Tank construction and method of manufacture

Assignee: State Industries LLC
•
Filing: 1992-07-13
•
Granted: 1993-06-08
•
Expires: 2012-07-13
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A tank construction including an outer shell of steel material comprised of two half members welded together. The half members are formed by a deep drawing process. An inner shell of non-corrosive material is cast inside the outer shell by a rotational casting procedure with the external surface of the inner shell located adjacent the internal surface of the outer shell. The inner shell of non-corrosive material provides a substantially leak-tight liner for the outer shell to thus prevent contact between the contents of the tank and the outer shell. The rotational casting of the inner shell inside the outer shell is accomplished by charging the outer shell with a non-corrosive material and then subjecting the outer shell to a rotational casting movement while heat is applied to the outer shell. The outer shell serves as a mold for the inner shell wherein the mold (outer shell) becomes a permanent part of the completed tank.

Inventors

  • 👤 John R. Lindahl

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 00:45
CPC Classifications
B; B65; B65D; B65D90/00; B65D90/02; B65D90/04; B65D90/041; B65D90/044; B05; B05D; B05D7/00; B05D7/22; B05D7/227; B29; B29C; B29C33/00; B29C33/0011; B29C33/0016; B29C41/00; B29C41/02; B29C41/20; B05D1/00; B05D1/002; B05D2401/00; B05D2401/30; B05D2401/32; B29C41/04

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 126 words
A tank construction comprising: an outer shell of steel material having an internal surface, said outer shell comprised of two half members welded together, said half members formed by deep drawing; an inner shell of non-corrosive material having an internal surface, said inner shell of non-corrosive material being cast inside said outer shell by a rotational casting procedure with said external surface of said inner shell located adjacent said internal surface of said outer shell, said inner shell of non-corrosive material providing a substantially leak-tight liner for said outer shell to thus prevent contact between the contents of the tank and the outer shell, said outer shell serving as a mold for the inner shell wherein said mold becomes a permanent part of the completed tank.
Claim 2
Dependent Claim 126 words
A tank construction comprising: an outer shell of steel material having an internal surface, said outer shell comprised of two half members welded together, said half members formed by deep drawing; an inner shell of non-corrosive material having an internal surface, said inner shell of non-corrosive material being cast inside said outer shell by a rotational casting procedure with said external surface of said inner shell located adjacent said internal surface of said outer shell, said inner shell of non-corrosive material providing a substantially leak-tight liner for said outer shell to thus prevent contact between the contents of the tank and the outer shell, said outer shell serving as a mold for the inner shell wherein said mold becomes a permanent part of the completed tank.
Claim 3
Dependent Claim 20 words
A tank construction according to claim 1 in which said non-corrosive material of said inner shell is a polymer material.
Claim 4
Dependent Claim 17 words
A tank construction according to claim 2 wherein said inner shell is bonded to said outer shell.
Claim 5
Dependent Claim 36 words
A tank construction according to claim 3 wherein the internal surface of said outer shell is treated with a heated solution of zinc phosphate prior to the casting of the inner shell in said outer shell.
Claim 6
Dependent Claim 34 words
A tank construction according to claim 4 wherein the zinc phosphate solution is heated within a range of 130°-160° F. and the concentration of zinc in the solution is within the range of 14-16%.
Claim 7
Dependent Claim 40 words
The tank construction according to claim 4 wherein the polymer material is polyethylene which is heated to its melt point within the range of 200°-240° F. and is subsequently heated up to a temperature within the range of 400°-450° F.
Claim 8
Dependent Claim 163 words
A tank construction comprising: an outer shell of steel material having an internal surface, said outer shell comprised of two half members welded together, said half members formed by deep drawing; an inner shell of non-corrosive material having an internal surface, said inner shell of non-corrosive material being cast inside said outer shell by a rotational casting procedure with said external surface of said inner shell located adjacent said internal surface of said outer shell, said inner shell of non-corrosive material providing a substantially leak-tight liner for said outer shell to thus prevent contact between the contents of the tank and the outer shell, said rotational casting of said inner shell is accomplished by charging said outer shell with a non-corrosive material and then subjecting the outer shell to a rotational casting movement while heat is applied to the outer shell, said outer shell serving as a mold for the inner shell wherein said mold becomes a permanent part of the completed tank.
Claim 9
Dependent Claim 163 words
A tank construction comprising: an outer shell of steel material having an internal surface, said outer shell comprised of two half members welded together, said half members formed by deep drawing; an inner shell of non-corrosive material having an internal surface, said inner shell of non-corrosive material being cast inside said outer shell by a rotational casting procedure with said external surface of said inner shell located adjacent said internal surface of said outer shell, said inner shell of non-corrosive material providing a substantially leak-tight liner for said outer shell to thus prevent contact between the contents of the tank and the outer shell, said rotational casting of said inner shell is accomplished by charging said outer shell with a non-corrosive material and then subjecting the outer shell to a rotational casting movement while heat is applied to the outer shell, said outer shell serving as a mold for the inner shell wherein said mold becomes a permanent part of the completed tank.
Claim 10
Dependent Claim 29 words
A tank construction according to claim 7 in which said rotational movement of said outer shell is comprised of simultaneous rotation of the outer shell about two separate axes.

References Cited (Backward Citations)

GB1466774A Cited
US4154797A Cited
US4155787A Cited
US4625892A Cited
US4688691A Cited
US4800128A Cited
US4766019A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-06-07 1996-12-07 1997-06-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-06-07 2000-12-07 2001-06-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-06-07 2004-12-07 2005-06-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag