Lithium secondary battery with a cathode comprising lithium, cobalt and vanadium
Assignee: Ube Corp
•
Filing: 1992-03-06
•
Granted: 1993-03-23
•
Expires: 2012-03-06
Abstract
Abstract A lithium secondary battery comprising an anode active material which contains at least one member selected from the group consisting of lithium, a lithium alloy, and a compound capable of intercalating and deintercalating lithium, a cathode active material, and an electrolyte which is an organic electrolyte containing a lithium salt, wherein said cathode active material is a crystalline compound obtained by mixing a lithium compound, a cobalt compound, and a vanadium compound in a molar ratio of x:y:z, respectively, wherein x is from 0 to 1.1, y is from 0.12 to 0.98, and z is 1-y, and heating the mixture.
Inventors
- 👤 Yoshio Idota
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-02 17:54
CPC Classifications
H; H01; H01M; H01M10/00; H01M10/05; H01M10/056; H01M10/0564; H01M10/0566; H01M10/0567; C; C01; C01G; C01G51/00; C01G51/40; C01G51/42; H01M4/00; H01M4/02; H01M4/36; H01M4/48; H01M4/485; C01P; C01P2002/00; C01P2002/50; C01P2002/52; C01P2002/54; C01P2002/70; C01P2002/72; C01P2002/74; C01P2002/78; C01P2006/00; C01P2006/40; H01M6/00; H01M6/14; H01M6/16; H01M6/162; H01M6/164; H01M6/168; H01M6/18; Y; Y02; Y02E; Y02E60/00; Y02E60/10
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
100 words
A lithium secondary battery comprising an anode active material which contains at least one member selected from the group consisting of lithium, a lithium alloy, and a compound capable of intercalating and deintercalating lithium, a cathode active material, and an electrolyte which is an organic electrolyte containing a lithium salt, wherein said cathode active material is a crystalline compound obtained by mixing a lithium compound, a cobalt compound, and a vanadium compound in a molar ratio of x:y:z, respectively, wherein x is from 0 to 1.1, y is from 0.12 to 0.98, and z is 1-y, and heating the mixture.
Claim 2
Dependent Claim
100 words
A lithium secondary battery comprising an anode active material which contains at least one member selected from the group consisting of lithium, a lithium alloy, and a compound capable of intercalating and deintercalating lithium, a cathode active material, and an electrolyte which is an organic electrolyte containing a lithium salt, wherein said cathode active material is a crystalline compound obtained by mixing a lithium compound, a cobalt compound, and a vanadium compound in a molar ratio of x:y:z, respectively, wherein x is from 0 to 1.1, y is from 0.12 to 0.98, and z is 1-y, and heating the mixture.
Claim 3
Dependent Claim
63 words
The lithium secondary battery as claimed in claim 1, wherein at least one of said cathode active material is a crystalline compound obtained by mixing a lithium compound, a cobalt compound, and a vanadium compound in a molar ratio of x:y:z, respectively, wherein x is from 0 to 1.1, y is from 0.12 to 0.5, and z is 1-y, and heating the mixture.
Claim 4
Dependent Claim
63 words
The lithium secondary battery as claimed in claim 1, wherein at least one of said cathode active material is a crystalline compound obtained by mixing a lithium compound, a cobalt compound, and a vanadium compound in a molar ratio of x:y:z, respectively, wherein x is from 0 to 1.1, y is from 0.8 to 0.98, and z is 1-y, and heating the mixture.
Claim 5
Dependent Claim
20 words
The lithium secondary battery as claimed in claim 2, wherein said anode active material is lithium and/or a lithium alloy.
Claim 6
Dependent Claim
56 words
The lithium secondary battery as claimed in claim 1, wherein at least one of said cathode active material is a crystalline compound represented by Li x Co y V z O q in which x is from 0 to 1.1, y is from 0.12 to 0.98, z is 1-y, and q is from 2.05 to 3.0.
Claim 7
Dependent Claim
19 words
The lithium secondary battery as claimed in claim 1, wherein the heating temperature is from 250° to 2,000° C.
Claim 8
Dependent Claim
19 words
The lithium secondary battery as claimed in claim 1, wherein the heating temperature is from 500° to 1,300° C.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1996-03-22 | 1996-09-21 | 1997-03-23 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2000-03-22 | 2000-09-21 | 2001-03-23 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2004-03-22 | 2004-09-21 | 2005-03-23 | $7700.00 | Window Closed / Lapsed |