comprises from twenty to sixty weight percent of triazine and from one to ten weight percent of siloxane-caprolactone copolymer.
Claim 3
Dependent Claim 19 words
The method of claim 1 wherein: said mixture comprises zero to ten percent by weight of novolak epoxy acrylate.
Claim 4
Dependent Claim 82 words
The method of claim 2 wherein: the mixture comprises two to eight percent by weight of bis phenol-A diglycidyl ether monoepoxyacrylate, zero to twenty percent by weight of carboxylterminated butadiene nitrile, two to six weight percent of N-vinylpyrrolidone, one to ten weight percent trimethylolpropanetriacrylate, zero to five weight percent glycidoxypropyltrimethoxysilane, 0.05 to five weight percent photoinitiator, zero to two weight percent pigment, 0.1 to one weight percent surfactant, zero to 0.3 weight percent copper benzoylacetonate, and thirty to fifty weight percent solvent.
Claim 5
Dependent Claim 21 words
The method of claim 3 wherein: the step of solidifying the mixture comprises the step of irradiating the mixture with light.
Claim 6
Dependent Claim 17 words
The method of claim 4 wherein: the light includes a wavelength of about three hundred sixty-five nanometers.
Claim 7
Dependent Claim 21 words
The method of claim 1 wherein: the step of solidifying the mixture comprises the step of irradiating the mixture with light.
Claim 8
Dependent Claim 28 words
The method of claim 6 further comprising the steps of: selectively removing by means of a solvent portions of the mixture that have not been irradiated with light.
Claim 9
Dependent Claim 19 words
The method of claim 1 wherein: the mixture comprises zero to twenty weight percent of a multifunctional oligomeric acrylate.

References Cited (Backward Citations)

US4296171A Cited
US4554229A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1997-07-04 1998-01-03 1998-07-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2001-07-04 2002-01-03 2002-07-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2005-07-04 2006-01-03 2006-07-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag