Toner for developing electrostatic image, and image fixing method

Assignee: Canon Inc
•
Filing: 1991-12-26
•
Granted: 1993-10-05
•
Expires: 2011-12-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A toner for developing an electrostatic image has toner particles containing i) a binder resin comprising a resin composition with a domain-matrix structure and ii) a colorant. The resin composition with a domain-matrix a structure is comprised of a resin P1 that forms domain particles and a resin P2 that forms a matrix. The resin P1 has a glass transition temperature Tg1 of from 0° C. to 60° C., and the resin P2 has a glass transition temperature Tg2 of from 40° C. to 90° C. The glass transition temperature Tg2 of the resin P2 is at least 5° C. higher than the glass transition temperature Tg1 of the resin P1, and the domain particles having an average particle diameter of not larger than 5 μm.

Inventors

  • 👤 Minoru Shimojo
  • 👤 Takaaki Kohtaki
  • 👤 Tsuyoshi Takiguchi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 09:16
CPC Classifications
G; G03; G03G; G03G9/00; G03G9/08; G03G9/087; G03G9/08784; G03G9/08795; G03G9/08797

Claims Analysis

Total Claims: 81
Claim 1
Independent Claim 141 words
A heat fixable toner for developing an electrostatic image, comprising toner particles containing i) a binder resin comprising a resin composition with a domain-matrix structure and ii) a colorant; said resin composition with a domain-matrix structure being comprised of a heat fixable resin P1 that forms domain particles and a heat fixable resin P2 that forms a matrix; said heat fixable resin P1 having a glass transition temperature Tg1 of from 15° C. to 50° C., and said heat fixable resin P2 having a glass transition temperature Tg2 of from 55° C. to 80° C., provided that the glass transition temperature Tg2 of said heat fixable resin P2 is at least 5° C. higher than the glass transition temperature Tg1 of said heat fixable resin P1; and said domain particles having an average particle diameter of not larger than 5 μm.
Claim 2
Dependent Claim 141 words
A heat fixable toner for developing an electrostatic image, comprising toner particles containing i) a binder resin comprising a resin composition with a domain-matrix structure and ii) a colorant; said resin composition with a domain-matrix structure being comprised of a heat fixable resin P1 that forms domain particles and a heat fixable resin P2 that forms a matrix; said heat fixable resin P1 having a glass transition temperature Tg1 of from 15° C. to 50° C., and said heat fixable resin P2 having a glass transition temperature Tg2 of from 55° C. to 80° C., provided that the glass transition temperature Tg2 of said heat fixable resin P2 is at least 5° C. higher than the glass transition temperature Tg1 of said heat fixable resin P1; and said domain particles having an average particle diameter of not larger than 5 μm.
Claim 3
Dependent Claim 31 words
The toner according to claim 1, wherein said resin P1 that forms domain particles has a carboxyl group and said resin P2 that forms a matrix has substantially no carboxyl group.
Claim 4
Dependent Claim 30 words
The toner according to claim 2, wherein said resin P1 that forms domain particles has a vinyl resin and said resin P2 that forms a matrix has a vinyl resin.
Claim 5
Dependent Claim 40 words
The toner according to claim 2, wherein said resin P1 that forms domain particles has an acid value of not less than 15 and said resin P2 that forms a matrix has an acid value of not more than 10.
Claim 6
Dependent Claim 39 words
The toner according to claim 3, wherein said resin P1 that forms domain particles contains a carboxyl group-containing vinyl monomer in an amount of from 0.1% by weight to 50% by weight on the basis of said resin P1.
Claim 7
Dependent Claim 39 words
The toner according to claim 3, wherein said resin P1 that forms domain particles contains a carboxyl group-containing vinyl monomer in an amount of from 1% by weight to 30% by weight on the basis of said resin P1.
Claim 8
Dependent Claim 23 words
The toner according to claim 3, wherein said resin P1 that forms domain particles has a polymer synthesized from an unsaturated diolefin monomer.
Claim 9
Dependent Claim 45 words
The toner according to claim 3, wherein said resin P1 that forms domain particles has an acid-modified polymer synthesized from a vinyl monomer and thereafter subjected to acid addition, and said resin P2 that forms a matrix has a polymer synthesized from a vinyl monomer.
Claim 10
Dependent Claim 42 words
The toner according to claim 8, wherein said resin P1 that forms domain particles contains a monomer having an acid-modifiable unsaturated double bond, in an amount of from 0.1% by weight to 70% by weight on the basis of said resin P1.
Claim 11
Dependent Claim 42 words
The toner according to claim 8, wherein said resin P1 that forms domain particles contains a monomer having an acid-modifiable unsaturated double bond, in an amount of from 0.3% by weight to 55% by weight on the basis of said resin P1.
Claim 12
Dependent Claim 26 words
The toner according to claim 8, wherein said acid-modified polymer has a polymer formed by acid modification of a polymer synthesized from an unsaturated diolefin monomer.
Claim 13
Dependent Claim 35 words
The toner according to claim 8, wherein said acid-modified polymer is acid-modified by an acid used in an amount of from 0.1% by weight to 50% by weight on the basis of said resin P1.
Claim 14
Dependent Claim 35 words
The toner according to claim 8, wherein said acid-modified polymer is acid-modified by an acid used in an amount of from 1% by weight to 30% by weight on the basis of said resin P1.
Claim 15
Dependent Claim 21 words
The toner according to claim 2, wherein said resin P1 that forms domain particles is cross-linked with a cross-linkable metal compound.
Claim 16
Dependent Claim 20 words
The toner according to claim 14, wherein said cross-linkable metal compound has an organic metal compound containing a metal ion.
Claim 17
Dependent Claim 33 words
The toner according to claim 14, wherein said cross-linkable metal compound has a hydroxide of a metal ion selected from the group consisting of Na + , K + and Li + .
Claim 18
Dependent Claim 31 words
The toner according to claim 1, wherein said resin P2 that forms a matrix has a carboxyl group and said resin P1 that forms domain particles has substantially no carboxyl group.
Claim 19
Dependent Claim 30 words
The toner according to claim 17, wherein said resin P2 that forms a matrix has a vinyl resin and said resin P1 that forms domain particles has a vinyl resin.
Claim 20
Dependent Claim 40 words
The toner according to claim 17, wherein said resin P2 that forms a matrix has an acid value of not less than 15 and said resin P1 that forms domain particles has an acid value of not more than 10.
Claim 21
Dependent Claim 39 words
The toner according to claim 18, wherein said resin P2 that forms a matrix contains a carboxyl group-containing vinyl monomer in an amount of from 0.1% by weight to 50% by weight on the basis of said resin P2.
Claim 22
Dependent Claim 39 words
The toner according to claim 18, wherein said resin P2 that forms a matrix contains a carboxyl group-containing vinyl monomer in an amount of from 1% by weight to 30% by weight on the basis of said resin P2.
Claim 23
Dependent Claim 23 words
The toner according to claim 18, wherein said resin P2 that forms a matrix has a polymer synthesized from an unsaturated diolefin monomer.
Claim 24
Dependent Claim 45 words
The toner according to claim 17, wherein said resin P2 that forms a matrix has an acid-modified polymer synthesized from a vinyl monomer and thereafter subjected to acid addition, and said resin P1 that forms domain particles has a polymer synthesized from a vinyl monomer.
Claim 25
Dependent Claim 42 words
The toner according to claim 23, wherein said resin P2 that forms a matrix contains a monomer having an acid-modifiable unsaturated double bond, in an amount of from 0.1% by weight to 70% by weight on the basis of said resin P2.
Claim 26
Dependent Claim 42 words
The toner according to claim 23, wherein said resin P2 that forms a matrix contains a monomer having an acid-modifiable unsaturated double bond, in an amount of from 0.3% by weight to 55% by weight on the basis of said resin P2.
Claim 27
Dependent Claim 26 words
The toner according to claim 23, wherein said acid-modified polymer has a polymer formed by acid modification of a polymer synthesized from an unsaturated diolefin monomer.
Claim 28
Dependent Claim 35 words
The toner according to claim 23, wherein said acid-modified polymer is acid-modified by an acid used in an amount of from 0.1% by weight to 50% by weight on the basis of said resin P2.
Claim 29
Dependent Claim 35 words
The toner according to claim 23, wherein said acid-modified polymer is acid-modified by an acid used in an amount of from 1% by weight to 30% by weight on the basis of said resin P2.
Claim 30
Dependent Claim 21 words
The toner according to claim 17, wherein said resin P2 that forms a matrix is cross-linked by a cross-linkable metal compound.
Claim 31
Dependent Claim 20 words
The toner according to claim 29, wherein said cross-linkable metal compound has an organic metal compound containing a metal ion.
Claim 32
Dependent Claim 33 words
The toner according to claim 29, wherein said cross-linkable metal compound has a hydroxide of a metal ion selected from the group consisting of Na + , K + and Li + .
Claim 33
Dependent Claim 34 words
The toner according to claim 1, wherein said resin P1 that forms domain particles has a vinyl resin synthesized from a vinyl monomer and said resin P2 that forms a matrix has a polyester.
Claim 34
Dependent Claim 65 words
The toner according to claim 32, wherein said resin P1 that forms domain particles has a polymer having an unsaturated double bond, formed from a vinyl monomer, and said resin P2 that forms a matrix is a polyester having an unsaturated double bond; said unsatutrated double bond of said resin P1 and that of said resin P2 being chemically bonded in part to each other.
Claim 35
Dependent Claim 40 words
The toner according to claim 33, wherein the glass transition temperature Tg2 of said resin P2 that forms a matrix is at least 10° C. higher than the glass transition temperature Tg1 of said resin P1 that forms domain particles.
Claim 36
Dependent Claim 39 words
The toner according to claim 34, wherein said resin P1 that forms domain particles has an acid value of not less than 15 and said resin P2 that forms a matrix has an acid value of less than 15.
Claim 37
Dependent Claim 39 words
The toner according to claim 33, wherein said resin P1 that forms domain particles contains a carboxyl group-containing vinyl monomer in an amount of from 0.1% by weight to 50% by weight on the basis of said resin P1.
Claim 38
Dependent Claim 39 words
The toner according to claim 33, wherein said resin P1 that forms domain particles contains a carboxyl group-containing vinyl monomer in an amount of from 1% by weight to 30% by weight on the basis of said resin P1.
Claim 39
Dependent Claim 23 words
The toner according to claim 33, wherein said resin P1 that forms domain particles has a polymer synthesized from an unsaturated diolefin monomer.
Claim 40
Dependent Claim 29 words
The toner according to claim 33, wherein said resin P1 that forms domain particles has an acid-modified polymer synthesized from a vinyl monomer and thereafter subjected to acid addition.
Claim 41
Dependent Claim 42 words
The toner according to claim 39, wherein said resin P1 that forms domain particles contains a monomer having an acid-modifiable unsaturated double bond, in an amount of from 0.1% by weight to 70% by weight on the basis of said resin P1.
Claim 42
Dependent Claim 42 words
The toner according to claim 39, wherein said resin P1 that forms domain particles contains a monomer having an acid-modifiable unsaturated double bond, in an amount of from 0.3% by weight to 55% by weight on the basis of said resin P1.
Claim 43
Dependent Claim 26 words
The toner according to claim 39, wherein said acid-modified polymer has a polymer formed by acid modification of a polymer synthesized from an unsaturated diolefin monomer.
Claim 44
Dependent Claim 35 words
The toner according to claim 39, wherein said acid-modified polymer is acid-modified by an acid used in an amount of from 0.1% by weight to 50% by weight on the basis of said resin P1.
Claim 45
Dependent Claim 35 words
The toner according to claim 39, wherein said acid-modified polymer is acid-modified by an acid used in an amount of from 1% by weight to 30% by weight on the basis of said resin P1.
Claim 46
Dependent Claim 54 words
The toner according to claim 32, wherein said resin P1 that forms domain particles has a polymer having a carboxyl group, synthesized from a vinyl monomer, and said resin P2 that forms a matrix has a polyester having a carboxyl group said resin P1 and resin P2 being cross-linked by a cross-linkable metal compound.
Claim 47
Dependent Claim 40 words
The toner according to claim 45, wherein the glass transition temperature Tg2 of said resin P2 that forms a matrix is at least 10° C. higher than the glass transition temperature Tg1 of said resin P1 that forms domain particles.
Claim 48
Dependent Claim 40 words
The toner according to claim 46, wherein said resin P1 that forms domain particles has an acid value of not less than 15 and said resin P2 that forms a matrix has an acid value of not less than 15.
Claim 49
Dependent Claim 39 words
The toner according to claim 45, wherein said resin P1 that forms domain particles contains a carboxyl group-containing vinyl monomer in an amount of from 0.1% by weight to 50% by weight on the basis of said resin P1.
Claim 50
Dependent Claim 39 words
The toner according to claim 45, wherein said resin P1 that forms domain particles contains a carboxyl group-containing vinyl monomer in an amount of from 1% by weight to 30% by weight on the basis of said resin P1.
Claim 51
Dependent Claim 23 words
The toner according to claim 45, wherein said resin P1 that forms domain particles has a polymer synthesized from an unsaturated diolefin monomer.
Claim 52
Dependent Claim 29 words
The toner according to claim 45, wherein said resin P1 that forms domain particles has an acid-modified polymer synthesized from a vinyl monomer and thereafter subjected to acid addition.
Claim 53
Dependent Claim 42 words
The toner according to claim 50, wherein said resin P1 that forms domain particles contains a monomer having an acid-modifiable unsaturated double bond, in an amount of from 0.1% by weight to 70% by weight on the basis of said resin P1.
Claim 54
Dependent Claim 42 words
The toner according to claim 50, wherein said resin P1 that forms domain particles contains a monomer having an acid-modifiable unsaturated double bond, in an amount of from 0.3% by weight to 55% by weight on the basis of said resin P1.
Claim 55
Dependent Claim 26 words
The toner according to claim 50, wherein said acid-modified polymer has a polymer formed by acid modification of a polymer synthesized from an unsaturated diolefin monomer.
Claim 56
Dependent Claim 35 words
The toner according to claim 50, wherein said acid-modified polymer is acid-modified by an acid used in an amount of from 0.1% by weight to 50% by weight on the basis of said resin P1.
Claim 57
Dependent Claim 35 words
The toner according to claim 50, wherein said acid-modified polymer is acid-modified by an acid used in an amount of from 1% by weight to 30% by weight on the basis of said resin P1.
Claim 58
Dependent Claim 20 words
The toner according to claim 45, wherein said cross-linkable metal compound has an organic metal compound containing a metal ion.
Claim 59
Dependent Claim 33 words
The toner according to claim 45, wherein said cross-linkable metal compound has a hydroxide of a metal ion selected from the group consisting of Na + , K + and Li + .
Claim 60
Dependent Claim 44 words
The toner according to claim 1, wherein said resin P1 that forms domain particles is mixed in an amount of from 3 parts by weight to 300 parts by weight based on 100 parts by weight of said resin P2 that forms a matrix.
Claim 61
Dependent Claim 44 words
The toner according to claim 1, wherein said resin P1 that forms domain particles is mixed in an amount of from 3 parts by weight to 100 parts by weight based on 100 parts by weight of said resin P2 that forms a matrix.
Claim 62
Dependent Claim 40 words
The toner according to claim 1, wherein the glass transition temperature Tg2 of said resin P2 that forms a matrix is at least 10° C. higher than the glass transition temperature Tg1 of said resin P1 that forms domain particles.
Claim 63
Dependent Claim 58 words
The toner according to claim 1, wherein said resin composition has a domain-matrix structure formed by heat-melting a resin P1 that forms domain particles and a resin P2 that forms a matrix, blending them with stirring in a molten state to form a blend solution, and further heating the blend solution to compatibilize it, followed by rapid cooling.
Claim 64
Dependent Claim 55 words
The toner according to claim 1, wherein said resin composition has a domain-matrix structure formed by synthesizing a resin P1 that forms domain particles by solution polymerization in a non-polar solvent, and thereafter synthesizing a resin P2 that forms a matrix by solution polymerization in said non-polar solvent in which said resin P1 is present.
Claim 65
Dependent Claim 55 words
The toner according to claim 1, wherein said resin composition has a domain-matrix structure formed by synthesizing a resin P2 that forms a matrix by solution polymerization in a non-polar solvent, and thereafter synthesizing a resin P1 that forms domain particles by solution polymerization in said non-polar solvent in which said resin P2 is present.
Claim 66
Dependent Claim 43 words
The toner according to claim 1, wherein said resin composition has a domain-matrix structure formed by bulk polymerization which is stopped at a stage in the course of reaction, and subjecting a polymer dissolved in unreacted monomers, to suspension polymerization or solution polymerization.
Claim 67
Dependent Claim 45 words
The toner according to claim 1, wherein said resin composition has a domain-matrix structure formed by dissolving in a non-polar solvent a resin P1 that forms domain particles and a resin P2 that forms a matrix, followed by heating and stirring to blend the resins.
Claim 68
Dependent Claim 59 words
The toner according to claim 1, wherein said resin composition has a domain-matrix structure formed by dissolving in a solvent a resin P1 that forms domain particles and a resin P2 that forms a matrix, both having no or less compatibility with each other, and cross-linking the residual double bonds thereof each other in the presence of a peroxide.
Claim 69
Dependent Claim 68 words
The toner according to claim 1, wherein said resin composition has a domain-matrix structure formed by dissolving in a solvent a resin P1 that forms domain particles and a resin P2 that forms a matrix, both having no or less compatibility with each other, followed by cross-linking in the presence of a peroxide or a radical polymerization initiator and using a vinyl monomer or a divinyl cross-linkable monomer.
Claim 70
Dependent Claim 70 words
The toner according to claim 1, wherein said resin P1 that forms domain particles has a number average molecular weight (Mn) of from 1,500 to 40,000 and a weight average molecular weight (Mw) of from 3,000 to 300,000, and said resin P2 that forms a matrix has a number average molecular weight (Mn) of from 1,500 to 20,000 and a weight average molecular weight (Mw) of from 3,000 to 50.000.
Claim 71
Dependent Claim 70 words
The toner according to claim 1, wherein said resin P1 that forms domain particles has a number average molecular weight (Mn) of from 3,500 to 30,000 and a weight average molecular weight (Mw) of from 5,000 to 100,000, and said resin P2 that forms a matrix has a number average molecular weight (Mn) of from 3,000 to 10,000 and a weight average molecular weight (Mw) of from 5,000 to 30,000.
Claim 72
Dependent Claim 70 words
The toner according to claim 1, wherein said resin P1 that forms domain particles has a number average molecular weight (Mn) of from 3,000 to 150,000 and a weight average molecular weight (Mw) of from 6,000 to 1,000,000, and said resin P2 that forms a matrix has a number average molecular weight (Mn) of from 2,000 to 50,000 and a weight average molecular weight (Mw) of from 6,000 to 250,000.
Claim 73
Dependent Claim 70 words
The toner according to claim 1, wherein said resin P1 that forms domain particles has a number average molecular weight (Mn) of from 5,000 to 100,000 and a weight average molecular weight (Mw) of from 10,000 to 700,000, and said resin P2 that forms a matrix has a number average molecular weight (Mn) of from 4,000 to 30,000 and a weight average molecular weight (Mw) of from 10,000 to 150,000.
Claim 74
Dependent Claim 14 words
The toner according to claim 1, wherein said toner particles contains a release agent.
Claim 75
Dependent Claim 96 words
The toner according to claim 73, wherein said release agent has a melt-starting temperature of of not lower than 40° C., and i) has at least two melting points in a temperature range of from 50° C. to 250° C. as measured using a DSC or ii) comprises at least two kinds of those having different melting points each other in that range said release agent being contained in said toner particles in an amount of from 0.1 part by weight to 20 parts by weight based on 100 parts by weight of the binder resin.
Claim 76
Dependent Claim 17 words
The toner according to claim I, wherein said binder resin is cross-linked by a cross-linkable metal compound.
Claim 77
Dependent Claim 41 words
The toner according to claim 1, wherein said toner particles comprise a particle on the surface of which a conductive fine powder particle is buried in the inside of the toner particle by 0.05 μm or more from the surface thereof.
Claim 78
Dependent Claim 40 words
The toner according to claim 2, wherein the glass transition temperature Tg2 of said resin P2 that forms a matrix is at least 10° C. higher than the glass transition temperature Tg1 of said resin P1 that forms domain particles.
Claim 79
Dependent Claim 22 words
The toner according to claim 2, wherein part or the whole of said resin P1 is cross-linked by a cross-linkable metal compound.
Claim 80
Dependent Claim 221 words
An image fixing method comprising passing a transfer medium bearing a toner image, through a heat-roller fixing device comprised of a fixing roller and a pressure roller each having a rubbery elastic material layer formed on a mandrel, to fix said toner image to said transfer medium, and outputting said transfer medium in the direction inclined toward the pressure roller side with respect to the direction perpendicular to a line connecting the centers of said fixing roller and said pressure roller, wherein; said toner for forming the toner image comprises toner particles containing i) a binder resin comprising a resin composition with a domain-matrix structure and ii) a colorant; said resin composition with a domain-matrix structure being comprised of a heat fixable resin P1 that forms domain particles and a heat fixable resin P2 that forms a matrix; said heat fixable resin P1 having a glass transition temperature Tg1 of from 15° C. to 50° C., and said heat fixable resin P2 having a glass transition temperature Tg2 of from 55° C. to 80° C., provided that the glass transition temperature Tg2 of said heat fixable resin P2 is at least 5° C. higher than the glass transition temperature Tg1 of said heat fixable resin P1; and said domain particles having an average particle diameter of not larger than 5 μm.
Claim 81
Dependent Claim 221 words
An image fixing method comprising passing a transfer medium bearing a toner image, through a heat-roller fixing device comprised of a fixing roller and a pressure roller each having a rubbery elastic material layer formed on a mandrel, to fix said toner image to said transfer medium, and outputting said transfer medium in the direction inclined toward the pressure roller side with respect to the direction perpendicular to a line connecting the centers of said fixing roller and said pressure roller, wherein; said toner for forming the toner image comprises toner particles containing i) a binder resin comprising a resin composition with a domain-matrix structure and ii) a colorant; said resin composition with a domain-matrix structure being comprised of a heat fixable resin P1 that forms domain particles and a heat fixable resin P2 that forms a matrix; said heat fixable resin P1 having a glass transition temperature Tg1 of from 15° C. to 50° C., and said heat fixable resin P2 having a glass transition temperature Tg2 of from 55° C. to 80° C., provided that the glass transition temperature Tg2 of said heat fixable resin P2 is at least 5° C. higher than the glass transition temperature Tg1 of said heat fixable resin P1; and said domain particles having an average particle diameter of not larger than 5 μm.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-10-04 1997-04-05 1997-10-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-10-04 2001-04-05 2001-10-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-10-04 2005-04-05 2005-10-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag