Abstract

Abstract A laminated amorphous metal strip has a first layer having at least two side-by-side strips of amorphous metal of unequal widths. A second layer has at least two side-by-side strips of amorphous metal of unequal widths, the layers being in reverse order with respect to the widths of the strips such that the wider strips overlap and form a brickwork cross-section pattern. A flexible polymeric bonding material is disposed between the layers. The polymeric bonding material is an adhesive and has excellent electrical properties. A device for forming the laminated strip of amorphous metal has a plurality of rolls of amorphous metal. Strips from a roll are positioned side-by-side with strips from a wider roll. A bonding material is applied from spray guns to the surface of the strips. Strips from a roll of metal and a wide roll of metal are positioned on the bonding material in a reverse order of the wider strips. Pressure is applied to the laminate. The laminate is advanced by a continuous belt to which the laminate is magnetically coupled. The device includes a means for cutting the laminate to a desired length. A method for fabricating a laminated strip of amorphous metal includes providing the rolls of metal, positioning the strips having differing widths, applying the bonding material, applying pressure advancing the laminate and cutting the laminate.

Inventors

  • 👤 Kou C. Lin
  • 👤 Frank R. Zickar
  • 👤 Eugene E. Zook
  • 👤 Paul W. Martincic

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 12:27
CPC Classifications
B; B32; B32B; B32B3/00; B32B3/10; H; H01; H01F; H01F27/00; H01F27/24; H01F27/25; H01F3/00; H01F3/04; H01F41/00; H01F41/02; H01F41/0206; H01F41/0213; H01F41/0226; Y; Y10; Y10T; Y10T156/00; Y10T156/10; Y10T156/1052; Y10T156/1084; Y10T156/1085; Y10T156/1089; Y10T156/1092; Y10T156/1097; Y10T156/1098; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/4902; Y10T29/49075; Y10T29/49078; Y10T428/00; Y10T428/12; Y10T428/1234; Y10T428/24; Y10T428/24132; Y10T428/24752; Y10T428/24942

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 369 words
A method of fabricating a laminated strip of amorphous metal which comprises the steps of: providing a first roll and a second roll of amorphous metal strips, the strips of the first roll and of the second roll having an equal width; providing a third roll and a fourth roll of amorphous metal strips, the strips of the third roll and of the fourth roll having an equal width, the width of the strips of the third roll and the fourth roll begin wider than the width of the strips of the first roll and the second roll; unrolling the first roll and the wider third roll such that the strips of the first roll are positioned side-by-side with the strips of the third roll to from a first layer, the layer having a top surface; applying a thin coating of a polymeric bonding material which is compatible with dielectric coolants used in transformers, does not contribute to losses due to eddy currents and hysteresis and has a coefficient of expansion similar to that of the amorphorous metal to the top surface of the layer of strips of the first roll and the third roll; unrolling the second roll and the wider fourth roll such that the strips of the second roll are positioned side-by-side with the strips of the fourth roll to form a second layer and further such that the wider strip is int the reverse order of the position of wider strip of the first and third strips; positioning the side-by-side strips of the second and fourth rolls on the polymeric bonding material on the surface of the strips of the first and third rolls at a curved pressure point such that the wider strips overlap and a brickwork cross-section pattern is formed; applying pressure to the curved pressure point at approximately room temperature to bond the first layer to the second layer to form a single laminated strip having a width substantially equal to the combined widths of the strips of the first roll and the third roll, such that compressive forces that could result in fracture of the laminated strip are eliminated; advancing the laminated strip; cutting the laminated strip to a desired length,
Claim 2
Independent Claim 369 words
A method of fabricating a laminated strip of amorphous metal which comprises the steps of: providing a first roll and a second roll of amorphous metal strips, the strips of the first roll and of the second roll having an equal width; providing a third roll and a fourth roll of amorphous metal strips, the strips of the third roll and of the fourth roll having an equal width, the width of the strips of the third roll and the fourth roll begin wider than the width of the strips of the first roll and the second roll; unrolling the first roll and the wider third roll such that the strips of the first roll are positioned side-by-side with the strips of the third roll to from a first layer, the layer having a top surface; applying a thin coating of a polymeric bonding material which is compatible with dielectric coolants used in transformers, does not contribute to losses due to eddy currents and hysteresis and has a coefficient of expansion similar to that of the amorphorous metal to the top surface of the layer of strips of the first roll and the third roll; unrolling the second roll and the wider fourth roll such that the strips of the second roll are positioned side-by-side with the strips of the fourth roll to form a second layer and further such that the wider strip is int the reverse order of the position of wider strip of the first and third strips; positioning the side-by-side strips of the second and fourth rolls on the polymeric bonding material on the surface of the strips of the first and third rolls at a curved pressure point such that the wider strips overlap and a brickwork cross-section pattern is formed; applying pressure to the curved pressure point at approximately room temperature to bond the first layer to the second layer to form a single laminated strip having a width substantially equal to the combined widths of the strips of the first roll and the third roll, such that compressive forces that could result in fracture of the laminated strip are eliminated; advancing the laminated strip; cutting the laminated strip to a desired length,
Claim 3
Dependent Claim 35 words
The method as defined by claim 1 wherein the step of unrolling the respective rolls comprises using a separate power uncoiler connected to each respective roll, each power uncoiler being controlled by a sonic sensor.
Claim 4
Dependent Claim 29 words
The method as defined by claim 1 wherein the step of advancing the laminated strip comprises magnetically coupling the laminated strip to a continuous belt conveyor having magnets thereon.

References Cited (Backward Citations)

US4201837A Cited
US4413406A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-08-30 1997-03-01 1997-08-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-08-30 2001-03-01 2001-08-31 $3760.00 Window Closed / Lapsed