US5286517A
Expired / Lapsed
US
⏱️ 0.0 years remaining
A process for making an electroluminescent cell using a ZnS host including molecules of a ternary europium tetrafluoride compound
Assignee: NEC Corp
•
Filing: 1992-08-07
•
Granted: 1994-02-15
•
Expires: 2012-08-07
Abstract
Abstract A flat panel display utilizes an array of eletroluminescent cells in which the active layer is of polycrystalline zinc sulfide that is the host for molecules of a ternary europium fluoride compound, advantageously lithium europium tetrafluoride. Each cell includes a pair of electrodes between which are a silicon dioxide barrier layer, sufficiently thin for electrons to tunnel therethrough, the active layer, and a capacitive dielectric layer. Other ternary europium tetrafluoride compounds are described for use as the active layer.
Inventors
- 👤 Dawon Kahng
- 👤 T. Yoshioka
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-07 21:17
CPC Classifications
H; H05; H05B; H05B33/00; H05B33/12; H05B33/14; C; C09; C09K; C09K11/00; C09K11/08; C09K11/77; C09K11/7728; C09K11/7729; C09K11/773; C09K11/7743; C09K11/7744; C09K11/7745
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
216 words
A process for forming an array of electroluminescent cells comprising, depositing on a transparent support member a conductive patterned layer of indium-tin oxide suitable for providing a first set of electrodes for the array, depositing over the support member and the patterned layer a layer of silicon dioxide sufficiently thin to permit electron tunneling therethrough at operating voltages and sufficiently thin to permit electron tunneling therethrough at operating voltages and sufficiently thick to provide a chemically stable interface between the indium-tin oxide layer and the zinc sulfide layer to be deposited thereover, preparing and heating a source of zinc sulfide and a source of an activator material taken from the group consisting of lithium europium tetrafluoride, sodium europium tetrafluoride, beryllium europium tetrafluoride, and magnesium europium tetrafluoride, codepositing on the support member by evaporation material from two sources to form a layer of zinc sulfide including a concentration of the activator material sufficient for electroluminescence, the heating and deposition conditions being such that the activator material sublimes and condenses primarily in molecular form in the layer of zinc sulfide, forming over the zinc sulfide layer a dielectric layer sufficiently thick for serving as a charge storage medium, and forming over said dielectric layer a conductive pattern suitable to provide the second set of electrodes of the array.
Claim 2
Dependent Claim
216 words
A process for forming an array of electroluminescent cells comprising, depositing on a transparent support member a conductive patterned layer of indium-tin oxide suitable for providing a first set of electrodes for the array, depositing over the support member and the patterned layer a layer of silicon dioxide sufficiently thin to permit electron tunneling therethrough at operating voltages and sufficiently thin to permit electron tunneling therethrough at operating voltages and sufficiently thick to provide a chemically stable interface between the indium-tin oxide layer and the zinc sulfide layer to be deposited thereover, preparing and heating a source of zinc sulfide and a source of an activator material taken from the group consisting of lithium europium tetrafluoride, sodium europium tetrafluoride, beryllium europium tetrafluoride, and magnesium europium tetrafluoride, codepositing on the support member by evaporation material from two sources to form a layer of zinc sulfide including a concentration of the activator material sufficient for electroluminescence, the heating and deposition conditions being such that the activator material sublimes and condenses primarily in molecular form in the layer of zinc sulfide, forming over the zinc sulfide layer a dielectric layer sufficiently thick for serving as a charge storage medium, and forming over said dielectric layer a conductive pattern suitable to provide the second set of electrodes of the array.
Claim 3
Dependent Claim
24 words
The process of claim 1 in which the activator material is lithium europium tetrafluoride and the silicon dioxide layer is about 50 angstroms thick.
Claim 4
Dependent Claim
24 words
The process of claim 2 in which the zinc sulfide layer includes a concentration of about 0.5 per cent of lithium europium tetrafluoride molecules.
Claim 5
Dependent Claim
14 words
The process of claim 1 in which the activator material is lithium europium tetrafluoride.
Claim 6
Dependent Claim
14 words
The process of claim 1 in which the activator material is sodium europium tetrafluoride.
Claim 7
Dependent Claim
14 words
The process of claim 1 in which the activator material is beryllium europium tetrafluoride.
Claim 8
Dependent Claim
14 words
The process of claim 1 in which the activator material is magnesium europium tetrafluoride.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1997-02-14 | 1997-08-16 | 1998-02-15 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2001-02-14 | 2001-08-16 | 2002-02-15 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2005-02-14 | 2005-08-16 | 2006-02-15 | $7700.00 | Window Closed / Lapsed |