Negative photosensitive composition and method for forming a resist pattern by means thereof
Assignee: Mitsubishi Chemical Corp
•
Filing: 1992-08-10
•
Granted: 1994-02-15
•
Expires: 2012-08-10
Abstract
Abstract A negative photosensitive composition comprising (a-1) a compound having at least two organic groups of the following formula (I): --OCH.sub.2 OR.sup.1 (I) wherein R 1 is an alkyl group, in its molecule and an alkali-soluble resin, or (a-2) an alkali-soluble resin having at least two organic groups of the above formula (I) in its molecule, and (b) a photo-acid-generating material.
Inventors
- 👤 Tameichi Ochiai
- 👤 Noriaki Takahashi
- 👤 Yasuhiro Kameyama
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-31 18:43
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/26; G03F7/38; G03F7/004; G03F7/0045; G03F7/038; Y; Y10; Y10S; Y10S430/00; Y10S430/1053; Y10S430/1055; Y10S430/128; Y10S430/146
Claims Analysis
Total Claims: 21
Claim 1
Independent Claim
85 words
A negative photosensitive composition, comprising: (a-1) an aromatic compound having at least two organic groups of formula (I): --OCH.sub.2 OR.sup.1 (I) wherein R 1 is an alkyl group, in its molecule and an alkali-soluble resin having phenolic groups, or (a-2) an alkali-soluble resin having at least two organic groups of the above formula (I) in its molecule; and (b) a photo-acid-generating material, said aromatic compound (a-1), upon acid decomposition of the --OCH 2 OR 1 groups, acting as a cross-linking agent for the alkali-soluble resin.
Claim 2
Dependent Claim
85 words
A negative photosensitive composition, comprising: (a-1) an aromatic compound having at least two organic groups of formula (I): --OCH.sub.2 OR.sup.1 (I) wherein R 1 is an alkyl group, in its molecule and an alkali-soluble resin having phenolic groups, or (a-2) an alkali-soluble resin having at least two organic groups of the above formula (I) in its molecule; and (b) a photo-acid-generating material, said aromatic compound (a-1), upon acid decomposition of the --OCH 2 OR 1 groups, acting as a cross-linking agent for the alkali-soluble resin.
Claim 3
Dependent Claim
171 words
The negative photosensitive composition according to claim 1, wherein the compound having at least two organic groups of the formula (I) in its molecule, is a compound having the organic groups of the formula (I) substituted for at least two hydroxyl groups of at least one phenol selected from the group consisting of (1) phenols having a structure in which a plurality of structures each having one hydroxyl group bonded to one aromatic ring, are connected directly or via an at least bivalent organic group, (2) polyhydric phenols having a structure in which at least two hydroxyl groups are bonded to one aromatic ring, and (3) polyhydric phenols having a structure in which a plurality of structures each having at least two hydroxyl groups bonded to one aromatic ring, or a plurality of structures including a structure having at least two hydroxyl groups bonded to one aromatic ring and a structure having one hydroxyl group bonded to one aromatic ring, are connected directly or via an at least bivalent organic group.
Claim 4
Dependent Claim
165 words
The negative photosensitive composition according to claim 1, wherein the compound having at least two organic groups of the formula (I) in its molecule, is a compound having the organic groups of the formula (I) substituted for at least two hydroxyl groups of at least one phenol selected from the group consisting of compounds of the following formulas (i) to (iv): ##STR10## wherein each of A 1 and A 6 is a lower alkylene, phenylene or lower alkylenephenylene group which may have a substituent, or a direct bond, R 2 is a hydrogen atom or a lower alkyl or phenyl group which may have a substituent, each of n and m is an integer, provided that either one of n and m is an integer of at least 2, or a compound having the organic groups of formula (I) substituted for at least two hydroxyl groups of a polyhydric phenol having a structure wherein at least two hydroxyl groups are bonded to one aromatic ring.
Claim 5
Dependent Claim
49 words
The negative photosensitive composition according to claim 3, wherein the compound having at least two organic groups of the formula (I) in its molecule, is a compound having the organic groups of the formula (I) substituted for at least two hydroxyl groups of a phenol of the formula (ii).
Claim 6
Dependent Claim
74 words
The negative photosensitive composition according to claim 1, wherein the alkali-soluble resin having at least two organic groups of the formula (I) in its molecule, is a compound having the organic groups of the formula (I) substituted for at least two hydroxyl groups of a polymer having repeating units of the following formula (v) or (vi): ##STR11## wherein each of R 3 or R 7 is a hydrogen atom or a lower alkyl group.
Claim 7
Dependent Claim
53 words
The negative photosensitive composition according to claim 5, wherein the alkali-soluble resin having at least two organic groups of the formula (I) in its molecule, is a compound having the organic groups of the formula (I) substituted for at least two hydroxyl groups of a polymer having repeating units of the formula (vi).
Claim 8
Dependent Claim
42 words
The negative photosensitive composition according to claim 1, wherein the compound having at least two organic groups of the formula (I) in its molecule, is a compound selected from the group consisting of compounds of the following formulas (vii) to (xii): ##STR12##
Claim 9
Dependent Claim
39 words
The negative photosensitive composition according to claim 1, wherein the alkali-soluble resin having at least two organic groups of the formula (I) in its molecule, is a polymer having repeating units of the following formula (xiii) or (xiv): ##STR13##
Claim 10
Dependent Claim
15 words
The negative photosensitive composition according to claim 1, wherein the alkali-soluble resin is a polyvinylphenol.
Claim 11
Dependent Claim
16 words
The negative photosensitive composition according to claim 1, wherein the alkali-soluble resin is a novolak resin.
Claim 12
Dependent Claim
20 words
The negative photosensitive composition according to claim 1, wherein the alkali-soluble resin is a polycondensation product of cresol with formaldhyde.
Claim 13
Dependent Claim
32 words
The negative photosensitive composition according to claim 1, wherein the photo-acid-generating material is at least one member selected from the group consisting of organic halogen compounds, onium salts and sulfonic acid esters.
Claim 14
Dependent Claim
17 words
The negative photosensitive composition according to claim 1, wherein the photo-acid-generating material is an organic halogen compound.
Claim 15
Dependent Claim
124 words
The negative photosensitive composition according to claim 1, which comprises: (a-1) an aromatic compound having at least two organic groups of formula (I): --OCH.sub.2 OR.sup.1 (I) wherein R 1 is an alkyl group, in its molecule and an alkali-soluble resin having phenolic groups, and (b) a photo-acid-generating material, said aromatic compound (a-1), upon acid decomposition of the --OCH 2 OR 1 groups, acting as a cross-linking agent for the alkali-soluble resin, wherein the compound (a-1) having at least two organic groups of formula (I) in its molecule, is present in an amount ranging from 1-50 parts by weight, and the photo-acid-generating material is present in an amount ranging from 0.05 to 20 parts by weight, per 100 parts by weight of the alkali-soluble resin.
Claim 16
Dependent Claim
53 words
The negative photosensitive composition according to claim 14, wherein the compound having at least two organic groups of the formula (I) in its molecule, is from 5 to 30 parts by weight, and the photo-acid-generating material is from 0.1 to 10 parts by weight, per 100 parts by weight of the alkali-soluble resin.
Claim 17
Dependent Claim
64 words
The negative photosensitive composition according to claim 1, which comprises (a-2) an alkali-soluble resin having two organic groups of the formula (I) in its molecule, and (b) a photo-acid-generating material, wherein the photo-acid-generating material is from 1 to 100 parts by weight, per 100 parts by weight of the alkali-soluble resin having at least two organic groups of the formula (I) in its molecule.
Claim 18
Dependent Claim
42 words
The negative photosensitive composition according to claim 16, wherein the photo-acid-generating material is from 5 to 50 parts by weight, per 100 parts by weight of the alkali-soluble resin having at least two organic group of the formula (I) in its molecule.
Claim 19
Dependent Claim
15 words
The negative photosensitive composition according to claim 1, which contains a phenothiazine as a sensitizer.
Claim 20
Independent Claim
148 words
A method for forming a resist pattern on a substrate for a semiconductor, which comprises: coating on the substrate a negative photocomposition comprising (a-1) an aromatic compound having at least two organic groups of formula (I): --OCH.sub.2 OR.sup.1 (I) wherein R 1 is an alkyl group, in its molecule and an alkali-soluble resin having phenolic groups, or (a-2) an alkali-soluble resin having at least two organic groups of the formula (I) in its molecule; and (b) a photo-acid-generating material, said aromatic compound (a-1), upon acid decomposition of the --OCH 2 OR 1 groups, acting as a cross-linking agent for the alkali-soluble resin; exposing the coated substrate to light from a mercury lamp or an excimer laser to form a pattern on the coated substrate; heat treating the exposed patterned substrate; developing the patterned coated substrate with an aqueous alkali solution thereby forming a resist pattern on the substrate.
Claim 21
Independent Claim
148 words
A method for forming a resist pattern on a substrate for a semiconductor, which comprises: coating on the substrate a negative photocomposition comprising (a-1) an aromatic compound having at least two organic groups of formula (I): --OCH.sub.2 OR.sup.1 (I) wherein R 1 is an alkyl group, in its molecule and an alkali-soluble resin having phenolic groups, or (a-2) an alkali-soluble resin having at least two organic groups of the formula (I) in its molecule; and (b) a photo-acid-generating material, said aromatic compound (a-1), upon acid decomposition of the --OCH 2 OR 1 groups, acting as a cross-linking agent for the alkali-soluble resin; exposing the coated substrate to light from a mercury lamp or an excimer laser to form a pattern on the coated substrate; heat treating the exposed patterned substrate; developing the patterned coated substrate with an aqueous alkali solution thereby forming a resist pattern on the substrate.
References Cited (Backward Citations)
GB1539192A
Cited
JPS5423574A
Cited
EP0164248A2
Cited
EP0232972A2
Cited
JPH0215270A
Cited
JPH02170165A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1997-02-14 | 1997-08-16 | 1998-02-15 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2001-02-14 | 2001-08-16 | 2002-02-15 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2005-02-14 | 2005-08-16 | 2006-02-15 | $7700.00 | Window Closed / Lapsed |