Abstract

Abstract A preform (70) has an open top portion (72), a cylindrical barrel portion (74) and a bottom portion (76) formed to close the barrel portion (74) at the end opposite to the open top portion (72). The preform (70) also has an internal partition wall (78) formed to extend across the interior of the barrel portion and from the bottom portion (76). In the transverse direction relative to the longitudinal center axis of the preform (70), the internal partition wall (78) has the maximum wall thickness (a2) at the connection (84) between the inner wall of the barrel portion (74) and the internal partition wall (78), the maximum wall thickness of the internal partition wall being gradually reduced toward the longitudinal center axis of the preform with the minimum wall thickness (a1) at a position (82) near the longitudinal center axis of the preform.

Inventors

  • 👤 Yoshinori Nakamura

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 07:43
CPC Classifications
B; B65; B65D; B65D1/00; B65D1/02; B65D1/04; B29; B29B; B29B11/00; B29B11/06; B29B11/08; B29B11/14; B29C; B29C49/00; B29C49/071; B29C49/08; B29C49/10; B29C49/42; B29C49/64; B29C49/6409; B29C49/6463; B29C2949/00; B29C2949/07; B29C2949/0715; B29C2949/072; B29C2949/073; B29C2949/0733; B29C2949/074; B29C2949/075; B29C2949/0751; B29C2949/0753; B29C2949/0754; B29C2949/076; B29C2949/0768; B29C2949/077; B29C2949/0771; B29C2949/0772; B29C2949/0773; B29C2949/20; B29C2949/22; B29C2949/24; B29C2949/26; B29C2949/28; B29C49/02; B29C49/06; B29C49/12; B29C49/1206; B29C49/122; B29C49/123

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 140 words
A preform to be biaxially stretched and blow molded into a plastic vessel, said preform comprising an open top portion, a cylindrical barrel portion, a bottom portion formed to close the barrel portion at the end opposite to the open top and an internal partition wall formed within said barrel portion to extend from one side to the other side of the inner wall and to extend longitudinally from the bottom portion, said preform being characterized by that said internal partition wall has a thickness profile in the transverse direction relative to the longitudinal axis of the preform in which the wall thickness is maximum at the connection between the internal partition wall and the inner wall of the barrel portion, the wall thickness of the internal partition wall is gradually reduced toward the longitudinal center axis of the preform.
Claim 2
Dependent Claim 140 words
A preform to be biaxially stretched and blow molded into a plastic vessel, said preform comprising an open top portion, a cylindrical barrel portion, a bottom portion formed to close the barrel portion at the end opposite to the open top and an internal partition wall formed within said barrel portion to extend from one side to the other side of the inner wall and to extend longitudinally from the bottom portion, said preform being characterized by that said internal partition wall has a thickness profile in the transverse direction relative to the longitudinal axis of the preform in which the wall thickness is maximum at the connection between the internal partition wall and the inner wall of the barrel portion, the wall thickness of the internal partition wall is gradually reduced toward the longitudinal center axis of the preform.
Claim 3
Dependent Claim 61 words
A preform as defined in claim 1, characterized by that said internal partition wall has a thickness profile in the longitudinal direction in which the wall thickness is maximum at the connection between said internal partition wall and said bottom portion, the wall thickness of said internal partition wall is gradually reduced toward the top edge of said internal partition wall.
Claim 4
Dependent Claim 62 words
A preform as defined in claim 2, characterized by that said internal partition wall has at least one uniform thickness portion at a position near the longitudinal center axis of said internal partition wall and has a thickness transition portion formed to extend from the maximum wall thickness in the longitudinal and transverse directions to the end of said uniform thickness portion.
Claim 5
Dependent Claim 32 words
A preform as defined in claim 1, characterized by that the top edge of said internal partition wall is located in said barrel portion at a position short of said top portion.
Claim 6
Dependent Claim 57 words
A preform as defined in claim 4, characterized by that the top edge of said internal partition wall near the longitudinal center axis of said preform has a height lower than that of the top edge of said internal partition wall near the connection between said internal partition wall and the inner wall of said barrel portion.
Claim 7
Dependent Claim 95 words
A preform as defined in claim 5, characterized by that the central portion of said internal partition wall having its top edge lower than that of the side portion is a substantially uniform thickness portion in the transverse direction relative to the longitudinal center axis of said preform and that said internal partition wall has a thickness transition portion formed to extend from the maximum wall thickness at the connection between said internal partition wall and the inner wall of said barrel portion to the end of said uniform thickness portion in the transverse direction.
Claim 8
Dependent Claim 67 words
A preform as defined in claim 1, characterized by that the top edge of said internal partition wall is located at the same level as the top edge of said open top portion and that the portion of said internal partition wall located within said top portion has a wall thickness smaller than the minimum wall thickness of said internal partition wall located within said barrel portion.
Claim 9
Dependent Claim 82 words
A preform as defined in claim 1, characterized by that the top edge of said internal partition wall is located in said open top portion at a position short of the top edge of said open top portion and formed to be flat in the transverse direction and that the portion of said internal partition wall located within said open top portion has a wall thickness smaller than the minimum wall thickness of said internal partition wall located within said barrel portion.
Claim 10
Dependent Claim 190 words
A process of biaxial-stretch blow molding a plastic vessel, said process being characterized by the steps of injection molding a preform having an open top portion, a cylindrical barrel portion having a closed bottom, and an internal partition wall formed to extend from one side of the inner wall of the barrel portion to the other side of the same and to extend longitudinally from the inner face of the closed bottom, stretchedly driving said bottom portion along the longitudinal axis of said preform by the use of a plurality of stretching rods each arranged for the respective one of partitions divided by the internal partition wall of said preform while at the substantially same time stretching said preform in the transverse direction by introducing a pressurized air into the respective divided partitions, the inner end of each of said stretching rods including a tip member arranged therein at a position offset toward the longitudinal center axis of said preform than the center of the corresponding partition, whereby said internal partition wall can be guided by said tip members when said preform is being stretched along the longitudinal axis thereof.
Claim 11
Dependent Claim 190 words
A process of biaxial-stretch blow molding a plastic vessel, said process being characterized by the steps of injection molding a preform having an open top portion, a cylindrical barrel portion having a closed bottom, and an internal partition wall formed to extend from one side of the inner wall of the barrel portion to the other side of the same and to extend longitudinally from the inner face of the closed bottom, stretchedly driving said bottom portion along the longitudinal axis of said preform by the use of a plurality of stretching rods each arranged for the respective one of partitions divided by the internal partition wall of said preform while at the substantially same time stretching said preform in the transverse direction by introducing a pressurized air into the respective divided partitions, the inner end of each of said stretching rods including a tip member arranged therein at a position offset toward the longitudinal center axis of said preform than the center of the corresponding partition, whereby said internal partition wall can be guided by said tip members when said preform is being stretched along the longitudinal axis thereof.
Claim 12
Dependent Claim 99 words
A process as defined in claim 9, characterized by that said internal partition wall includes three or more partition portions radially extending from the longitudinal center axis of said preform, said partition portions being joined together at said longitudinal center axis to form a joint portion and that each of said tip members has an external contour corresponding to the configuration of a corner formed at the intersection between two adjacent partition portions defining one partition, whereby said tip members can guide said joint portion along said longitudinal center axis when said preform is stretched in the longitudinal direction.
Claim 13
Dependent Claim 148 words
A process as defined in claim 9, characterized by that said injection molding step includes a step of injection molding said preform such that the top edge of said internal partition wall is located within said barrel portion at a position short of said open top portion and the top edge of said internal partition wall at a position near said longitudinal center axis of said preform has a height lower than that of the top edge of said internal partition wall near the connection between said internal partition wall and the inner wall of said barrel portion and that said biaxial-stretch blow molding step includes a step of stretching said internal partition wall in the longitudinal direction with the central portion thereof near the longitudinal center axis being sandwiched by two adjacent tip members which are in contact with the central portion of said internal partition wall.
Claim 14
Dependent Claim 92 words
A process as defined in claim 11, characterized by that said internal partition wall includes three or more partition portions radially extending from the longitudinal center axis of said preform, said partition portions being joined together at said longitudinal center axis to form a joint portion and that each of said tip members has an external contour capable of contacting a corner formed at the intersection between two adjacent partition portions defining one partition, whereby said internal partition wall sandwiched by said tip members can be stretched along said longitudinal center axis.
Claim 15
Dependent Claim 95 words
A process as defined in claim 9, characterized by that said process comprises, prior to said biaxial-stretch blow molding step, a step of temperature regulating the inner and outer walls of said barrel portion and the opposite walls of said internal partition wall in said preform into an appropriate stretching temperature, said temperature regulating step including a step of providing a distribution of temperature in said internal partition wall that at least the upper region of said internal partition wall has a temperature higher than that of the lower region of said internal partition wall.
Claim 16
Dependent Claim 66 words
A process as defined in claim 13, characterized by that said temperature regulating step uses a temperature regulating core for temperature regulating the inner wall of said barrel portion and the opposite sides of said internal partition wall, said temperature regulating core being locally placed adjacent to or in contact with the region of said internal partition wall that should be regulated to a higher temperature.

References Cited (Backward Citations)

US3144152A Cited
US3696919A Cited
US4121976A Cited
US4279349A Cited
US5160059A Cited
JPH03236932A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-08-02 1997-02-01 1997-08-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-08-02 2001-02-01 2001-08-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-08-02 2005-02-01 2005-08-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag