Abstract

Abstract A target track (20) of an anode (14) of an x-ray tube becomes heated adjacent a focal spot (18) to temperatures on the order of 1100°-1400° C. To protect the anode, a body portion (34) is coated (46) with a thermal energy emissive oxide layer (48). In order to prevent carbon from the body portion from migrating out to the oxide layer and forming carbon monoxide gas, a carbide forming barrier layer (36) is formed (38,40) between the body and the oxide coating. The barrier layer is a dense, substantially pore-free coating of a metal that has a free energy of carbide formation of at least 100 KJ/mole at 1200° C. Preferably, the barrier layer material is zirconium, although hafnium, titanium, vanadium, uranium, tantalum, niobium, chromium, and their alloys also provide acceptable barriers to carbon atom migration. A molybdenum layer (44) is disposed (42) between the oxide layer and the barrier layer to prevent the zirconium or other of the above-listed barrier materials from interacting detrimentally with constituents of the oxide layer.

Inventors

  • 👤 Donald Frank DeCou, Jr.
  • 👤 James G. Hull

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 20:03
CPC Classifications
H; H01; H01J; H01J35/00; H01J35/02; H01J35/04; H01J35/08; H01J35/10; H01J35/105; H01J2235/00; H01J2235/12; H01J2235/1204; H01J2235/1225; H01J2235/1229; H01J2235/1233; H01J2235/1237

Claims Analysis

Total Claims: 30
Claim 1
Independent Claim 111 words
An x-ray tube comprising: an envelope having an evacuated interior region; a cathode disposed within the envelope vacuum interior; and an anode target disposed within the envelope vacuum region, the anode target having a target track which is impacted by electrons emanating from the cathode to generate x-rays, the anode target including: body portion, an oxide layer for dissipating thermal energy from the target, a dense, substantially pore-free layer of a material that forms carbides with sufficient stability that carbon is not released from the carbide to form carbon monoxide gas at temperatures below about 1200° C., the stable carbide forming layer being between the body portion and the oxide coating.
Claim 2
Dependent Claim 111 words
An x-ray tube comprising: an envelope having an evacuated interior region; a cathode disposed within the envelope vacuum interior; and an anode target disposed within the envelope vacuum region, the anode target having a target track which is impacted by electrons emanating from the cathode to generate x-rays, the anode target including: body portion, an oxide layer for dissipating thermal energy from the target, a dense, substantially pore-free layer of a material that forms carbides with sufficient stability that carbon is not released from the carbide to form carbon monoxide gas at temperatures below about 1200° C., the stable carbide forming layer being between the body portion and the oxide coating.
Claim 3
Dependent Claim 28 words
The x-ray tube as set forth in claim 1 wherein the stable carbide forming material has a free energy of carbide formation over 100 KJ/mole at 1200° C.
Claim 4
Dependent Claim 30 words
The x-ray tube as set forth in claim 1 wherein the stable carbide forming material includes at least one of zirconium, hafnium, vanadium, uranium, tantalum, niobium, chromium, and alloys thereof.
Claim 5
Dependent Claim 24 words
The x-ray tube as set forth in claim 3 further including a buffer layer between the stable carbide forming layer and the oxide layer.
Claim 6
Dependent Claim 25 words
The x-ray tube as set forth in claim 1 wherein the stable carbide forming material includes at least one of zirconium, hafnium, and alloys thereof.
Claim 7
Dependent Claim 24 words
The x-ray tube as set forth in claim 5 further including a buffer layer between the stable carbide forming layer and the oxide layer.
Claim 8
Dependent Claim 18 words
The x-ray tube as set forth in claim 6 wherein the buffer layer is a layer of molybdenum.
Claim 9
Dependent Claim 149 words
An x-ray tube comprising: an envelope having an evacuated interior region; a cathode disposed within the envelope vacuum interior; and an anode target disposed within the envelope vacuum region, the anode target having a target track which is impacted by electrons emanating from the cathode to generate x-rays, the anode target including; body portion, an oxide layer for dissipating thermal energy from the target, a layer which is at least 50 atom percent of a stable carbide forming material that includes at least one of titanium, zirconium, hafnium, vanadium, uranium, tantalum, niobium, chromium, and alloys thereof between the body portion and the oxide coating, the layer being sufficiently dense and pore-free that carbon migrating through the body portion form carbides with the dense pore-free layer, which carbides have sufficient stability that carbon is not released from the carbide to form carbon monoxide gas at temperatures below about 1200° C.
Claim 10
Dependent Claim 149 words
An x-ray tube comprising: an envelope having an evacuated interior region; a cathode disposed within the envelope vacuum interior; and an anode target disposed within the envelope vacuum region, the anode target having a target track which is impacted by electrons emanating from the cathode to generate x-rays, the anode target including; body portion, an oxide layer for dissipating thermal energy from the target, a layer which is at least 50 atom percent of a stable carbide forming material that includes at least one of titanium, zirconium, hafnium, vanadium, uranium, tantalum, niobium, chromium, and alloys thereof between the body portion and the oxide coating, the layer being sufficiently dense and pore-free that carbon migrating through the body portion form carbides with the dense pore-free layer, which carbides have sufficient stability that carbon is not released from the carbide to form carbon monoxide gas at temperatures below about 1200° C.
Claim 11
Dependent Claim 73 words
An anode for a high temperature x-ray tube, the anode comprising: body portion; an oxide layer for dissipating thermal energy; a non-porous layer of a material that forms carbides with a free energy of carbide formation of at least 100 KJ/mole at 1200° C., the carbide forming layer being disposed between the body portion and the oxide layer to block carbon from migrating from the anode body and reacting with the oxide layer.
Claim 12
Dependent Claim 73 words
An anode for a high temperature x-ray tube, the anode comprising: body portion; an oxide layer for dissipating thermal energy; a non-porous layer of a material that forms carbides with a free energy of carbide formation of at least 100 KJ/mole at 1200° C., the carbide forming layer being disposed between the body portion and the oxide layer to block carbon from migrating from the anode body and reacting with the oxide layer.
Claim 13
Dependent Claim 30 words
The anode as set forth in claim 9 wherein the carbide forming layer material includes at least one of titanium, zirconium, hafnium, vanadium, uranium, tantalum, niobium, chromium, and alloys thereof.
Claim 14
Dependent Claim 23 words
The anode as set forth in claim 9 wherein the carbide forming material includes at least one of zirconium, hafnium, and alloys thereof.
Claim 15
Dependent Claim 22 words
The anode as set forth in claim 11 further including a buffer layer between the carbide forming material and the oxide layer.
Claim 16
Independent Claim 68 words
A method of forming an anode target for an x-ray tube, the method comprising: forming a target body portion with a target track extending therearound; coating at least a part of the body portion with a dense, substantially pore-free coating of a material that forms carbides with a free-energy of carbide formation of at least 100 KJ/mole at 1200° C.; coating the carbide forming layer with an oxide.
Claim 17
Independent Claim 68 words
A method of forming an anode target for an x-ray tube, the method comprising: forming a target body portion with a target track extending therearound; coating at least a part of the body portion with a dense, substantially pore-free coating of a material that forms carbides with a free-energy of carbide formation of at least 100 KJ/mole at 1200° C.; coating the carbide forming layer with an oxide.
Claim 18
Dependent Claim 29 words
The method as set forth in claim 13 wherein the carbide forming material includes at least one of titanium, zirconium, hafnium, vanadium, uranium, tantalum, niobium, chromium, and alloys thereof.
Claim 19
Dependent Claim 11 words
An anode target constructed according to the method of claim 13.
Claim 20
Independent Claim 108 words
A method of forming an anode target for an x-ray tube, the method comprising: forming a target body portion with a target track extending therearound; applying a porous layer of the carbide forming material that forms carbides with a free-energy of carbide formation at least 100 KJ/mole at 1200° C. to the body portion; heating the carbide forming material sufficiently near to the carbide forming material melting point that the carbide forming material flows into a dense and pore-free layer; coating the carbide forming layer with an oxide, such that the dense, pore-free layer prevents carbon from the body portion from reaching the oxide to form carbon monoxide.
Claim 21
Independent Claim 108 words
A method of forming an anode target for an x-ray tube, the method comprising: forming a target body portion with a target track extending therearound; applying a porous layer of the carbide forming material that forms carbides with a free-energy of carbide formation at least 100 KJ/mole at 1200° C. to the body portion; heating the carbide forming material sufficiently near to the carbide forming material melting point that the carbide forming material flows into a dense and pore-free layer; coating the carbide forming layer with an oxide, such that the dense, pore-free layer prevents carbon from the body portion from reaching the oxide to form carbon monoxide.
Claim 22
Dependent Claim 30 words
The method as set forth in claim 16 further including coating the carbide forming material with a buffer layer and wherein the oxide coating is applied over the buffer layer.
Claim 23
Dependent Claim 23 words
The method as set forth in claim 16 wherein the carbide forming material includes at least one of zirconium, hafnium, and alloys thereof.
Claim 24
Dependent Claim 24 words
The method as set forth in claim 18 further including applying a buffer layer on the carbide forming material before applying the oxide coating.
Claim 25
Dependent Claim 14 words
The method as set forth in claim 19 wherein the buffer layer includes molybdenum.
Claim 26
Dependent Claim 25 words
The method as set forth in claim 16 wherein in the heating step, the target body and coating are heated to less than 1750° C.
Claim 27
Dependent Claim 83 words
An anode for a high temperature x-ray tube, the anode comprising: body portion; an oxide layer for dissipating thermal energy; a non-porous, hydrogen-free layer which is at least 50 percent of a material that forms carbides with a free energy of carbide formation of at least 100 KJ/mole at 1200° C., the carbide forming layer being disposed between the body portion and the oxide layer such that carbon is blocked from migrating out of the anode body and reacting with the oxide layer.
Claim 28
Dependent Claim 83 words
An anode for a high temperature x-ray tube, the anode comprising: body portion; an oxide layer for dissipating thermal energy; a non-porous, hydrogen-free layer which is at least 50 percent of a material that forms carbides with a free energy of carbide formation of at least 100 KJ/mole at 1200° C., the carbide forming layer being disposed between the body portion and the oxide layer such that carbon is blocked from migrating out of the anode body and reacting with the oxide layer.
Claim 29
Dependent Claim 61 words
An x-ray tube comprising: an envelope having an evacuated interior region; a cathode disposed within the vacuum envelope; and an anode target disposed within the vacuum envelope, the anode target including: a body portion; a hydrogen-free barrier layer of a material that forms carbides with migrating free carbon at temperatures above 1100° C., a heat emissive layer for dissipating thermal energy.
Claim 30
Dependent Claim 61 words
An x-ray tube comprising: an envelope having an evacuated interior region; a cathode disposed within the vacuum envelope; and an anode target disposed within the vacuum envelope, the anode target including: a body portion; a hydrogen-free barrier layer of a material that forms carbides with migrating free carbon at temperatures above 1100° C., a heat emissive layer for dissipating thermal energy.

References Cited (Backward Citations)

US4090103A Cited
US5157706A Cited
US5159619A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-11-22 1997-05-24 1997-11-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-11-22 2001-05-24 2001-11-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-11-22 2005-05-24 2005-11-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag