← Back to Patent Explorer
US5248576A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of producing color filter using a micellar disruption method

Assignee: Idemitsu Kosan Co Ltd
•
Filing: 1990-09-13
•
Granted: 1993-09-28
•
Expires: 2010-09-13
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for producing color filters which enable a transparent electrode for forming a coloring matter film to be used as a transparent electrode for driving liquid crystals, and a resist for a light-shielding film used in this process for forming an insulating black matrix, is disclosed. The above production method comprises forming a black matrix over electrodes other than those corresponding to the individual separated colors and, at the same time, insulating layers as electrode contact window belts by utilizing the black matrix material; forming the electrode contact window belts by forming an electrically conductive layer over the black matrix so that they connect within each electrode contact window belt unit, but do not connect with those in different electrode contact window belt units; and forming a coloring matter layer by a micellar disruption method.

Inventors

  • 👤 Seiichiro Yokoyama
  • 👤 Hideaki Kurata
  • 👤 Mitsuru Eida

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 06:35
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/0005; G03F7/0007; G02; G02B; G02B5/00; G02B5/20; G02F; G02F1/00; G02F1/01; G02F1/13; G02F1/133; G02F1/1333; G02F1/1335; G02F1/133509; G02F1/133512; G02F1/1345

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 326 words
A process for producing a color filter, the color filter including an insulating substrate, transparent electrodes for a plurality of colors, a black matrix and a coloring matter layer, the color filter further including, near one side of the surface thereof, an electrode contact zone having an electrode contact window belt for each group of the transparent electrodes corresponding to each kind of color, the process comprising: (a) forming a lamination of an insulating substrate and patterned transparent electrodes laminated thereon for a plurality of colors, said lamination including an electrode contact zone having a plurality of units of electrode lines, each unit having a number of electrode lines equal and corresponding to the number of the colors; (b) forming a black matrix on said lamination, said black matrix having a surface resistance of not less than 10 7 Ω/cm 2 ; (c) simultaneously with the step of forming said black matrix, covering sections of said electrode contact zone with the material of said black matrix so that the material of said black matrix covers all electrode lines except a part of each electrode line for each color in each unit of electrode lines; (d) forming an electrically conductive layer in said electrode contact zone over said material of said black matrix and over the electrode lines for each color so that an electrode contact window belt unit is formed for each color and all of the electrode lines in one electrode contact window belt unit for one color are electrically connected with each other but insulated from the electrode lines in other electrode contact window belt units for the other colors, whereby all of the transparent electrodes for one color are electrically connected and the transparent electrodes for different colors are electrically insulated from each other; and (e) forming a porous coloring matter layer on said transparent electrodes by a micellar disruption method for one color at a time by selectively using said transparent electrodes.
Claim 2
Dependent Claim 326 words
A process for producing a color filter, the color filter including an insulating substrate, transparent electrodes for a plurality of colors, a black matrix and a coloring matter layer, the color filter further including, near one side of the surface thereof, an electrode contact zone having an electrode contact window belt for each group of the transparent electrodes corresponding to each kind of color, the process comprising: (a) forming a lamination of an insulating substrate and patterned transparent electrodes laminated thereon for a plurality of colors, said lamination including an electrode contact zone having a plurality of units of electrode lines, each unit having a number of electrode lines equal and corresponding to the number of the colors; (b) forming a black matrix on said lamination, said black matrix having a surface resistance of not less than 10 7 Ω/cm 2 ; (c) simultaneously with the step of forming said black matrix, covering sections of said electrode contact zone with the material of said black matrix so that the material of said black matrix covers all electrode lines except a part of each electrode line for each color in each unit of electrode lines; (d) forming an electrically conductive layer in said electrode contact zone over said material of said black matrix and over the electrode lines for each color so that an electrode contact window belt unit is formed for each color and all of the electrode lines in one electrode contact window belt unit for one color are electrically connected with each other but insulated from the electrode lines in other electrode contact window belt units for the other colors, whereby all of the transparent electrodes for one color are electrically connected and the transparent electrodes for different colors are electrically insulated from each other; and (e) forming a porous coloring matter layer on said transparent electrodes by a micellar disruption method for one color at a time by selectively using said transparent electrodes.
Claim 3
Dependent Claim 44 words
A process according to claim 1, wherein said black matrix is formed by a photo-lithography method using a resist for a light-shielding film comprising at least one of an insulating organic dye dispersed resist and an insulating transparent resist, and a high light-shielding resist.
Claim 4
Dependent Claim 34 words
A process according to claim 1, wherein said black matrix is formed by a photo-lithography method using a resist for a light-shielding film comprising at least two kinds of insulating organic dye dispersed resists.
Claim 5
Dependent Claim 36 words
A process according to claim 1, wherein said black matrix is formed by a photo-lithography method using a resist for a light-shielding film which is an insulating transparent resist containing a black organic dye dispersed therein.

References Cited (Backward Citations)

JPS587608A Cited
JPS605558A Cited
JPS61172103A Cited
JPS62136621A Cited
JPS63144305A Cited
JPS63243298A Cited
US4902592A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-09-27 1997-03-29 1997-09-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-09-27 2001-03-29 2001-09-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-09-27 2005-03-29 2005-09-28 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag