Abstract

Abstract A bonded wafer enjoying high strength of bonding of component wafers thereof is produced by a method which comprises causing the surfaces for mutual attachment of two semiconductor wafers to be irradiated with an ultraviolet light in an atmosphere of oxygen immediately before the two semiconductor wafers are joined to each other. One of the two semiconductor wafers to be used for the bonded wafer optionally has an oxide film formed on one surface thereof. One of the component wafers of the bonded wafer is optionally polished until the component wafer is reduced to a thin film.

Inventors

  • 👤 Tatsuo Ito
  • 👤 Yasuaki Nakazato

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 18:10
CPC Classifications
H; H10; H10P; H10P90/00; H10P90/19; H10P90/1904; H10P90/1906; H10P90/1914; H10P14/00; H10P14/60; H10P14/63; H10P14/6302; H10P14/6304; H10P14/6306; H10W; H10W10/00; H10W10/10; H10W10/181; Y; Y10; Y10S; Y10S148/00; Y10S148/012; Y10S438/00; Y10S438/974

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 70 words
A method for the production of a bonded semiconductor wafer which is characterized by the fact that in the process for production of said bonded wafer, the surfaces of two semiconductor wafers which are to be bonded are washed with a fluid which leaves defiling substances on said surfaces and said surfaces are irradiated with an ultraviolet light in an atmosphere of oxygen before said two semiconductor wafers are bonded.
Claim 2
Independent Claim 70 words
A method for the production of a bonded semiconductor wafer which is characterized by the fact that in the process for production of said bonded wafer, the surfaces of two semiconductor wafers which are to be bonded are washed with a fluid which leaves defiling substances on said surfaces and said surfaces are irradiated with an ultraviolet light in an atmosphere of oxygen before said two semiconductor wafers are bonded.
Claim 3
Independent Claim 67 words
A method for the production of a bonded semiconductor wafer, wherein at least one wafer has an oxide film formed on one surface thereof and, the surface of said one semiconductor wafer and a second semiconductor wafer intended for mutual bonding are washed with a fluid which leaves defiling substance on said surfaces and said surfaces are irradiated with an ultraviolet light in an atmosphere of oxygen.
Claim 4
Independent Claim 67 words
A method for the production of a bonded semiconductor wafer, wherein at least one wafer has an oxide film formed on one surface thereof and, the surface of said one semiconductor wafer and a second semiconductor wafer intended for mutual bonding are washed with a fluid which leaves defiling substance on said surfaces and said surfaces are irradiated with an ultraviolet light in an atmosphere of oxygen.
Claim 5
Dependent Claim 36 words
A method for the production of a bonded wafer in accordance with claim 1 wherein said bonded wafer is polished until a polished surface is removed to form a thin semiconductor film above the bonding surface.
Claim 6
Independent Claim 109 words
A method of producing semiconductor bonded wafers by joining principal surfaces of two semiconductor wafers together, said method comprising: (a) smoothing the principal surfaces of said two wafers by mirror polishing; (b) washing with a fluid which leaves defiling substances on said surfaces; (c) irradiating the mirror polished surfaces of said two wafers with a ultraviolet light in the presence of oxygen; (d) directly contacting the mirror polished surfaces of said two wafers to each other during irradiating; and (e) bonding said surfaces giving a thermal treatment to said wafers while being held in contact at a temperature of no lower than 1100° C. at least for two hours.
Claim 7
Independent Claim 109 words
A method of producing semiconductor bonded wafers by joining principal surfaces of two semiconductor wafers together, said method comprising: (a) smoothing the principal surfaces of said two wafers by mirror polishing; (b) washing with a fluid which leaves defiling substances on said surfaces; (c) irradiating the mirror polished surfaces of said two wafers with a ultraviolet light in the presence of oxygen; (d) directly contacting the mirror polished surfaces of said two wafers to each other during irradiating; and (e) bonding said surfaces giving a thermal treatment to said wafers while being held in contact at a temperature of no lower than 1100° C. at least for two hours.
Claim 8
Independent Claim 147 words
A method of producing semiconductor bonded wafers by joining principal surfaces of first and second semiconductor wafers together, said method comprising: (a) smoothing the principal surfaces of said first and second wafers by mirror polishing; first mirror polished wafer in an oxidizing atmosphere; (b) thermal oxidizing the principal surface of said first mirror polished wafer in an oxidizing atmosphere; (c) washing with a fluid which leaves defiling substances on said surfaces; (d) irradiating the oxidized principal surface of said first wafer and the mirror polished principal surface of said second wafer with a ultraviolet light in the presence of oxygen; (e) directly contacting the thermal oxidized surface of said first wafer and the mirror polished surface of said second wafer to each other during irradiating; and (f) giving a thermal treatment to said wafers while being held in contact at a temperature no lower than 800° C.
Claim 9
Independent Claim 147 words
A method of producing semiconductor bonded wafers by joining principal surfaces of first and second semiconductor wafers together, said method comprising: (a) smoothing the principal surfaces of said first and second wafers by mirror polishing; first mirror polished wafer in an oxidizing atmosphere; (b) thermal oxidizing the principal surface of said first mirror polished wafer in an oxidizing atmosphere; (c) washing with a fluid which leaves defiling substances on said surfaces; (d) irradiating the oxidized principal surface of said first wafer and the mirror polished principal surface of said second wafer with a ultraviolet light in the presence of oxygen; (e) directly contacting the thermal oxidized surface of said first wafer and the mirror polished surface of said second wafer to each other during irradiating; and (f) giving a thermal treatment to said wafers while being held in contact at a temperature no lower than 800° C.
Claim 10
Dependent Claim 37 words
A method for the production of a bonded semiconductor wafer in accordance with claim 2, wherein said bonded wafer is polished until a polished surface is removed to form a thin semiconductor film above the bonding surface.
Claim 11
Dependent Claim 52 words
The method for production of a bonded semiconductor wafer in accordance with claim 1, wherein said fluid is selected from the group consisting of NH 3 /H 2 O 2 , H 2 SO 4 /H 2 O 2 , HCl/H 2 O 2 , HF, and i-C 3 H 7 OH.
Claim 12
Dependent Claim 52 words
The method for production of a bonded semiconductor wafer in accordance with claim 2, wherein said fluid is selected from the group consisting of NH 3 /H 2 O 2 , H 2 SO 4 /H 2 O 2 , HCl/H 2 O 2 , HF, and i-C 3 H 7 OH.
Claim 13
Dependent Claim 52 words
The method for production of a bonded semiconductor wafer in accordance with claim 4, wherein said fluid is selected from the group consisting of NH 3 /H 2 O 2 , H 2 SO 4 /H 2 O 2 , HCl/H 2 O 2 , HF, and i-C 3 H 7 OH.
Claim 14
Dependent Claim 52 words
The method for production of a bonded semiconductor wafer in accordance with claim 5, wherein said fluid is selected from the group consisting of NH 3 /H 2 O 2 , H 2 SO 4 /H 2 O 2 , HCl/H 2 O 2 , HF, and i-C 3 H 7 OH.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-08-02 1997-02-01 1997-08-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-08-02 2001-02-01 2001-08-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-08-02 2005-02-01 2005-08-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag