Abstract

Abstract A hot melt adhesive crosslinkable by UV irradiation comprising a hot melt adhesive base, a saturated hydrocarbon oligomer containing at least one acryloyl group in a molecule for affording crosslinkability by UV irradiation, and a photopolymerization initiator, an optical disc comprising a pair of substrate, at least one of which is provided with an information recording layer, adhered to each other by means of a hot melt adhesive crosslinkable by UV irradiation and the process for preparing the same are disclosed. The adhesive of the present invention has a high heat resistance and heat stability, is applicable at a low temperature and at a low viscosity, has high softening point and high viscosity by UV irradiation. The optical disc of the present invention has high productivity, no corrosion and high heat resistance.

Inventors

  • 👤 Isamu Komori
  • 👤 Satoshi Nishikawa
  • 👤 Masao Shizuki

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 21:27
CPC Classifications
G; G11; G11B; G11B7/00; G11B7/24; G11B7/26; C; C08; C08F; C08F299/00; C09; C09J; C09J4/00; G11B7/24018; G11B7/24024; Y; Y10; Y10S; Y10S428/00; Y10S428/913; Y10S430/00; Y10S430/146

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 88 words
An optical disc comprising a pair of substrates, at least one of which is provided with an information recording layer, attached to each other by means of a hot melt adhesive crosslinkable by ultraviolet irradiation, wherein said hot melt adhesive comprises a hot melt adhesive base, a saturated hydrocarbon oligomer containing at least one acryloyl group in a molecule for affording crosslinkability by ultraviolet irradiation, and a photopolymerization initiator and wherein said hot melt adhesive is irradiated by said ultraviolet irradiation other than through said information recording layer.
Claim 2
Dependent Claim 88 words
An optical disc comprising a pair of substrates, at least one of which is provided with an information recording layer, attached to each other by means of a hot melt adhesive crosslinkable by ultraviolet irradiation, wherein said hot melt adhesive comprises a hot melt adhesive base, a saturated hydrocarbon oligomer containing at least one acryloyl group in a molecule for affording crosslinkability by ultraviolet irradiation, and a photopolymerization initiator and wherein said hot melt adhesive is irradiated by said ultraviolet irradiation other than through said information recording layer.
Claim 3
Dependent Claim 27 words
The optical disc of claim 1, wherein said hot melt adhesive is irradiated with said ultraviolet irradiation prior to attaching said pair of substrates to each other.
Claim 4
Dependent Claim 144 words
The optical disc of claim 1, wherein said hot melt adhesive crosslinkable by ultraviolet irradiation comprises (i) a hot melt adhesive base which comprises: (a) one or two of a block thermoplastic elastomer represented by the formula: A--B, A--B--A, or B--A--B wherein A is a polystyrene block having a molecular weight of 2,000 to 12,500 and B is selected from the group consisting of a polybutadiene block, a polyisoprene block and an ethylene-butylene copolymer block each of which has a molecular weight of 1,000 to 250,000, (b) a tackifier, and (c) a softening agent; (ii) an acrylate of a saturated hydrocarbon oligomer containing at least one hydroxy group or carboxy group in a molecule for affording crosslinkability by ultraviolet irradiation, wherein said saturated hydrocarbon oligomer is selected from the group consisting of hydrogenated polybutadiene, polybutene, hydrogenated polyisoprene and polyisobutylene; and (iii) a photopolymerization initiator.
Claim 5
Dependent Claim 26 words
The optical disc of claim 3, wherein said acrylate is selected from the group consisting of a urethane acrylate, an epoxy acrylate and an ester acrylate.
Claim 6
Dependent Claim 65 words
The optical disc of claim 3, wherein 5 to 100 parts by weight of the acrylate for affording crosslinkability by ultraviolet irradiation is employed per 100 weight of the hot melt adhesive base, and 0.5 to 5 weight % of the photopolymerization initiator is employed based on a total amount of the hot melt adhesive base and the acrylate for affording crosslinkability by ultraviolet irradiation.
Claim 7
Dependent Claim 30 words
The optical disc of claim 5, wherein 10 to 40 parts by weight of the acrylate for affording crosslinkability is employed per 100 parts of the hot melt adhesive base.
Claim 8
Dependent Claim 63 words
A process for preparing an optical disc which comprises applying a hot melt adhesive crosslinkable by ultraviolet irradiation onto one of a pair of substrate, at least one of which is provided with an information recording layer, irradiating ultraviolet to the hot melt adhesive applied, and then put the other substrate onto the surface of said substrate applied with the hot melt adhesive.
Claim 9
Dependent Claim 63 words
A process for preparing an optical disc which comprises applying a hot melt adhesive crosslinkable by ultraviolet irradiation onto one of a pair of substrate, at least one of which is provided with an information recording layer, irradiating ultraviolet to the hot melt adhesive applied, and then put the other substrate onto the surface of said substrate applied with the hot melt adhesive.

References Cited (Backward Citations)

US4253899A Cited
US4574142A Cited
US4430417A Cited
US4431723A Cited
US4556464A Cited
US4751124A Cited
US4857434A Cited
US4948825A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-07-12 1997-01-11 1997-07-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-07-12 2001-01-11 2001-07-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-07-12 2005-01-11 2005-07-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag